    • 4. 发明授权
    • 콘크리트 구조물의 표면침투성 코팅보호재의 제조방법 및 그에 의해 제조된 콘크리트 구조물의 표면침투성 코팅보호재
    • 用于制造用于保护混凝土结构表面和用于保护混凝土结构表面的透明涂层材料的渗透涂层材料的方法
    • KR101685001B1
    • 2016-12-12
    • KR1020160053540
    • 2016-04-29
    • 계룡건설산업 주식회사주식회사 케이알산업주식회사트라이포드(주) 삼강기업
    • 이승찬한승구윤길호윤만수유영민박종화박상혁신장섭이재열윤현도길배수박용순강용식최재윤길민우
    • C04B41/49C04B41/48C09D4/00
    • C04B41/4905C04B41/48C09D4/00
    • 본발명은콘크리트구조물의표면침투성코팅보호재의제조방법및 그에의해제조된콘크리트구조물의표면침투성코팅보호재에관한것이다. 본발명에따른콘크리트구조물의표면침투성코팅보호재의제조방법은제1 액상을제조하는단계; 제2 액상을제조하는단계; 상기제1 액상및 제2 액상을혼합하여제3 액상을제조하는단계; 제4 액상을제조하는단계; 및상기제3 액상및 제4 액상을혼합하여제5 액상을제조하는단계를포함하되, 상기제1 액상을제조하는단계는물 70 내지 80 중량부, 유화안정제 1 내지 5 중량부, 유화제 0.5 내지 3 중량부및 카보머 10 내지 20 중량부를순서대로혼합하여형성하고, 상기제2 액상을제조하는단계는옥틸트리에톡시실란 80 내지 90 중량부, 불소실란 0.5 내지 2 중량부및 유화제 0.5 내지 3 중량부를순서대로혼합하여형성하며, 상기제1 액상및 제2 액상을혼합하여제3 액상을제조하는단계는제1 액상 60 내지 70 중량부및 제2 액상 30 내지 40 중량부의비율로혼합하여제3 액상을형성하고, 상기제4 액상을제조하는단계는물 10 내지 20 중량부, 메틸트리메톡시실란 80 내지 90 중량부및 촉매 0.1 내지 0.5 중량부를순서대로혼합하여형성하며, 상기제3 액상및 제4 액상을혼합하여제5 액상을제조하는단계는상기제3 액상 80 내지 90 중량부및 제4 액상 5 내지 10 중량부의비율로혼합하여제5 액상을형성한다. 상기한구성에의해본 발명에따른콘크리트구조물의표면침투성코팅보호재는콘크리트의구성성분과유사한무기질재료를원료로하여콘크리트구조물과의친화력을증대시킴과동시에친환경적이고, 분자량이작아콘크리트구조물의표면침투가용이하며, 콘크리트와완전한화학적복합화를이루어콘크리트구조물의열화를방지함으로써콘크리트구조물의내구성을향상시킬수 있고, 콘크리트구조물의표면침투력이우수하고안정된표층강화및 보호기능을갖는다.
    • 8. 发明公开
    • 개질 셀룰로오스계 1차 탄화물을 함유하는 친환경 모르타르 조성물
    • 环境友好的MORTAR组成包含改性的CHARCOAL
    • KR1020120092859A
    • 2012-08-22
    • KR1020110012746
    • 2011-02-14
    • 계룡건설산업 주식회사주식회사트라이포드
    • 이시구한승구윤길호윤만수이승재백종식길배수김도수박용순강용식이영석윤현도
    • C04B14/32C04B16/02C04B22/06
    • C04B14/06C04B14/322C04B16/02C04B20/04C04B22/062
    • PURPOSE: An environmentally-friendly mortar composition is provided to remove indoor harmful gas while satisfying base physical properties of the mortar composition for floors. CONSTITUTION: An environmentally-friendly mortar composition comprises 0.1-5 parts by weight of modified cellulose based primary carbide and 10-30 parts by weight of mixed solution based on 100 parts by weight of dried mortar which includes 10-50 weight% of cement and 50-90% of sand. A manufacturing method of the modified cellulose based primary carbide comprises the following steps: activating by adding the hydroxide solution to the cellulose-based primary carbide; and reacting the activated cellulose-based primary carbide with one of including fluorine, oxygen or a mixed gas of oxygen and fluorine. The concentration of the hydroxide solution is 2-8M. The activation process is performed at 700-900 deg. Celsius at a ramp-up rate of 5-10 deg. Celsius/min for 0.5-4 hours. If the activated cellulose-based primary carbide is reacted with fluorine or oxygen, the pressure of fluorine or oxygen is respectively 0.0102bar.
    • 目的:提供一种环保的砂浆组合物,用于去除室内有害气体,同时满足地板砂浆组成的基本物理性能。 构成:一种环保型砂浆组合物包含0.1-5重量份的基于改性纤维素的一次碳化物和10-30重量份的混合溶液,基于100重量份的干砂浆,其包括10-50重量%的水泥和 50-90%的沙子。 改性纤维素基一次碳化物的制造方法包括以下步骤:通过将氢氧化物溶液加入到基于纤维素的一次碳化物中来活化; 使活性纤维素类一次碳化物与氟,氧或氧和氟的混合气中的一种碳化物反应。 氢氧化物溶液的浓度为2-8M。 激活过程在700-900度进行。 摄氏度为5-10度。 摄氏度/分钟0.5-4小时。 如果活性纤维素基一次碳化物与氟或氧反应,氟或氧的压力分别为0.0102巴。