    • 1. 发明授权
    • 균열저항성이 우수한 고강도 수밀성 폴리머 개질 매크로파이버 콘크리트 조성물 및 이를 이용한 포장 시공 방법
    • 具有优异抗裂性,高强度和水强度的聚碳酸酯聚合物改性混凝土组合物,以及使用它的构造方法
    • KR101294796B1
    • 2013-08-08
    • KR1020130020654
    • 2013-02-26
    • 태륭건설(주)이영남정영준
    • 이영남정영준
    • C04B14/02C04B24/24C04B14/38C04B18/04
    • Y02A30/336Y02W30/91C04B24/2641C04B16/0633C04B18/146C04B28/04C04B2103/0065C04B2103/302C04B2111/343C04B2201/50E01C7/14E01C19/02
    • PURPOSE: A concrete composition of high intensity waterproofness polymer reforming macro fiber is characterized in excellent crack resistance. CONSTITUTION: A concrete composition of high intensity waterproofness polymer reforming macro fiber with excellent crack resistance comprises 8-25% by weight of cementation ash, 24-50% by weight of fine aggregate, 25-40% by weight of coarse aggregate, 2-8% by weight of water, 0.1-5% by weight of polymer emulsion, 01.-2% by weight of macro fiber, 0.1-4% by weight of water reducing agent as an admixture and 0.1-2% by weight of air controller. The glass transition temperature (Tg) of the polymer emulsion is within the range of -20 to 15 degree C and the weight ratio (P/C) of the solid content to the cement is within the range of 3-6%. The length of the macro fiber is within the range of 40-100 according to the length to diameter (L/D). The cementation ash includes 10-30 parts by mass of one or two admixtures selected from silica fume or blast furnace slag based on 100 parts by mass of the cementation ash. [Reference numerals] (S10) Cutting and cleaning; (S20) Maintaining state of wet; (S30) Calibration; (S40) Producing concrete; (S50) Pulling concrete; (S60) Tinning, curing and opening
    • 目的:高强度防水聚合物重整大分子纤维的具体组成特征在于优异的抗裂性。 构成:具有优异的抗裂性的高强度防水聚合物重整大分子纤维的具体组成包括8-25%重量的胶结灰,24-50%重量的细骨料,25-40%重量的粗骨料,2- 8重量%的水,0.1-5重量%的聚合物乳液,0.1-2重量%的大纤维,0.1-4重量%的减水剂作为混合物和0.1-2重量%的空气 控制器。 聚合物乳液的玻璃化转变温度(Tg)在-20〜15℃的范围内,固体成分与水泥的重量比(P / C)在3-6%的范围内。 根据长径比(L / D),宏观纤维的长度在40-100范围内。 基于100质量份的固井灰,固化灰含有10-30质量份选自硅粉或高炉矿渣的一种或两种混合物。 (附图标记)(S10)切割清洗; (S20)保持湿润状态; (S30)校准; (S40)生产混凝土; (S50)拉混凝土; (S60)镀锡,固化和开口
    • 2. 发明授权
    • 균열저항성이 우수한 초조강 수밀성 폴리머 개질 매크로파이버 콘크리트 조성물 및 이를 이용한 포장 시공 방법
    • 具有优异抗裂性和耐水性的高强度聚合物聚合物改性混凝土组合物,以及使用它的构造方法
    • KR101361833B1
    • 2014-02-11
    • KR1020130091443
    • 2013-08-01
    • 이영남윤문호정영준
    • 이영남윤문호정영준
    • C04B24/24C04B28/14C04B28/24C04B16/06
    • Y02A30/336C04B24/2641C04B16/0633C04B18/146C04B28/02C04B2103/0065C04B2103/20C04B2103/302C04B2111/72E01C7/12E01C11/005
