    • D01F6/10
    • A synthetic fiber is produced by (a) mixing 100 wt.pt. polyvinyl chloride of 700-1700 polymn. degree with 2-10 wt. pt. barium stearate as a thermal stabilizer, 1-5 wt. pt. wax as an activating agent, 1-10 wt. pt. DOP as a plasticizer, 0.1-10 wt. pt. pigment, flame-retardant, antistatic agent and gas trapping agent, and 0.1-1 wt. pt. benzotriazole as a light-stabilizer in the mixer at 70-120 deg.C, (b) melt- spinning the mixt. in the extruder at 100-200 deg.C cylinder and 220-300 deg.C dice, and (C) cold-drawing and hot-drawing it at 100-130 deg.C.
    • 合成纤维通过(a)混合100重量ppm 聚氯乙烯700-1700克。 度为2-10重量% PT。 硬脂酸钡作为热稳定剂,1-5wt。 PT。 蜡作为活化剂,1-10重量份 PT。 DOP作为增塑剂,0.1-10wt。 PT。 颜料,阻燃剂,抗静电剂和气体捕获剂,和0.1-1重量% PT。 苯并三唑作为光稳定剂,在70-120℃的混合器中,(b)熔融纺丝混合物。 在挤出机中在100-200℃的圆筒和220-300℃的骰子上,(C)在100-130℃冷拔拉伸。