    • 1. 发明授权
    • 폐유리를 이용한 지오폴리머의 제조방법 및 그 지오폴리머를 이용한 지오콘크리트 조성물
    • 使用地质学家生产使用废物玻璃和GEO混凝土组合物的地球化学工艺
    • KR101078336B1
    • 2011-11-01
    • KR1020110052940
    • 2011-06-01
    • 주식회사 영일화성
    • 김종영이현주이충로허수현
    • C04B18/16C04B28/24C04B22/06C03C3/062
    • C04B12/005C04B28/006Y02P40/165C04B14/22C04B14/361C04B20/008
    • PURPOSE: A method for manufacturing a geopolymer and a geoconcrete composition using the waste glass are provided to recycle the waste glass as an inorganic binder for the geoconcrete composition and to improve the treating efficiency of wastes. CONSTITUTION: A method for manufacturing a geopolymer using waste glass includes the following: Waste glass is washed, dried, and pulverized. An alkaline component is introduced into the pulverized waste glass to adjust the mixing ratio of the pulverized waste glass. The waste glass with the adjusted mixing ratio is stirred to be dissolved at 60-80 rpm and at a pressure of 15-20kgf/cm^2 in order to obtain a liquid geopolymer. The waste glass with the adjusted mixing ratio includes 17.5-19.5 weight% of Na_2O+K_2O, 28-30 weight% of SiO_2, 0.5-1.2 weight% of Al_2O_3, 0.8-1.4 weight% of CaO, and 0.4-0.8 weight% of MgO. A geoconcrete composition includes 1-30 weight% of the geopolymer.
    • 目的:提供使用废玻璃制造地质聚合物和地球混凝土组合物的方法,用于将废玻璃作为地球混凝土组合物的无机粘合剂再循环,并提高废物的处理效率。 构成:使用废玻璃制造地质聚合物的方法包括:废玻璃被洗涤,干燥和粉碎。 将粉碎的废弃玻璃中的碱性成分引入粉碎废弃玻璃的混合比。 将具有调节混合比的废玻璃在60-80rpm,15-20kgf / cm 2的压力下搅拌溶解,得到液态地质聚合物。 具有调整混合比的废玻璃包括17.5-19.5重量%的Na_2O + K_2O,28-30重量%的SiO_2,0.5-1.2重量%的Al_2O_3,0.8-1.4重量%的CaO和0.4-0.8重量%的 氧化镁。 地质混凝土组合物包含1-30重量%的地质聚合物。
    • 2. 发明授权
    • 규산염을 이용한 지오폴리머의 제조방법 및 지오폴리머
    • 使用硅酸钠和地质醇生产地球物质的方法
    • KR101078335B1
    • 2011-11-01
    • KR1020110052939
    • 2011-06-01
    • 주식회사 영일화성
    • 김종영이현주이충로허수현
    • C04B28/24C04B22/14C04B22/16C04B22/06
    • C04B12/005Y02P40/165
    • PURPOSE: A method for manufacturing a geopolymer using silicate and the geopolymer are provided to fimly combine alumino silicate and a geo concrete composition by accelerating a reaction with respect to soil and sintering waste materials contained in the geo concrete composition. CONSTITUTION: A method for manufacturing a geopolymer using silicate includes the following: An aluminum silicate dispersing solution is formed by adding aluminum potassium sulfate into sodium silicate. Sodium phosphate and sodium hydroxide are added into the aluminum silicate dispersing solution. Heating, cooling, and aging processes are implemented to form a crystal nucleus. A filtering or dehydrating process is implemented to obtain phospho-aluminosilicate. The geopolymer includes 250-300 parts by weight of aluminum potassium sulfate based on 100 parts by weight of sodium silicate and 10-20 parts by weight of water based on the total mixed weight of the sodium silicate and the aluminum potassium sulfate. The phospho-aluminosilicate includes 14-16 weight% of silicon oxide, 0.5-1.5 weight% of aluminum oxide, 26-28 weight% of sodium oxide, and 2-5 weight% of phosphorus oxide.
    • 目的:提供使用硅酸盐和地质聚合物制造地质聚合物的方法,通过加速与土壤混合物组合物中包含的土壤和烧结废料的反应,将铝硅酸盐和地质混凝土组合物结合在一起。 构成:使用硅酸盐制造地质聚合物的方法包括以下:通过将硅酸钾加入硫酸铝中而形成硅酸铝分散液。 将磷酸钠和氢氧化钠加入到硅酸铝分散溶液中。 加热,冷却和老化过程被实现以形成晶核。 实施过滤或脱水工艺以获得磷酸铝硅酸盐。 基于100重量份的硅酸钠和10-20重量份的水,基于硅酸钠和硫酸铝钾的总混合重量,地质聚合物包括250-300重量份的硫酸铝钾。 磷酸铝硅酸盐包括14-16重量%的氧化硅,0.5-1.5重量%的氧化铝,26-28重量%的氧化钠和2-5重量%的氧化磷。