    • 4. 发明授权
    • 녹색발광 형광체 및 그것을 사용한 브라운관
    • 绿色发光荧光体和使用其的阴极射线管
    • KR1019930006932B1
    • 1993-07-24
    • KR1019900006751
    • 1990-05-11
    • 삼성에스디아이 주식회사
    • 양준모김민수김우찬
    • C09K11/77
    • C09K11/7774C09K11/595C09K11/7755C09K11/777H01J29/187
    • The green light-emitting fluorescent material for a projection type braun tube is mfd. by mixing LaOCl:Tb fluorescent material (A) with Y3(Al,Ga)5O12:Tb fluorescent material (B) and Zn2SiO4:Mn fluorescent material (C), (B) and InBO3:Tb fluorescent material (D), or (C) and (D). The material (A) is mfd. by mixing La2O3, NH4Cl and Tb4O7, and then firing the mixt. at 400-500 deg.C for 1 hr. and at 1050-1150 deg.C for 2 hr. The material (B) is mfd. by mixing Y2O3, Al2O3, Ga2O3 and Tb4O7 with BaF or BaCl2, and then firing the mixt. at 1450-1550 deg.C for 1-3 hr. The green fluorescent material has an improved color purity and luminance.
    • 用于投影式布朗管的绿色发光荧光材料是mfd。 通过将LaOCl:Tb荧光材料(A)与Y3(Al,Ga)5O12:Tb荧光材料(B)和Zn2SiO4:Mn荧光材料(C),(B)和InBO3:Tb荧光材料(D)或( C)和(D)。 材料(A)是mfd。 通过混合La2O3,NH4Cl和Tb4O7,然后焙烧混合物。 在400-500℃下1小时。 并在1050-1150℃下搅拌2小时。 材料(B)是mfd。 通过将Y 2 O 3,Al 2 O 3,Ga 2 O 3和Tb 4 O 7与BaF或BaCl 2混合,然后烧结混合物。 在1450-1550℃下1-3小时。 绿色荧光材料具有改善的色纯度和亮度。