    • 1. 发明授权
    • White emitting persistent phosphor
    • 白色发光持久荧光粉
    • US08506843B2
    • 2013-08-13
    • US12971569
    • 2010-12-17
    • Alok SrivastavaHolly Ann ComanzoSam CamardelloWilliam W. Beers
    • Alok SrivastavaHolly Ann ComanzoSam CamardelloWilliam W. Beers
    • C09K11/55C09K11/64
    • C09K11/778C09K11/7758C09K11/7797
    • This disclosure features a persistent phosphor having the following formula I: Sra,Cab,BacAl2-m-n-o-pOd:Euy,REz,Bm,Znn,Coo,Scp  I where a and b each range from about 0.3 to about 0.7; c is between about 0 and about 0.1; 0.75≦a+b+c+y+z≦1.3; y is between about 0.0005 and about 0.1; RE is any rare earth element alone or in combination; z is between about 0.0005 and about 0.15; m is between about 0.0005 and about 0.30; n is between about 0 and about 0.10; o is between about 0 and about 0.01; p is between about 0 and about 0.10 and d ranges from about 3.945 to about 4.075. Once the persistent phosphor has been excited it appears white in an absence of ambient light. Also featured is an article of manufacture that includes the phosphor.
    • 本公开的特征在于具有以下式I的持久性荧光体:Sra,Cab,BacAl2-m-n-o-pOd:Euy,REz,Bm,Znn,Coo,ScpI,其中a和b各自为约0.3至约0.7; c在约0和约0.1之间; 0.75 @ a + b + c + y + z @ 1.3; y在约0.0005和约0.1之间; RE是单独或组合的任何稀土元素; z在约0.0005和约0.15之间; m在约0.0005和约0.30之间; n在约0和约0.10之间; o为约0至约0.01; p为约0至约0.10,d为约3.945至约4.075。 一旦持续的荧光体被激发,它在没有环境光的情况下看起来是白色的。 还有一个包括磷光体的制品。
    • 3. 发明申请
    • WHITE PERSISTENT PHOSPHOR BLEND OR LAYERED STRUCTURE
    • 白色磷灰石混合或层状结构
    • US20120153226A1
    • 2012-06-21
    • US12971504
    • 2010-12-17
    • Holly Ann COMANZOAlok SrivastavaWilliam W. Beers
    • Holly Ann COMANZOAlok SrivastavaWilliam W. Beers
    • C09K11/80C09K11/79
    • C09K11/7774C09K11/663C09K11/7734C09K11/7792
    • This disclosure features a blend, or use together in at least two layers of an article of manufacture, of a first persistent phosphor, a second persistent phosphor and a third phosphor. The first persistent phosphor has a formula I: Cax-y-z-aAaAl2-m-n-o-pOd:Euy,REz,Bm,Znn,Coo,Scp  I where the variables are defined in the disclosure. The second persistent phosphor has a formula II: Srx-y-z-aAaAl14-m-n-o-pOd:Euy,REz,Bm,Znn,Coo,Scp  II where the variables are defined in the disclosure. The third phosphor is a non-persistent phosphor that is excited at a wavelength in a range of 300-500 nm. Also featured is an article of manufacture including the blend or the phosphors present in at least two layers. Once the blend or layered structure comprising the three phosphors has been excited it can appear white in an absence of ambient light.
