    • 1. 发明公开
    • 저강도 및 초속경성을 갖는 유동화 되메움재용 고화재 조성물
    • 固化剂组合物
    • KR1020130122170A
    • 2013-11-07
    • KR1020120045284
    • 2012-04-30
    • 주식회사 씨엠디기술단주식회사 대웅
    • 문경주박원춘안양진박성순음현미
    • C09K17/06C09K17/40C09K103/00
    • The present invention relates to solidified agent composition for liquefaction back filling, and more particularly, to solidified agent composition for liquefaction back filling stabilizing soil as quickly as possible by reducing the percentage of water content and removing soil pore water using cubical expansion and exothermic reaction of CaO contained in incinerlator bottom ash as a material used in construction processes where stabilized soil is manufactured by mixing a solidified agent with soil produced in the site after excavation for laying water, gas, and power transmission pipes underground in a city and then is filled and cured in the excavated part and the backside of the pipes. The solidified agent composition for liquefaction back filling in the present invention comprises 80-150 parts by weight of furnace slag powder, 40-100 parts by weight of petrol coke plaster, 5-10 parts by weight of sulphate stimulant, and 1-5 parts by weight of plasticiser powder for 100 parts by weight of paper sludge incinerlator bottom ash of which the content of CaO is 35-70%.
    • 本发明涉及用于液化回填的固化剂组合物,更具体地说,涉及用于液化反渗透稳定化土壤的固化剂组合物,通过降低含水率和除去土壤孔隙水,尽可能快地使用立方膨胀和放热反应 焚烧炉底灰中所含的CaO作为施工过程中使用的材料,其中稳定的土壤是通过混合固化剂与在开挖后生产的土壤中生产的土壤一起制造的,用于在城市地下铺设水,气体和输电管,然后填充, 在挖掘的部分和管道的背面固化。 本发明的液化回填用固化剂组合物包含80-150重量份的炉渣粉末,40-100重量份的汽油焦炭膏,5-10重量份的硫酸盐刺激剂和1-5份 100重量份的CaO含量为35-70%的纸泥焚化炉底灰。
    • 4. 发明公开
    • 저알칼리 저강도 및 초속경성을 갖는 유동화 되메움재용 고화재 조성물
    • 固化剂组合物
    • KR1020130122171A
    • 2013-11-07
    • KR1020120045285
    • 2012-04-30
    • 주식회사 씨엠디기술단주식회사 대웅
    • 문경주박원춘안양진박성순음현미
    • C09K17/06C09K17/08C09K103/00
    • The present invention relates to a solidified agent composition for liquefaction back filling and, more particularly, to a solidified agent composition for liquefaction back filling stabilizing soil as quickly as possible by reducing the percentage of water content and removing soil pore water using cubical expansion and exothermic reaction of CaO contained incinerator bottom ash as a material used in construction processes, wherein manufactured soil are insulated, for laying water, gas, and power transmission pipe underground in a city. The solidified agent composition for liquefaction back filling in the present invention comprises 20-30 parts by weight of sodium aluminium sulfate (SAS) or sodium aluminium fluoride (SAF) which are by-products from polysilicon manufacturing process, 30-50 parts by weight of furnace slag powder, 20-40 parts by weight of desulfurized gypsum in petroleum coke, 5-10 parts by weight of a sulphate stimulant, and 1-5 parts by weight of plasticizer powder for 100 parts by weight of paper sludge incinerator bottom ash of which the content of CaO is 35-70%.