    • The present invention is a polymer modified concrete pavement construction using this composition and method, in which the cement binder from 5 to 23% by weight, 32 to 45% by weight of fine aggregate, coarse aggregate, 28 to 44 wt%, 1 to 7% by weight of water, polymer emulsion 0.1 to 5% by weight, 0.1-2 % by weight of the macro fiber, 0.1 to 3% by weight of a water reducing agent as an admixture, wherein the cement binder is a cement steel of 50 to 80% by weight, of calcium aluminate of 0.1 to 40% by weight of sulfo, plaster 1 to 15% by weight, 0.1 to 5% by weight of an alkali silicate composition which is excellent in crack resistance fret steel watertight concrete composition and a polymer -modified fiber macro pavement construction using this method. according to the present invention, the cement binding agent in the polymer emulsion and Macro mix the proper amount of fiber concrete has excellent crack resistance and stiffness of Joe, the construction period is greatly shortened, and have improved water tightness, improved physical properties, as well as various basic field macro placed in continuous fiber supply to the connected mixer materials used for the continuous installation of each mixer can be supplied uniformly to a continuous, on-site production and laying of the concrete finishing process such as a serial number, and seek to the continuity, workability is improved, and a constant quality can be assured. [Reference numerals] (S10) Cutting and cleaning step; (S20) Wet state keeping step; (S30) Investing and correcting step; (S40) Concrete producing step; (S50) Concrete paving step; (S60) Tining, curing and opening
    • 本发明是一种使用该组合物和方法的聚合物改性混凝土路面结构,其中水泥粘结剂为5〜23重量%,32〜45重量%的细骨料,粗骨料,28〜44重量%,1〜 7重量%的水,聚合物乳液0.1〜5重量%,0.1〜2重量%的大纤维,0.1〜3重量%的减水剂作为混合物,其中水泥粘合剂为水泥钢 50〜80重量%的0.1〜40重量%的硫酸钙,1〜15重量%的石膏,0.1〜5重量%的耐裂纹钢水密混凝土的碱性硅酸盐组合物 组合物和使用该方法的聚合物改性的纤维宏观路面施工。 根据本发明,聚合物乳液中的水泥粘合剂和Macro混合适量的纤维混凝土具有优异的抗裂性和刚度,施工周期大大缩短,具有改善的防水性,物理性能改善, 以及为了连续安装每个混合器所使用的连接的混合器材料连续供应纤维的各种基本现场宏可以均匀地提供给连续的,现场的生产和铺设诸如序列号的混凝土整理过程,以及 寻求连续性,可操作性得到改善,可以保证质量的不变。 (附图标记)(S10)切割和清洁步骤; (S20)湿态保持步骤; (S30)投资纠正措施; (S40)混凝土生产步骤; (S50)混凝土铺路步骤; (S60)定型,固化和打开
    • 3. 发明授权
    • 균열저항성이 우수한 조강 수밀성 폴리머 개질 매크로파이버 콘크리트 조성물 및 이를 이용한 포장 시공 방법
    • 高强度聚合物改性混凝土组合物具有优异的抗裂性和耐水性,并且使用该方法构建了铺设方法
    • KR101361832B1
    • 2014-02-11
    • KR1020130091442
    • 2013-08-01
    • 이영남윤문호정영준
    • 이영남윤문호정영준
    • C04B28/22C04B28/30C04B26/02E01C7/14
    • Y02A30/336C04B24/2641C04B7/32C04B16/0633C04B22/0093C04B22/143C04B28/04C04B2103/0065C04B2111/0075C04B2111/343E01C7/12
    • The present invention is a polymer modified concrete pavement construction using this composition and method, in which the cement binder from 5 to 23% by weight, 32 to 45% by weight of fine aggregate, coarse aggregate, 28 to 44 wt%, 1 to 7% by weight of water, polymer emulsion 0.1 to 5% by weight, 0.1-2 % by weight of the macro fiber, 0.1 to 3% by weight of a water reducing agent as an admixture, wherein the cement binder is usually 50 to 