会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 2. 发明专利
    • Pickling method of stainless steel
    • 不锈钢切割方法
    • JP2013213239A
    • 2013-10-17
    • JP2012083050
    • 2012-03-30
    • Aichi Steel Works Ltd愛知製鋼株式会社
    • KUBOTA KAZUMASAKURIHARA NARIAKI
    • C23G1/08C23G1/36
    • PROBLEM TO BE SOLVED: To provide a pickling method for removing scales generated on a surface of stainless steel by using an acid liquid based on hydrochloric acid and for generating white color without smut adhesion.SOLUTION: A pickling method of stainless steel uses a nitrogen-less and fluorine-less mixed acid liquid comprising hydrochloric acid and hydrogen peroxide, and performs: a new liquid pickling step of performing pickling treatment by using a new liquid of the acid liquid; and a treated liquid pickling step of performing the treated liquid pickling step at least once by using the treated acid liquid which is the acid liquid after used for the pickling treatment in the new liquid pickling step.
    • 要解决的问题:提供一种通过使用基于盐酸的酸性液体除去不锈钢表面产生的鳞片并产生白色而没有污迹附着的酸洗方法。解决方案:不锈钢的酸洗方法使用氮 - 包含盐酸和过氧化氢的少量无氟混合酸性液体,并且执行:通过使用酸液的新液体进行酸洗处理的新的液体酸洗步骤; 以及处理液体酸洗步骤,通过使用在新的液体酸洗步骤中用于酸洗处理后的酸性液体处理的酸性液体进行至少一次处理的液体酸洗步骤。
    • 3. 发明专利
    • Nitrided component and method for producing the same
    • 硝基组分及其生产方法
    • JP2013087320A
    • 2013-05-13
    • JP2011228140
    • 2011-10-17
    • Aichi Steel Works Ltd愛知製鋼株式会社
    • ITO YUKIOKOZUKA TAKUMI
    • C23C8/26C21D1/06C21D3/04C21D9/00C21D9/02C21D9/30C21D9/32C22C38/00C22C38/24C22C38/54C23C8/02
    • PROBLEM TO BE SOLVED: To provide a nitrided component capable of being improved in fatigue characteristics without applying an expensive shot peening, and a method for producing the same.SOLUTION: The nitrided component includes a surface hardened layer including a decarburized layer and a nitrided layer. Chemical composition inside the nitrided component includes, by mass%, C: 0.15% or more and less than 0.5%; one or more elements selected from a group of Cr: 6.0% or less, V: 2.5% or less, Mo: 3.0% or less, and Al: 1.5% or less; N: 0.03% or less. A nitriding factor N1 expressed by (0.08×[%Cr]+0.29×[%V]+0.15×[%Mo]+0.65×[%Al])/[%C] is 1.0 or more. At the surface hardened layer, a decarburization rate expressed by (C-C)/C is 0.30 or more, wherein Cdenotes carbon concentration of the surface, and a surface nitrogen concentration factor Ns expressed by N2/(C-C+0.2) is 1.0 or more, wherein N2 denotes nitrogen concentration of the surface.
