    • 4. 发明授权
    • 코팅사용 조성물
    • 涂料组合物
    • KR101711573B1
    • 2017-03-02
    • KR1020150093884
    • 2015-07-01
    • 도맥 유한회사
    • 오귀환
    • D06M15/19D06M11/00D02G3/36D06B3/04D03D15/00D03D1/00
    • D02G3/36D06B3/04D06M11/00D06M15/19
    • 본발명은코팅사용조성물에관한것으로, 더욱상세하게는열가소성수지, 규산나트륨, 규산칼륨, 내부에진공상태의중공을포함하는구 형상의세라믹분말및 알칼리화합물을포함하는코팅사용조성물, 이를포함하는코팅사및 제품에관한것이다. 본발명은원사와의접착강도가우수하고난연성, 내열성, 흡음성, 단열성, 내구성등이우수한코팅사용조성물을제공할수 있다. 또한본 발명은촉감이탁월하고난연성, 내열성, 흡음성, 단열성, 내구성및 내오염성이우수하여벽지, 바닥재, 자동차내장재, 블라인드, 인테리어소재등에사용될수 있는코팅사를제공할수 있다.
    • 更具体地说,本发明涉及包含热塑性树脂,硅酸钠,硅酸钾,在其内部包含真空的球形陶瓷粉末和碱性化合物的涂料组合物, 涂层纱线和物品。 本发明所用的粘合强度的光纤之间提供一种阻燃性优异,使用耐热涂层是优异的,吸声,隔热性,耐久性,等等的组合物。 在另一个方面,本发明可以提供经涂覆的纱线,其可以通过触摸被使用优良,并且阻燃性,耐热性,吸声,隔热性,耐久性和耐污染性yiwoosu壁纸,地板,汽车内部装饰材料,窗帘,室内材料或类似物。
    • 9. 发明授权
    • 황토 부직포 제조방법 및 이를 이용한 침구류
    • 黄土无纺布的制作方法和使用相同的床上用品
    • KR101447647B1
    • 2014-10-07
    • KR1020140064796
    • 2014-05-29
    • 송민호배종훈
    • 송민호배종훈
    • D04H1/488D04H1/60D04H1/425D04H1/435D04H13/00
    • D04H1/60D01G13/00D01G15/00D04H1/425D04H1/435D04H1/4374D04H1/498D04H13/00D06M11/00D10B2401/13D10B2503/06
    • The present invention relates to a manufacturing method of a yellow soil non-woven fabric and bedding using the same and, more specifically, to manufacture a yellow soil non-woven fabric having excellent thermal insulation and excellent effects of keeping warm, wherein an impurity and a toxic substance are removed by processing a raw material mixed with corn and soybeans or wheat, polyester in yellow soil water and pressing the resultant into three folds, and to manufacture a variety of bedding using the manufactured yellow soil non-woven fabric. According to the present invention, a manufacturing method of a yellow soil non-woven fabric includes: a blending step blending raw materials of 60-70 parts by weight of corn, 30-40 parts by weight of any one material selected from soybean or wheat, 10-20 parts by weight of polyester, and 10-20 parts by weight of a cotton swab; a mixing step putting and evenly mixing the blended raw material in a mixing tank; a carding step continuously dusting the mixed raw material off with a carding device and rolling the mixed raw material thin; a molding step forming a web with the carded raw material in a continuous state to each other to mold the carded raw material into a non-woven fabric; a yellow soil preparation step mixing 60-70 parts by weight of water and 30-40 parts by weight of yellow soil gathered as a fine particle by ten times of a wicker tray process and precipitating the mixed resultant for 24 hours; a manufacturing step passing the molded non-woven fabric through a ready-yellow soil water to manufacture a yellow soil coated non-woven fabric; a drying step removing moisture from the yellow soil coated non-woven fabric at high temperatures of 200-230°C for 30 minutes; a cutting step cutting the dried yellow soil non-woven fabric into a certain size with a cutter; a compressing step compressing the cut yellow soil non-woven fabric in a molding compressor; and a pressing step applying an adhesive to the compressed yellow soil non-woven fabric and laminating three folds of the soil non-woven fabric to perform pressing.
    • 本发明涉及一种黄土无纺织物的制造方法和使用该方法的床上用品,更具体地说,涉及制造具有优异绝热性和优良保暖效果的黄土无纺织物,其中杂质和 通过加工与玉米和大豆或小麦混合的原料,在黄土壤水中的聚酯,并将所得物压成三层,并使用制造的黄土无纺织物制造各种床上用物去除有毒物质。 根据本发明,黄土无纺织物的制造方法包括:混合60-70重量份玉米原料,30-40重量份选自大豆或小麦的任何一种材料的混合步​​骤 ,10-20重量份的聚酯和10-20重量份的棉签; 将混合原料均匀混合在混合槽中的混合步骤; 梳理步骤用梳理装置连续地将混合的原料粉碎并将混合的原料薄化; 成型步骤,将梳理的原料彼此连续地形成,将梳理的原料模塑成无纺布; 黄土制备步骤将60-70重量份的水和30-40重量份作为细颗粒聚集的黄土浸入10倍的柳条盘中,并将混合的产物沉淀24小时; 制造步骤使成型的无纺织物通过现成黄色的土壤水,以制造黄土涂布的无纺织物; 干燥步骤,在200-230℃的高温下从黄土涂布的无纺布中除去水分30分钟; 切割步骤用切割机将干燥的黄土无纺布切成一定尺寸; 在成型压缩机中压缩切割的黄色土壤无纺织物的压缩步骤; 以及对压缩的黄土无纺布施加粘合剂并层压三层土壤无纺织物以进行压制的压制步骤。