    • 本发明涉及一种用于液化回填的固化剂组合物,更具体地说,涉及一种用于液化反渗透稳定土壤的固化剂组合物,其通过降低含水率和使用立方膨胀和放热来除去土壤孔隙水尽可能快 含有焚烧炉底灰的CaO作为施工过程中使用的材料,其中制造的土壤是绝缘的,用于在城市地下铺设水,气体和输电管。 本发明的液化回填用固化剂组合物包含20-30重量份作为多晶硅制造工序的副产物的硫酸铝钠(SAS)或氟化铝钠(SAF),30〜50重量份 炉渣粉末,石油焦炭中20-40重量份脱硫石膏,5-10重量份硫酸盐刺激剂和1-5重量份增塑剂粉末,用于100重量份的纸泥浆焚烧炉底灰 其中CaO的含量为35-70%。
    • 8. 发明公开
    • 광산 폐기물 및 친환경고화재를 활용한 저강도, 고유동성 광산 채굴적 충진재 조성물 제조방법 및 시스템
    • 填充剂组合物及其制法的制备方法
    • KR1020130122163A
    • 2013-11-07
    • KR1020120045273
    • 2012-04-30
    • 주식회사 씨엠디기술단
    • 문경주박원춘안양진박성순음현미
    • C04B18/04C04B22/14C04B26/04B28C3/00
    • Y02W30/91C04B18/12B28C3/00C04B18/0418C04B18/141C04B22/14C04B26/04C04B2103/44
    • The present invention relates to a method for manufacturing the low-strength, highly flowable mine goaf filling agent composition utilizing an eco-friendly solidification material as a bonding agent while utilizing mine wastes of debris, mine tailing as an aggregate and system therefor, and more specifically to a method for manufacturing the filling agent composition of a flowable concrete form and a system therefor by utilizing debris of rock and gravel forms and mine tailing as particles in the order of sand among wastes remaining after dressing valuable resources from abandoned mines in the past as an aggregate and mixing with eco-friendly solidification materials without using cement as a bonding agent. The manufacturing method for low-strength, highly flowable mine goaf filling agent according to the present invention includes; 1) a stage of preparing mine wastes with a particle size in the range of tailing 5mm~40mm and mine tailing with a particle size smaller than 5mm by crushing debris; and 2) a stage of preparing a solidification material; and 3) a stage of mixing 80~120 parts by weight of the mine tailing, 15~45 parts by weight of the solidification material. 1~5 parts by weight of the fluidization material and 1~5 parts by weight of the thickener for 100 parts by weight of the mine debris. [Reference numerals] (11,31) Debris storage;(12) Fixed quantity supplier;(13) Crusher;(14) Vibrating screen;(21) Filler storage;(22) Complex mixer;(23) Aggregate meter;(24) Fission meter;(25) Liquid meter;(32) Mine tailing storage;(33) Solidification agent storage;(34) Water-reducing agent storage;(35) Thickener storage;(AA) More than 40mm;(BB) 5-40mm;(CC) Below 5mm
    • 本发明涉及一种利用生物友好型固化材料作为粘合剂的低强度高流动性矿山填充剂组合物的制造方法,同时利用矿山废弃物,矿石尾矿作为骨料,其系统等。 具体涉及一种用于制造可流动混凝土形式的填充剂组合物的方法及其系统,其通过利用岩石和砾石形式的碎屑以及煤矿尾矿作为过去从废弃的矿井中获取有价值的资源之后剩下的废物中的沙子的粒子 作为骨料,并与环保型固化材料混合而不使用水泥作为粘合剂。 根据本发明的低强度,高流动性矿山填充剂的制造方法包括: 1)通过粉碎碎屑制备粒度在5mm〜40mm范围内的矿石废料和粒径小于5mm的矿尾矿的阶段; 和2)制备凝固材料的阶段; 和3)混合80〜120重量份的矿尾,15〜45重量份固化物的阶段。 1〜5重量份的流化材料和1〜5重量份的增稠剂用于100重量份的矿山碎片。 (11,31)碎屑储存;(12)固定量供应商;(13)破碎机;(14)振动筛;(21)填料储存;(22)复合混合器;(23)聚集计;(24 )裂变仪;(25)液体计;(32)矿尾料储存;(33)固化剂储存;(34)减水剂储存;(35)增稠剂储存;(AA)40mm以上;(BB)5 -40mm;(CC)5mm以下
    • 9. 发明公开
    • 광산 폐기물 및 친환경고화재를 활용한 저강도, 고유동성 광산 채굴적 충진재 조성물
    • 填充剂组合物
    • KR1020130122162A
    • 2013-11-07
    • KR1020120045272
    • 2012-04-30
    • 주식회사 씨엠디기술단
    • 문경주박원춘안양진박성순음현미
    • C04B18/04C04B22/14C04B26/04C04B24/00
    • Y02W30/91C04B18/12C04B18/141C04B18/241C04B22/143C04B22/148C04B26/04C04B2103/44
    • The present invention relates to mine goaf filling agent compositions with a low strength and a high flowability by utilizing mine wastes of debris, mine tailing as an aggregate and eco-friendly solidification materials as a bonding agent, and more specifically to filling material compositions having a form of concrete with flowability by utilizing debris of rock and gravel forms and mine tailings as particles in the order of sand among wastes remaining after dressing valuable resources from abandoned mines in the past as an aggregate, and mixing with eco-friendly solidification materials without using cement as a bonding agent. The low-strength, highly flowable mine goaf filling agent compositions according to the present invention comprise; 80-120 parts by weight of the mine tailing with a particle size below 5mm; and 15-45parts by weight of the solidification material; and 1-5 parts by weight of the fluidization material; and 1-5 parts by weight of the thickener for 100 parts by weight of the mine debris with a particle size in the range of 5mm-40mm.