    • 解决的问题:提供能够在不施加昂贵的喷丸硬化的情况下能够改善疲劳特性的氮化组分及其制备方法。 解决方案:氮化组分包括包括脱碳层和氮化层的表面硬化层。 氮化成分中的化学成分以质量%计含有C:0.15%以上且小于0.5% 选自Cr:6.0%以下,V:2.5%以下,Mo:3.0%以下,Al:1.5%以下的一种以上的元素; N:0.03%以下。 由(0.08×[%Cr] + 0.29×[%V] + 0.15×[%Mo] + 0.65×[%Al])/ [%C]表示的氮化因子N1为1.0以上。 在表面硬化层,由(CC 1 / SB)表示的脱碳率为0.30以上,其中,C 1 表面的碳浓度和由N2 /(CC 1 +0.2)表示的表面氮浓度因子Ns为1.0以上,其中,N2表示表面的氮浓度。 版权所有(C)2013,JPO&INPIT
    • 4. 发明专利
    • Soft magnetic stainless steel for dental attachment
    • 用于牙科附件的软磁不锈钢
    • JP2013079417A
    • 2013-05-02
    • JP2011219379
    • 2011-10-03
    • Aichi Steel Works Ltd愛知製鋼株式会社
    • MOTOKURA YOSHINOBUARAI KAZUO
    • C22C38/00C22C38/28
    • PROBLEM TO BE SOLVED: To provide a soft magnetic stainless steel for a dental attachment which has magnetic properties with excellent saturation magnetic flux density Bs, while maintaining corrosion resistance equal to or higher than that of SUS316 (JIS steel) under a very severe corrosion environment, such as that in an oral cavity.SOLUTION: The soft magnetic stainless steel for a dental attachment includes, in mass ratio, 0.02% or less of C, 0.50% or less of Si, 0.40% or less of Mn, 0.015% or less of S, 14.0-18.0% of Cr, 0.3-2.5% of Mo, 0.02% or less of Al, 0.05-0.30% of Ti, 0.02% or less of N, 0.01% or less of O, and 0.05-1.00% of Sn, with the balance including Fe and impurity elements.
    • 要解决的问题:为了提供具有优异的饱和磁通密度Bs的磁性能的牙科用粘合剂的软磁性不锈钢,同时保持等于或高于SUS316(JIS钢)的耐腐蚀性, 严重的腐蚀环境,如在口腔中。 解决方案:用于牙科配件的软磁性不锈钢的质量比包括C:0.02%以下,Si:0.50%以下,Mn:0.40%以下,S:0.015%以下,14.0〜 18.0%的Cr,0.3〜2.5%的Mo,0.02%以下的Al,0.05〜0.30%的Ti,0.02%以下的N,0.01%以下的O和0.05〜1.00%的Sn, 余量包括Fe和杂质元素。 版权所有(C)2013,JPO&INPIT
    • 7. 发明专利
    • Method for manufacturing chromium-based stainless-steel reinforcing bar
    • 用于制造基于铬的不锈钢加固棒的方法
    • JP2011026686A
    • 2011-02-10
    • JP2009176378
    • 2009-07-29
    • Aichi Steel Works Ltd愛知製鋼株式会社
    • GOTO MANKEIMATSUURA KOTARONAKAGAWA HIDEKI
    • C21D9/52C21D1/26C21D6/00C22C38/00C22C38/40
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a chromium-based stainless-steel reinforcing bar, which can stably and easily manufacture the reinforcing bar so as to enter an aimed strength classification.
      SOLUTION: The method for manufacturing the chromium-based stainless-steel reinforcing bar includes: preparing a steel material including, by mass%, 0.15% or less C, 1.00% or less Si, 1.00% or less Mn, 0.040% or less P, 0.030% or less S, 0.60% or less Ni, 11.0-13.5% Cr, 0.15% or less N and the balance Fe with unavoidable impurities; hot-rolling the steel material; and annealing the hot-rolled material at a temperature of 600°C or higher and in such a condition that a tempering parameter of T(20+logt)/1,000 (T is annealing temperature (K), t is annealing period of time (hr) and log is a common logarithm) is in a range of 17.0-23.0.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 解决的问题:提供一种可以稳定且容易地制造钢筋的铬基不锈钢钢筋的制造方法,以进入目标强度分级。 解决方案:用于制造铬基不锈钢钢筋的方法包括:制备钢材,以质量%计含有0.15%以下的C,1.00%以下的Si,1.00%以下的Mn,0.040% 或更小的P,0.030%以下的S,0.60%以下的Ni,11.0〜13.5%的Cr,0.15%以下的N,余量为Fe的不可避免的杂质; 热轧钢材; 在600℃以上的温度下退火,在回火参数T(20 + logt)/ 1000(T为退火温度(K))的条件下退火,t为退火时间 hr),log为常用对数)在17.0-23.0的范围内。 版权所有(C)2011,JPO&INPIT
