    • 8. 发明授权
    • Titanium based high-K dielectric films
    • 钛基高K电介质膜
    • US08737036B2
    • 2014-05-27
    • US13657782
    • 2012-10-22
    • Intermolecular, Inc.
    • Hanhong ChenNobumichi FuchigamiImran HashimEdward L. HaywoodPragati KumarSandra G. MalhotraMonica Sawkar MathurPrashant B. PhatakSunil Shanker
    • H01G4/30
    • H01G4/1218C23C16/405C23C16/45531C23C16/56H01G4/33H01L21/02186H01L21/022H01L21/0228H01L21/02312H01L21/02337H01L21/3141H01L21/3142H01L28/40
    • This disclosure provides (a) methods of making an oxide layer (e.g., a dielectric layer) based on titanium oxide, to suppress the formation of anatase-phase titanium oxide and (b) related devices and structures. A metal-insulator-metal (“MIM”) stack is formed using an ozone pretreatment process of a bottom electrode (or other substrate) followed by an ALD process to form a TiO2 dielectric, rooted in the use of an amide-containing precursor. Following the ALD process, an oxidizing anneal process is applied in a manner is hot enough to heal defects in the TiO2 dielectric and reduce interface states between TiO2 and electrode; the anneal temperature is selected so as to not be so hot as to disrupt BEL surface roughness. Further process variants may include doping the titanium oxide, pedestal heating during the ALD process to 275-300 degrees Celsius, use of platinum or ruthenium for the BEL, and plural reagent pulses of ozone for each ALD process cycle. The process provides high deposition rates, and the resulting MIM structure has substantially no x-ray diffraction peaks associated with anatase-phase titanium oxide.
    • 本公开内容提供(a)制造基于氧化钛的氧化物层(例如电介质层)的方法,以抑制锐钛矿相氧化钛的形成和(b)相关的器件和结构。 使用底部电极(或其他基底)的臭氧预处理随后进行ALD工艺来形成金属 - 绝缘体 - 金属(“MIM”)堆叠,以形成根植于使用含酰胺的前体的TiO 2电介质。 在ALD工艺之后,氧化退火工艺的应用热度足以愈合TiO2电介质中的缺陷,并降低TiO2和电极之间的界面态; 选择退火温度以使其不那么热,以致破坏BEL表面粗糙度。 进一步的工艺变型可以包括在ALD工艺期间掺杂氧化钛,基座加热至275-300摄氏度,对于BEL使用铂或钌,对于每个ALD工艺循环使用多个试剂脉冲的臭氧。 该方法提供高沉积速率,并且所得MIM结构基本上没有与锐钛矿相氧化钛相关的x射线衍射峰。
    • 10. 发明申请
    • Method for Fabricating a DRAM Capacitor
    • 制造DRAM电容器的方法
    • US20130154057A1
    • 2013-06-20
    • US13738794
    • 2013-01-10
    • Intermolecular, Inc.Elpida Memory, Inc
    • Karthik RamaniHanhong ChenWim DeweerdNobumichi FuchigamiHiroyuki Ode
    • H01L49/02
    • H01L28/40H01G4/1218H01G4/33H01L28/60H01L28/75Y10T29/43Y10T29/435Y10T29/49002
    • A method for fabricating a dynamic random access memory (DRAM) capacitor stack is disclosed wherein the stack includes a first electrode, a dielectric layer, and a second electrode. The first electrode is formed from a conductive binary metal compound and the conductive binary metal compound is annealed in a reducing atmosphere to promote the formation of a desired crystal structure. The binary metal compound may be a metal oxide. Annealing the metal oxide (i.e. molybdenum oxide) in a reducing atmosphere may result in the formation of a first electrode material (i.e. MoO2) with a rutile-phase crystal structure. This facilitates the formation of the rutile-phase crystal structure when TiO2 is used as the dielectric layer. The rutile-phase of TiO2 has a higher k value than the other possible crystal structures of TiO2 resulting in improved performance of the DRAM capacitor.
    • 公开了一种用于制造动态随机存取存储器(DRAM)电容器堆叠的方法,其中堆叠包括第一电极,电介质层和第二电极。 第一电极由导电二元金属化合物形成,并且导电二元金属化合物在还原气氛中退火以促进所需晶体结构的形成。 二元金属化合物可以是金属氧化物。 在还原气氛中退火金属氧化物(即氧化钼)可导致形成具有金红石相晶体结构的第一电极材料(即MoO 2)。 当使用TiO 2作为电介质层时,这有助于金红石相晶体结构的形成。 TiO 2的金红石相具有比其他可能的TiO 2晶体结构更高的k值,从而改善了DRAM电容器的性能。