    • 3. 发明公开
    • 경량성 피혁의 제조 방법.
    • 生产轻量皮革的方法
    • KR1020000074426A
    • 2000-12-15
    • KR1019990018346
    • 1999-05-17
    • 한국신발피혁연구원주식회사 해성기업
    • 김원주김상철신수범고재용
    • C14B1/20
    • C14C1/08C14C3/06
    • PURPOSE: Provided is a process for producing light weight leather, which has the excellent sense of wearing, activity and functional property, and is applicable for in shoes, clothes and bags, and then the process is simple, and then density is low without being changed property of natural leather. CONSTITUTION: The process comprises the steps of: i) adding one or mixture of 0.1-10% of a nitrogen deliming agent and 0.1-3.0% of a nitrogen free deliming agent to a pelt, and deliming the pelt for 10-240min in a drum; ii) adding 0.1-3.0% of protease to in the drum, and rotating it to remove unstructured protein and fat for 10-180min; iii) adding 1.0-2.0% of chrome sulfate powder, 0.1-3.0% of a tanning branching agent and 0.1-1.5% of a basicity synergist, and tanning it for 1-10hrs.; iv) adding 1.0-2.0% of chrome powder to the tanned leather to neutralize, followed by applying 0.1-3.0% an acid bating agent for 10-120min.; v) mixing 0.1-10.0% of an acrylic synthetic tanning agent, 0.1-10% of a polymer tanning agent and 0.1-3% of a polyurethane binder, and dye-branching it for 10-240min.; and then vi) coating it with a top-coating.
    • 目的:提供轻质皮革的制造工艺,具有优异的穿着感,活性和功能性,适用于鞋,衣服和袋子,然后工艺简单,密度低,无 改变天然皮革的属性。 构成:该方法包括以下步骤:i)向皮毛中加入0.1-10%的氮气分离剂和0.1-3.0%的无氮分离剂的一种或混合物,并将毛皮分离10-240分钟 鼓; ii)在滚筒中加入0.1-3.0%的蛋白酶,旋转它去除非结构蛋白质和脂肪10-180分钟; iii)加入1.0-2.0%的硫酸铬粉末,0.1-3.0%的鞣制支化剂和0.1-1.5%的碱性增效剂,并将其鞣制1-10小时。 iv)向鞣制的皮革中加入1.0-2.0%的铬粉末中和,然后加入0.1-3.0%的酸化剂10-120分钟。 v)混合0.1-10.0%的丙烯酸合成鞣剂,0.1-10%的聚合物鞣剂和0.1-3%的聚氨酯粘合剂,并将其分支10-240分钟。 然后vi)用顶涂层涂布。