    • 8. 发明专利
    • lathe
    • 车床
    • JP2010228015A
    • 2010-10-14
    • JP2009075505
    • 2009-03-26
    • Aichi Steel Works Ltd愛知製鋼株式会社
    • MAETANI TETSUYA
    • B23B31/10B23B31/02
    • PROBLEM TO BE SOLVED: To provide a lathe which eliminates the need of adjusting a weight even when two types of eccentric workpieces with different eccentric positions are treated alternately and has superior machining accuracy. SOLUTION: A chuck 4 is provided with four clampers 3a-3d. A first eccentric workpiece 2a is affixed to the chuck 4 using the first clamper 3a and the second clamper 3b. Also, a second eccentric workpiece 2b is affixed to the chuck 4 using the third clamper 3c and the fourth clamper 3d. The eccentric workpiece 2 is affixed using two clampers 3 among the four clampers 3a-3d, and the chuck 4 is axially rotated together with the eccentric workpiece 2. The two clampers 3 to which the eccentric workpiece 2 is not affixed keeps the weight balance between the eccentric workpiece 2 and the chuck 4 since an arm 6 is rotated a predetermined angle about a rotating shaft 5 by the centrifugal force. COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:即使当具有不同偏心位置的两种类型的偏心工件被交替地处理并且具有优异的加工精度时,提供一种不需要调整重量的车床。 解决方案:卡盘4设有四个夹具3a-3d。 使用第一夹持器3a和第二夹持器3b将第一偏心工件2a固定到卡盘4。 此外,第二偏心工件2b使用第三夹持器3c和第四夹持器3d固定到卡盘4。 偏心工件2使用四个夹紧器3a-3d中的两个夹持器3固定,并且卡盘4与偏心工件2一起轴向旋转。偏心工件2未被固定的两个夹紧器3保持其间的重量平衡 偏心工件2和卡盘4,因为臂6通过离心力绕旋转轴5旋转预定角度。 版权所有(C)2011,JPO&INPIT
    • 9. 发明专利
    • Component for machine structure and method for producing the same
    • 机械结构部件及其制造方法
    • JP2010167492A
    • 2010-08-05
    • JP2009244295
    • 2009-10-23
    • Aichi Steel Works Ltd愛知製鋼株式会社
    • ITO YUKIONISHIKAWA TOMOAKIKOZUKA TAKUMI
    • B23K35/30B23K9/00B23K9/04B23K9/167B23K10/02B23K26/34
    • PROBLEM TO BE SOLVED: To provide a component for a machine structure which has rigidity effectively increased by a simple method, and to provide a method for producing the same. SOLUTION: The component for a machine structure comprises: a base material 2 composed of a steel material; and an overlay weld zone 3 provided with one or a plurality of overlay weld layers 31 formed by feeding a raw material for overlay welding to the surface 20 of the base material 2 and performing welding. Each overlay weld layer 31 is composed of a high rigidity steel obtained by dispersing boride including one or more elements selected from the group 4A, 5A and 6A elements and Fe or/and the composite thereof into a matrix phase composed of pure iron or an iron alloy in an amount of 10 to 70% by volume ratio, and the overlay weld layer 31 has a Young's modulus higher than that of the base material 2. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种通过简单的方法有效提高刚性的机器结构的部件,并提供其制造方法。 解决方案:机器结构的部件包括:由钢材构成的基材2; 以及设置有通过将基材2的表面20供给用于覆盖焊接的原料进行焊接而形成的一个或多个重叠焊接层31的覆盖焊接区域3。 每个覆盖层31由通过将包含选自4A,5A和6A族元素中的一种或多种元素的硼化物和Fe或其复合物分散到由纯铁或铁构成的基质相中而获得的高刚性钢构成 合金的量为10〜70体积%,覆盖层31的杨氏模量高于基材2的杨氏模量。(C)2010,JPO&INPIT