    • 122. 发明授权
    • Production of metal and metalloid nitrides
    • 生产金属和准金属氮化物
    • US5466310A
    • 1995-11-14
    • US107812
    • 1993-08-18
    • Barry W. NinhamAndrzej CalkaJames S. Williams
    • Barry W. NinhamAndrzej CalkaJames S. Williams
    • B22F1/00B22F9/04C01B21/06C04B35/56C04B35/58C04B35/65C22C1/05
    • C04B35/58014C04B35/58007C04B35/58028C04B35/645C04B35/65C22C1/055
    • A nitride of a metal or solid metalloid is produced by ball milling a powder of a metal or metalloid in a nitrogen, or nitrogen-containing atmosphere (such as ammonia). The pressure in the ball mill is normally from 100 to 5,000 kPa, typically about 300 kPa. The ball mill temperature may be from room temperature to 500.degree. C., preferably from 200.degree. C. to 400.degree. C. The product powder is normally pressure moulded and annealed at 800.degree. C. for about 1 hour to produce a strong, hard body. Controlling the degree of nitration, or mixing the product nitride powder with a metal powder before pressure moulding, enables a composite comprising a metal matrix with a dispersed nitride phase to be produced. An alternative technique, involves ball milling the metal or metalloid powder with an organic nitrogen-containing chemical which dissociates in the ball mill. This yields a mixture of the nitride and carbide of a metal or solid metalloid.
    • PCT No.PCT / AU92 / 00073 Sec。 371日期:1993年8月18日 102(e)日期1993年8月18日PCT提交1992年2月19日PCT公布。 出版物WO92 / 14568 日期:1992年9月3日。金属或固体准金属的氮化物通过在氮气或含氮气氛(如氨)中球磨研磨金属或准金属的粉末来制备。 球磨机中的压力通常为100-5,000kPa,通常为约300kPa。 球磨机温度可以为室温至500℃,优选为200℃至400℃。产品粉末通常在800℃下进行加压成型并退火约1小时,以产生强烈的硬质 身体。 在压力成型之前控制硝化程度或者将氮化物粉末与金属粉末混合,可以制备包含具有分散的氮化物相的金属基质的复合材料。 一种替代技术涉及用在球磨机中解离的有机含氮化合物球磨金属或准金属粉末。 这产生了金属或固体准金属的氮化物和碳化物的混合物。