    • 3. 发明授权
    • 초고분자량 폴리에틸렌 섬유와 고강력 폴리에스터 섬유로 구성된 세일클로스용 코팅 원단의 제조방법
    • 包含超高分子量聚乙烯纤维和高强度聚酯纤维的涂层胶囊的制备方法
    • KR101325606B1
    • 2013-11-20
    • KR1020120068627
    • 2012-06-26
    • 영풍화성(주)다이텍연구원한국섬유개발연구원
    • 양성용양정호최송아권오병손현식민문홍심승범
    • D06M11/38D06M15/39D06C7/02D06M101/32D06M101/30
    • D06M11/38D06C7/02D06M15/39D06M2101/30D06M2101/32D10B2321/021D10B2331/04D10B2401/00
    • The present invention relates to a method for manufacturing a coated fabric for sailcloth. The coated fabric for sailcloth is manufactured by subjecting a fabric for sailcloth consisting of an ultra high-molecular polyethylene fiber and a high-strength polyester fiber to pretreatment, curing, tentering, resin coating, and thermosetting. In order to prevent the deterioration in physical properties of the ultra high-molecular weight polyethylene fiber, the curing treatment is performed at a temperature of 130-140, which is relatively lower than the curing temperature of the general high-strength polyester textile. Considering the deterioration in setting characteristics of the high-strength polyester due to the curing treatment, the width widening is minimized at the time of tentering and the thermosetting is conducted at a temperature of 100 or lower. The process for manufacturing a coated fabric for sailcloth of the present invention can effectively prevent the deterioration in physical properties of the ultra high-molecular weight polyethylene fiber contained in the coated fabric for sailcloth and effectively prevent the slow reduction in the width of the coated fabric for sailcloth during storage.
    • 本发明涉及帆布用涂布织物的制造方法。 用于帆布的涂布织物通过将由超高分子量聚乙烯纤维和高强度聚酯纤维组成的帆布织物进行预处理,固化,拉幅,树脂涂布和热固化来制造。 为了防止超高分子量聚乙烯纤维的物理性能的劣化,固化处理在相对低于一般的高强度聚酯织物的固化温度的130-140℃的温度下进行。 考虑到由于固化处理而导致的高强度聚酯的凝固特性的劣化,拉幅时的宽度变宽被最小化,并且在100℃以下的温度下进行热固化。 本发明的帆布用涂布织物的制造方法可以有效地防止包覆在织物中的超高分子量聚乙烯纤维的物理性能劣化,有效地防止了涂布织物的宽度的缓慢降低 在储存期间用于帆布。
    • 7. 发明授权
    • 다운프루프 직물용 가연복합사의 제조방법
    • 为防绒面料生产拉丝纹纱的工艺
    • KR101205666B1
    • 2012-11-27
    • KR1020110051311
    • 2011-05-30
    • 한국섬유개발연구원(주)보광다이텍연구원
    • 심승범조대현한재성최광석윤원보김동권조숙경
    • D02G1/16D01D5/30D01F8/14D02J1/22
    • PURPOSE: A method for fabricating a false twist conjugate yarn for a down proof fabric is provided to improve dye fastness and to obtain the conjugate yarn with excellent uniformity and even bulkiness. CONSTITUTION: A method for fabricating a false twist conjugate yarn for a down proof fabric comprises: a step of fusing nylon and polyester; a step of spinning the fused nylon and polyester at 275-280 deg. C and 3,000-3,500 m/min to prepare a splittable conjugate filament(1); a step of passing the conjugate filament through a first feed roller(2); a step of performing thermal treatment on the conjugate filament at 165-175 deg. C; a step of false-twisting the conjugate filament in a false-twisting ratio of 1.50-1.60, passing through a second feed roller(5), and drawing the same; and a step of treating the conjugate filament with oil and winding at 350-450 m/min.
    • 目的:提供一种用于制造用于防绒织物的假捻共轭纱的方法,以提高染色牢度,并获得具有优异均匀性和均匀度的复合纱。 构成:用于制造防倒绒织物的假捻复合纱的方法包括:将尼龙和聚酯熔合的步骤; 在275-280度纺丝熔融尼龙和聚酯的步骤。 C和3,000-3,500m / min以制备可裂合的共轭丝(1); 将复合长丝通过第一进料辊(2)的步骤; 在165-175度对共轭丝进行热处理的步骤。 C; 通过第二进料辊(5)以1.5-1.60的假捻比假捻捻合共轭丝,并将其拉伸的步骤; 以及用油处理共轭长丝并以350-450m / min卷绕的步骤。