80% by weight of Portland cement, magnesium aluminate, 0.1 to 30 wt% sulfonate, anhydrous 0.1 to 15% by weight of gypsum, alumina cement and from 0.01 to 10% by weight of calcium aluminate of 0.1 to 15 % by weight of the composition is excellent in crack resistance of the steel fiber concrete composition and the water-tightness polymer Modification macro this construction provides a method of using the package of this invention According to the macro fiber cement binder polymer emulsion mixed with an appropriate amount of concrete has excellent crack resistance and stiffness of Joe, the construction period is greatly shortened, and the tightness has improved, the basic prerequisite properties to be improved, as well as placed in the field a continuous supply to the connected mixer install fiber to each macro uses material uniformly continuous mixer, continuous supply and laying of concrete finishing, such as a series of on-site production and seek to the continuity of the process can be improved workability, constant quality can be assured. [Reference numerals] (S10) Cutting and cleaning step; (S20) Wet state keeping step; (S30) Investing and correcting step; (S40) Concrete producing step; (S50) Concrete paving step; (S60) Tining, Curing and Opening
    • 本发明是一种使用该组合物和方法的聚合物改性混凝土路面结构,其中水泥粘结剂为5〜23重量%,32〜45重量%的细骨料,粗骨料,28〜44重量%,1〜 7重量%的水,聚合物乳液0.1〜5重量%,0.1〜2重量%的大纤维,0.1〜3重量%的减水剂作为混合物,其中,水泥粘合剂通常为50〜 80重量%的波特兰水泥,铝酸镁,0.1至30重量%磺酸盐,无水0.1至15重量%的石膏,氧化铝水泥和0.01至10重量%的0.1至15重量%的铝酸钙, 钢纤维混凝土组合物和水密性聚合物的组合物的抗裂性优异改性宏观该构造提供了使用本发明包装的方法根据大纤维水泥粘合剂聚合物乳液与适量的混凝土混合物具有优异的 裂缝 Joe的阻力和刚度,施工期大大缩短,密封性有所提高,基本要求性能得到提高,并且在现场连续供应连接的混合器,每个宏安装纤维均匀连续使用材料 搅拌机,连续供应和铺设混凝土整理,如一系列现场生产和寻求连续性的工艺可以提高可加工性,可以保证质量的一致。 (附图标记)(S10)切割和清洁步骤; (S20)湿态保持步骤; (S30)投资纠正措施; (S40)混凝土生产步骤; (S50)混凝土铺路步骤; (S60)定型,固化和开放
    • 4. 发明授权
    • 균열저항성이 우수한 초속경 수밀성 폴리머 개질 매크로파이버 콘크리트 조성물 및 이를 이용한 포장 시공 방법
    • 非常早期的强度聚合物改性混凝土组合物具有优异的抗裂性和耐水性,并且使用它的构造方法
    • KR101294797B1
    • 2013-08-08
    • KR1020130020655
    • 2013-02-26
    • 이영남윤문호정영준
    • 이영남윤문호정영준
    • C04B24/24C04B26/06C04B16/06E01C3/02
    • Y02A30/336C04B24/2641C04B16/0633C04B28/04C04B2103/0065C04B2103/20C04B2103/302C04B2103/304C04B2111/343E01C7/12E01C11/005
    • PURPOSE: A concrete composition of rapid hardening waterproofness polymer reforming macro fiber is characterized in excellent crack resistance. CONSTITUTION: A concrete composition of rapid hardening waterproofness polymer reforming macro fiber with excellent crack resistance comprises 5-23% by weight of cementation ash, 32-35% by weight of fine aggregate, 28-44% by weight of coarse aggregate, 1-7% by weight of water, 01.