会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明公开
    • 난연성 원사를 제조하는 신규한 방법
    • 制造阻燃纱线的新型工艺
    • KR1020160143834A
    • 2016-12-14
    • KR1020167031878
    • 2015-04-21
    • 메르메
    • 다무르,프랑수와-자비에
    • D02G3/40D02G3/44D01D11/06D01F1/07D01F8/04
    • D02G3/404D01D11/06D01F1/07D01F8/04D02G3/443
    • 본발명은중합체시스로코팅된다중-필라멘트코어(1)로구성된원사(I)를제조하는방법에관한것이다. 상기시스는용융중합체의혼화성혼합물을상기다중-필라멘트코어(1) 위에부착시키는단계에의하여제조되지만, 상기혼합물은ㆍ상기적어도하나의난연제(4), 및ㆍ한편으로는기저중합체로알려진다른중합체의유리전이온도보다상당히더 낮은유리전이온도, 및다른한편으로는또한상기기저중합체의용융온도보다상당히더 낮은용융온도를갖는, 공-난연성중합체로서알려진, 2개의중합체중의하나와상호간의영구적인화학결합을, 용융상태에서, 설정하지않는적어도 2개의중합체를포함한다.
    • 本发明涉及由涂覆有聚合物护套的复丝芯(1)组成的纱线(I)的制造方法。 护套通过在多丝芯(1)上沉积熔融聚合物的可混溶混合物来制备,所述混合物包括:至少一种阻燃剂(4)和至少两种在熔融状态下不形成的聚合物 与两种聚合物中的一种称为共阻燃聚合物,其一方面玻璃化转变温度明显低于另一种被称为基础聚合物的聚合物的玻璃化转变温度,以及 另一方面,熔点也显着低于基础聚合物的熔点。
    • 3. 发明授权
    • 필라멘트 코팅 장치와 시스템 및 방법
    • 纤维涂料设备及其制程及其工艺
    • KR100320619B1
    • 2002-01-15
    • KR1020010023365
    • 2001-04-30
    • 일리노이즈 툴 워크스 인코포레이티드
    • 곽규-치우
    • D01D11/06
    • A61F13/15593B05C5/0241
    • 신체상의유체흡수위생물품의제작시스트랜드(strand)에유동체(fluids)를적용하며유동체가코팅된스트랜드를기초재에접착하는데이용할수 있는방법은, 격리된경로를따라스트랜드를인발(drawing)하며, 필라멘트(유동체섬유)가스트랜드쪽으로분배될때 스트랜드의경로를가로질러앞 뒤로유동체또는유동체섬유를움직이게하며, 격리된스트랜드상에필라멘트의모두를실제적으로포착(capturing)하며, 그리고어떤경우에스트랜드를접착하기위해유동체가코팅된스트랜드를기초재에접착시킴에의해서이루어진다. 유동체섬유는모든측부를유동체로적어도부분적으로코팅하기위해스트랜드의경로를가로질러대향측부를넘어앞 뒤로흔들린다. 신체상의유체흡수위생물품에서, 상기방법은, 섬유의딱딱해짐및 흡습력의손실을실제적으로줄이며, 섬유의균일한다발묶음, 최적의유체흡수, 및편안함을보장하기위해스트랜드의축 방향치수를따라실제적으로균일하게접착을제공한다.
    • 8. 发明公开
    • 항균성 폴리올레핀계 단섬유 및 이의 제조방법과 이를이용한 서멀본드 부직포
    • 抗真菌聚酯纤维及其制造方法和使用其的热粘合非织造布
    • KR1020080054937A
    • 2008-06-19
    • KR1020060127644
    • 2006-12-14
    • 코오롱글로텍주식회사
    • 김기연이상원신도수서은교이원열
    • D01F6/30D01D11/06D06M11/42D01F1/10D02G1/12
    • D01F6/30D01D11/06D01F1/10D02G1/12D06M11/42
    • An antifungal polyolefin staple fiber, a fabricating method thereof and a thermal bonding non-woven cloth by using the same are provided to have the properties of matter and to maintain the general properties of matter of the fiber and non-woven cloth. A polyolefin group resin is melted. Thereafter, the melted thing is spun at the spinning temperature of about 250 degrees in centigrade by the speed of about 1,500 to 2,000 m/min. The spun non-twisted yarn is drafted by the draft ratio of 1.35 to 1.65 at the pre-heat temperature of 50 to 80 degrees in centigrade. Thereafter, the winding shaft is offered to the drafted filament. Thereafter, in a surface treatment process, the liquid resin having the functional spinning emulsion and silver nano particles is injected to the filament with the winding shaft and solidified. After the heat fixation of the surface-treated filament, the filament is cut by a predetermined length. The polyolefin group resin is the antibacterial polyolefin group signal fiber as the homo polypropylene.
    • 提供抗真菌聚烯烃短纤维,其制造方法和通过使用它们的热粘合无纺布具有物质的性质并保持纤维和无纺布的物质的一般性质。 聚烯烃类树脂被熔化。 此后,熔化的物质以约250摄氏度的纺丝温度旋转约1500-2,000m / min的速度。 纺丝非加捻纱线在加热温度为50至80摄氏度的牵伸比为1.35至1.65的条件下起草。 此后,卷绕轴被提供到牵伸的长丝。 然后,在表面处理工序中,将具有功能纺丝乳液和银纳米粒子的液状树脂用卷绕轴注入长丝并固化。 在表面处理的细丝的热固化之后,将细丝切割预定长度。 聚烯烃类树脂是作为均聚丙烯的抗菌聚烯烃基团信号纤维。