    • 94. 发明授权
    • Melt-kneaded products, molded resin products, and production method thereof
    • 熔融捏合产品,模塑树脂产品及其制备方法
    • US07935417B2
    • 2011-05-03
    • US12028213
    • 2008-02-08
    • Hiroshi ShimizuYongjin Li
    • Hiroshi ShimizuYongjin Li
    • B32B5/16B29B7/90
    • C08J3/201C08J3/005C08J2321/00C08J2327/16Y10S977/742Y10S977/773Y10T428/25
    • A melt-kneading method for filling material and elastomer or resin, characterized in that a filling material constituted by a filler, and an elastomer or resin (thermoplastic resin or thermosetting resin), are introduced from a material introduction part at the end of a melt-kneading part having a cylinder with a screw and a heater, and the molten elastomer or resin and filling material constituted by a filler are kneaded under the conditions of 1000 to 3000 rpm in the rotation speed of the screw and 1500 to 4500 sec−1 in shear speed to feed the mixture from the rear edge to tip of the screw to be trapped in a space provided at the tip of the screw, after which the mixture is moved from the space to the rear edge of the screw through a hole provided at the center of the screw, with the cycle process performed for a specified period based on recirculation using the screw.
    • 一种用于填充材料和弹性体或树脂的熔融捏合方法,其特征在于,由填料构成的填充材料和弹性体或树脂(热塑性树脂或热固性树脂)在熔体末端的材料导入部分引入 - 具有螺杆和加热器的圆筒的中空部件和由填料构成的熔融弹性体或树脂和填充材料在螺杆的旋转速度为1000〜3000rpm的条件下混炼,并且在1500〜4500秒-1 在剪切速度下将混合物从后边缘到螺杆的尖端进入,以将其捕获在设置在螺钉尖端处的空间中,之后混合物通过提供的孔从螺钉的空间移动到后边缘 在螺杆的中心处,循环过程基于使用螺杆的循环进行一段指定的时间段。