    • 本发明涉及利用矿渣的碎片,尾矿作为骨料和环保型固化材料作为粘合剂,具有低强度和高流动性的矿山垛填充剂组合物,更具体地涉及具有 通过利用岩石和砾石形式的碎屑形式的混凝土形式和尾矿作为粒子,以过去从废弃矿山中选择有价值的资源后剩余的废物中的砂粒排列,并与环保型固化材料混合,而不使用 水泥作为粘合剂。 根据本发明的低强度,高度流动的矿山填充剂组合物包含: 80-120重量份矿石尾矿,粒度小于5mm; 和15-45重量份的固化材料; 和1-5重量份的流化材料; 和1-5重量份的增稠剂,用于100重量份的粒度在5mm-40mm范围内的矿山碎屑。
    • 10. 发明公开
    • 친환경고화재를 활용한 방초토 조성물 및 이를 이용한 시공방법
    • 环境友好的防止生长发育的土壤代谢物及其构建方法
    • KR1020130134414A
    • 2013-12-10
    • KR1020120057897
    • 2012-05-31
    • 주식회사 씨엠디기술단
    • 문경주박원춘안양진박성순음현미
    • A01G13/00A01M21/00E01C15/00
    • A01G13/00A01G13/0262A01M21/00E01C15/00
    • The present invention relates to a soil composition for preventing weed growing on the road using an environment-friendly firming agent and a method of constructing soil for preventing weed growing using the same, and, more specifically, to a soil composition for preventing weed growing in a soil-concrete form which prevents weed from producing and growing for the purpose of pedestrian's safe walk on the shoulder of the road and accident prevention by using spoil dredged from a reservoir and river and in-situ soil, and mixing an environment-friendly firming agent without using cement as a bonding agent, and a method of constructing soil for preventing weed growing using the same. The environment-friendly soil composition for preventing weed growing according to the present invention comprises 10-35 parts by weight of a firming agent to 100 parts by weight of soil and sand with a particle size of 40 mm or less, and the firming agent includes 150-250 parts by weight of blast furnace slag fine powder and 20-40 parts by weight of petrol cokes flue gas desulfurization gypsum to 100 parts by weight of the high calcium incineration residue produced in an in-furnace desulfurization type incinerator for combusting coal having 20-60% of the calcium oxide (CaO) content.
    • 本发明涉及一种用于防止杂环生长的土壤组合物,其使用环境友好的固化剂和用于防止杂草生长的土壤的施用方法,更具体地涉及用于防止杂草生长的土壤组合物 一种防止杂草生产和生长的道路,通过使用从水库和河流以及原地土壤疏浚的泥土,在道路肩膀上行走安全行走和预防事故,并混合环保型紧固 不使用水泥作为粘合剂的方法,以及使用该方法构建用于防止杂草生长的土壤的方法。 根据本发明的用于防止杂草生长的环境友好的土壤组合物包含10-35重量份的固化剂至100重量份的粒度为40mm或更小的土壤和沙子,并且固化剂包括 150-250重量份高炉矿渣细粉和20-40重量份汽油焦炭烟气脱硫石膏至100重量份在炉内脱硫型焚烧炉中生产的高钙焚烧残渣,用于燃烧煤 20-60%的氧化钙(CaO)含量。