    • PURPOSE:To improve the resistibility for dynamic fatigue and weatherability of a large tire for bus, etc. by such an arrangement wherein a specially mixed sheet is arranged to cover the surface of the tire from its shoulder part to the sidewall in the peripheral direction of the tire. CONSTITUTION:A composite rubber sheet 3 composed by such an arrangement wherein 20-60wt. parts of natural rubber, 10-50wt. parts of polybutadiene rubber, 10-50wt. parts of halogenation butylrubber and 5-30wt. parts of copolymer rubber of ethylene propylene diene are properly mixed so that a total of 100wt. parts can be obtained is arranged to cover the surface of a tire from its shoulder C to its sidewall B in the peripheral direction of the tire. In this case, the thickness of the sheet shall be approx. 0.5-5mm.. The resistibility for dynamic fatigue and weatherability of the tire can be improved.
    • 目的:为了提高公共汽车等的大型轮胎的动态疲劳和耐候性的抵抗性,通过这样的布置,特别混合的片材被布置成从轮胎的表面覆盖从胎肩部到侧壁的周向 轮胎。 构成:由这样的结构构成的复合橡胶片3,其中20-60wt。 部分天然橡胶,10-50wt。 聚丁二烯橡胶部件,10-50wt。 部分卤化丁基橡胶和5-30wt。 将乙烯丙烯二烯的共聚物橡胶的一部分合适地混合,使总共100wt。 可以获得的部分被布置成在轮胎的周向方向上从轮胎的肩部C覆盖轮胎表面到其侧壁B. 在这种情况下,纸张的厚度应为约 0.5-5mm。可以提高轮胎的动态疲劳和耐候性的抵抗性。