    • 9. 发明公开
    • 내열성이 우수한 생분해성 폴리에스테르 섬유 및 이를 이용한 원단
    • 具有改善耐热性的生物可降解聚酯纤维和包含其的织物
    • KR1020150061977A
    • 2015-06-05
    • KR1020130146416
    • 2013-11-28
    • 도레이케미칼 주식회사
    • 김민웅김도현임지영
    • D01F6/62D03D15/00
    • 본발명은생분해성폴리에스테르를포함하는내열성이우수한생분해성폴리에스테르섬유및 이를이용한원단에관한것으로, 보다상세하게는생분해성을가지는동시에높은 Tg를보유함으로써내열성이향상되고방사공정이가능한내열성이우수한생분해성폴리에스테르섬유, 내열성이향상된생분해성폴리에스테르섬유를포함하는원단, 내열성이향상된폴리에스테르섬유제조용생분해성폴리에스테르조성물및 내열성이향상된생분해성폴리에스테르를포함하는섬유제조용생분해성폴리에스테르칩에관한것이다.
    • 本发明涉及具有优异耐热性的生物可降解聚酯纤维,其包括可生物降解的聚酯和使用其的织物。 更具体地说,本发明涉及耐热性优异的生物降解性聚酯纤维,其具有增强的耐热性,并且可以通过具有生物降解性和高Tg的纺丝方法使用,包含具有增强的耐热性的可生物降解的聚酯纤维的织物,可生物降解的 用于制造耐热性提高的聚酯纤维的聚酯组合物,以及用于制造具有增强的耐热性的具有可生物降解的聚酯的纤维的可生物降解的聚酯片。
    • 10. 发明公开
    • 보온성을 갖는 생분해성 중공사 및 이의 제조방법
    • 混合组合物可生物降解的中空纤维布具有热绝缘及其制备
    • KR1020130092292A
    • 2013-08-20
    • KR1020120013938
    • 2012-02-10
    • 도레이케미칼 주식회사
    • 손정아지성대김도현신동수임지영
    • D01D5/24D01F6/62
    • D01D1/02D01D5/24D01F6/62
    • PURPOSE: A biodegradable hollow fiber and a manufacturing method thereof are provided to give biodegradable polyester hollow fiber with possible spinning and improved elongation property. CONSTITUTION: A biodegradation hollow fiber having heat insulation property is a fiber manufactured by esterification and polycondensation of a mixture consisting of acid components of aliphatic acids having carboxylic acid group and aromatic acids having phenylene group, sulfonic acid metal salt, and diol components of carbon number of 2-14. A biodegradable hollow fiber manufacturing method comprises a mixing step in which aliphatic acid of 9 to 20 mole %, aromatic acid of 79 - 90 mole %, and sulfonic acid metal salt of 0.1 to 1.5 mole % are mixed together and materials including acidic components (aliphatic acid and aromatic acid) and sulfonic acid metal salt are mixed with diol components in 1.0 : 1.0-1.4 weight ratio; an esterification step which manufactures oligomer by stirring for 210 to 330 minutes at 200 to 260°C and at a speed of 40 to 80 rpm; a polyester resin manufacturing step which manufactures polyester by polycondensing above mentioned oligomer for 180 - 210 minute at 240 - 285°C and at a speed of 40 - 100rpm; and a hollow fiber manufacturing step which manufactures hollow fiber of a hollow ratio of 10-30% by spinning polyester resin.
    • 目的:提供可生物降解的中空纤维及其制造方法,以提供具有可能的纺丝和改善的伸长性能的可生物降解的聚酯中空纤维。 构成:具有隔热性的生物降解中空纤维是由具有羧酸基的脂族酸的酸成分和具有亚苯基的芳香族酸,磺酸金属盐和碳数二醇成分组成的混合物的酯化和缩聚制造的纤维 2-14岁。 可生物降解的中空纤维制造方法包括混合步骤,其中将9-20摩尔%的脂族酸,79-90摩尔%的芳族酸和0.1至1.5摩尔%的磺酸金属盐混合在一起,并将含有酸性组分的材料 脂肪酸和芳香酸)和磺酸金属盐与二醇组分以1.0:1.0-1.4的重量比混合; 酯化步骤,其通过在200至260℃和40至80rpm的速度下搅拌210至330分钟制备低聚物; 聚酯树脂制造步骤,其通过在240-285℃和40-100rpm的速度下将上述低聚物缩聚180-210分钟制造聚酯; 以及通过纺丝聚酯树脂制造中空纤维的中空纤维的中空纤维为10-30%的中空纤维制造步骤。