-5% by weight of polymer emulsion, 0.1-2% by weight of macro fiber, 0.1-3% by weight of water reducing agent as an admixture and 0.1-2% by weight of air controller. The glass transition temperature of the polymer emulsion is within the range of -20-15°C and the weight ratio (P/C) of the solid content to the cement is within the range of 3-6%. The length of the macro fiber is within the range of 40-100 according to the length to diameter (L/D). The water reducing agent is a polycarboxylic acid based high functional water reducing agent. The air controller is a silicon based or an alcohol based air controller. [Reference numerals] (S10) Cutting and cleaning; (S20) Maintaining state of wet; (S30) Calibrating; (S40) Producing concrete; (S50) Pulling concrete; (S60) Tinning, curing and opening
    • 目的:快速硬化防水聚合物改性大分子纤维的具体组成特点是优良的抗裂性。 构成:具有优异抗裂性的快速硬化防水聚合物改性大分子纤维的混凝土组合物包含5-23%重量的胶结灰,32-35%重量的细骨料,28-44%重量的粗骨料,1- 7重量%的水,0.1-5重量%的聚合物乳液,0.1-2重量%的大纤维,0.1-3重量%的减水剂作为混合物和0.1-2重量%的空气 控制器。 聚合物乳液的玻璃化转变温度在-20〜15℃的范围内,固体成分与水泥的重量比(P / C)在3-6%的范围内。 根据长径比(L / D),宏观纤维的长度在40-100范围内。 减水剂是基于多元羧酸的高官能度减水剂。 空气控制器是基于硅的或基于醇的空气控制器。 (附图标记)(S10)切割清洗; (S20)保持湿润状态; (S30)校准; (S40)生产混凝土; (S50)拉混凝土; (S60)镀锡,固化和开口
    • 5. 发明公开
    • 불 투수 아스팔트 혼합물과 그리드를 이용한 도로 L형 측구 시공방법
    • 使用网格方法的不正确的沥青和路面L形形状的GUTTER安装
    • KR1020160010126A
    • 2016-01-27
    • KR1020140091064
    • 2014-07-18
    • 태륭건설(주)
    • 이영남정영준
    • E01C11/22E01C19/52
    • E01C11/221E01C11/24E01C19/52
    • 본발명은도로의경계블록일측에설치되는 L형측구에관한것으로서, 더욱상세하게는기층또는콘크리트층위에프라이머를적용하여 1차그리드를설치하는단계: 아스팔트혼합물을현장에적용하여쿠커에서 30분~120분동안쿠킹하는단계; 상기쿠킹된아스팔트혼합물을 1차그리드를설치한후 중간층의불 투수아스팔트혼합물을설치하는단계; 상기중간층의불 투수아스팔트혼합물을설치한후 그상면에 2차그리드를설치하는단계; 상기 2차그리드를설치한후 표층아스팔트혼합물을설치하는단계; 상기표층아스팔트혼합물을설치한상면에미끄럼방지골재를포설하고압착하는단계로이루어지는것으로본 발명은도로와의연결부위인 L형측구에서발생할수 있는겨울철동결및 환경오염물질로부터도로포장구조물과인도를보호할수 있도록함으로도로의파손을막고도로의관리비용을줄일수 있도록한 불투수아스팔트와그리드를이용한도로 L형측구설치방법에관한것이다.
    • 本发明涉及一种安装在道路边界块一侧的L形沟槽,更具体地说,涉及使用不透水沥青和网格在道路上安装L形沟槽的方法。 使用不透水沥青和网格在道路上安装L形沟槽的方法包括:将底漆施加到基层或混凝土层以安装第一格栅的步骤; 将沥青混合物施加到位置以在炊具中烹饪沥青混合物30-120分钟的步骤; 将煮熟的沥青混合物安装在第一格架上,然后安装中间层的不透水沥青混合物的步骤; 在安装中层不渗透沥青混合料之后,在不渗透沥青混合料的上表面安装第二格栅; 在安装第二格栅之后安装表层沥青混合料的步骤; 以及在安装的表面层沥青混合料的上表面上安装防滑集料的步骤,并压缩防滑剂。 本发明在冬季保护道路路面结构和人行道免受冻结,并且在连接到道路的部分的L形沟槽中可能发生的环境污染物,以防止道路损坏并减少道路管理费用。
    • 6. 发明授权
    • 줄눈부 보수용 진공 흡입장치 및 이를 이용한 줄눈부 보수공법
    • 用于修理部件的真空吸尘机和使用其的维修部件的维修方法
    • KR101319394B1
    • 2013-10-17
    • KR1020120012185
    • 2012-02-07
    • 태륭건설(주)
    • 이영남
    • E01C23/09
    • 본 발명은 스태플철근 삽입홈을 용이하게 천공할 수 있도록 하는 줄눈부 보수용 진공 흡입장치에 관한 것으로, 수분을 포함한 슬러지를 수용할 수 있는 일정한 수용공간을 구비하고 상기 수분을 외부로 배출할 수 있는 수분배출부가 형성된 수용탱크와; 상기 수용탱크의 일측과 연결되어 외부의 슬러지를 상기 수용공간으로 흡입할 수 있도록 하는 흡입력을 발생시키는 진공형성부와; 상기 수용탱크의 타측과 연결되어 상기 진공형성부에서 발생된 흡입력을 이용하여 외부의 슬러지가 상기 수용공간으로 흡입되는 통로를 형성하는 흡입부를; 포함하여 구성됨으로써, 줄눈부 컷팅 홈에 쌓이는 슬러지를 신속하고 효과적으로 제거하여 차량이나 혹은 보행자가 공사 현장 주변을 편리하게 통행할 수 있도록 함과 동시에 줄눈부 보수작업이 진행되는 주변 환경을 쾌적하게 유지할 수 있도록 하는 효과가 있다.