    • 本公开的特征在于共混物,或者在制品的至少两层中一起使用第一持久荧光体,第二持续荧光体和第三荧光体。 第一持久性荧光体具有式I:Cax-y-z-aAaAl2-m-n-o-pOd:Euy,REz,Bm,Znn,Coo,Scp I,其中变量在本公开中定义。 第二持续荧光体具有式II:Srx-y-z-aAaAl14-m-n-o-pOd:Euy,REz,Bm,Znn,Coo,Scp II,其中变量在本公开中定义。 第三荧光体是在300-500nm范围内的波长下激发的非持久荧光体。 还有一个包括共混物或至少两层中存在的荧光体的制品。 一旦包含三种荧光体的共混物或分层结构已经被激发,它可以在不存在环境光的情况下显现为白色。
    • 4. 发明授权
    • White persistent phosphor blend or layered structure
    • 白色持久荧光粉共混物或分层结构
    • US08404153B2
    • 2013-03-26
    • US12971504
    • 2010-12-17
    • Holly Ann ComanzoAlok SrivastavaWilliam W. Beers
    • Holly Ann ComanzoAlok SrivastavaWilliam W. Beers
    • C09K11/08
    • C09K11/7774C09K11/663C09K11/7734C09K11/7792
    • This disclosure features a blend, or use together in at least two layers of an article of manufacture, of a first persistent phosphor, a second persistent phosphor and a third phosphor. The first persistent phosphor has a formula I: Cax-y-z-aAaAl2-m-n-o-pOd:Euy,REz,Bm,Znn,Coo,Scp  I where the variables are defined in the disclosure. The second persistent phosphor has a formula II: Srx-y-z-aAaAl14-m-n-o-pOd:Euy,REz,Bm,Znn,Coo,Scp  II where the variables are defined in the disclosure. The third phosphor is a non-persistent phosphor that is excited at a wavelength in a range of 300-500 nm. Also featured is an article of manufacture including the blend or the phosphors present in at least two layers. Once the blend or layered structure comprising the three phosphors has been excited it can appear white in an absence of ambient light.
    • 本公开的特征在于共混物,或者在制品的至少两层中一起使用第一持久荧光体,第二持续荧光体和第三荧光体。 第一持久性荧光体具有式I:Cax-y-z-aAaAl2-m-n-o-pOd:Euy,REz,Bm,Znn,Coo,Scp I,其中变量在本公开中定义。 第二持续荧光体具有式II:Srx-y-z-aAaAl14-m-n-o-pOd:Euy,REz,Bm,Znn,Coo,Scp II,其中变量在本公开中定义。 第三荧光体是在300-500nm范围内的波长下激发的非持久荧光体。 还有一个包括共混物或至少两层中存在的荧光体的制品。 一旦包含三种荧光体的共混物或分层结构已经被激发,它可以在不存在环境光的情况下显现为白色。
    • 9. 发明授权
    • Fluorescent lamp with conductive coating
    • 荧光灯带导电涂层
    • US07378797B2
    • 2008-05-27
    • US11303149
    • 2005-12-16
    • Evan KarrsWilliam W. BeersMatthew PierceGary R. Allen
    • Evan KarrsWilliam W. BeersMatthew PierceGary R. Allen
    • H01J11/00
    • H01J61/35H01J9/20H01J61/547H01J61/72
    • Fluorescent lamps that comprise a glass envelope with an exterior surface and first and second electrodes located within the glass envelope include a transparent electrically conductive material affixed to the exterior surface of the glass envelope. The transparent electrically conductive material extends between the vicinity of the first electrode and the vicinity of the second electrode, thereby providing a path for an electric current to pass between the first and second electrodes and reduce the open circuit voltage required to start the fluorescent lamp. The transparent electrically conductive material affixed to the exterior surface of the glass envelope can comprise one or more stripes of the material so that less than the total exterior surface area of the glass envelope is covered by the transparent electrically conductive material.
    • 包括具有外表面的玻璃外壳和位于玻璃外壳内的第一和第二电极的荧光灯包括固定在玻璃外壳的外表面上的透明导电材料。 透明导电材料在第一电极附近和第二电极附近之间延伸,由此提供电流在第一和第二电极之间通过的路径,并降低启动荧光灯所需的开路电压。 固定在玻璃外壳表面上的透明导电材料可以包括该材料的一个或多个条纹,使得小于玻璃外壳的总外表面积被透明导电材料覆盖。