    • 7. 发明授权
    • 줄눈부 보수용 천공장치 및 이를 이용한 줄눈부 보수공법
    • 用于维修报废部件的钻孔机和维修部件的修理方法
    • KR101294273B1
    • 2013-08-07
    • KR1020110133161
    • 2011-12-12
    • 태륭건설(주)
    • 이영남
    • E04G23/02E04B1/682
    • 본 발명은 스태플철근 삽입홈을 용이하게 천공할 수 있도록 하는 줄눈부 보수용 천공장치에 관한 것으로, 높이 방향을 따라 일정 간격으로 이격 배치되는 상부플레이트 및 하부플레이트와, 상기 상부플레이트 및 하부플레이트가 일정 간격 이격되도록 상기 상부플레이트 및 하부플레이트에 결합되는 프레임을 포함한 본체부와; 상기 상부플레이트와 상기 하부플레이트 사이에 그 높이 방향을 따라 이동가능하게 배치되어 콘크리트 포장의 절삭부위를 선택적으로 천공하는 천공부와; 상기 본체부가 상기 콘크리트 포장의 절삭부위를 따라 이동되도록 하는 이동부를 포함하여 구성됨으로써, 절삭면에 대해서 수직으로 천공 작업이 이루어지도록 하여 스태플 철근이 뒤틀림 없이 삽입될 수 있도록 함과 동시에 천공 깊이 조절 및 간격 조절이 가능하도록 함으로써 설계된 위치에 소정의 깊이로 스태플 철근이 삽입될 수 있도록 하여 작업의 정확성 및 작업 속도를 향상시킬 수 있는 효과가 있다.
    • 10. 发明授权
    • 천연 아스팔트를 이용한 불투수성 아스팔트 포장공법 및 그 조성물
    • 使用天然FOR FOR FOR FOR FOR EN EN EN EN EN EN EN EN EN EN EN EN
    • KR101498661B1
    • 2015-03-06
    • KR1020140034940
    • 2014-03-25
    • 태륭건설(주)안수범
    • 안수범이영남정영준
    • E01C7/18C04B14/02
    • E01C7/18C04B14/02E01C7/182
    • 본 발명은 불투수성 아스팔트 포장공법에 관한 것으로서, 상세하게는 기층, 중간층, 표면층으로 구성되는 아스팔트포장공사시 중간층을 폴리머 개질 아스팔트 100에 대하여 천연 아스팔트를 30~75중량%로 혼합한 혼합액, 골재, 모래, 석회석분, 채움재를 온도170℃∼220℃에서 혼합한 불 투수 아스팔트 혼합물을 중간층에 포설하여 이루어지는 것으로 본 발명은 공극율이 0~2% 미만이고 포설시의 포설 온도가 약 160~220℃인 불 투수 아스팔트 혼합물을 제공함으로 쿠커의 사용 없이 시공하면서 Guss 또는 매스틱 아스팔트와 같은 불 투수성을 발휘하는 불 투수 아스팔트 포장공법을 제공함으로 공사기간 단축과 공사비용을 40%절감 함으로써 경제적인 효과를 얻을 수 있도록 한 천연 아스팔트를 이용한 불투수성 아스팔트 포장공법 및 그 조성물에 관한 것이다.
    • 本发明涉及使用天然沥青的不透水沥青铺装方法及其组合物。 更具体地说,在由基础路线,粘合剂路线和表面路线组成的沥青路面的施工中,粘合剂层具有不透水的沥青混合料,其中聚集体,砂,研磨石灰石,填料和混合液体,其中30 至75重量%的天然沥青与聚合物重整沥青100混合,在170-220℃下混合,将不透水沥青混合物铺在粘合剂层上。 本发明提供了一种不透水沥青混合料,其孔隙度小于0-2%,并且在约160-220℃的铺设工作中具有路面铺设温度,以便能够在不使用炊具的情况下进行施工并实现 防水性如Guss或乳香沥青。 因此,采用天然沥青的不透水沥青铺装方法及其组成降低了建设周期的40%和施工成本,从而具有经济效益。