    • Method for producing wet tissue
    • 生产组织的方法
    • JP2013075086A
    • 2013-04-25
    • JP2011217656
    • 2011-09-30
    • Unicharm Corpユニ・チャーム株式会社
    • KONISHI TAKAYOSHIHIRAOKA TOSHIOHIKOSAKA TOSHIFUMIKAMEDA HANHO
    • A47K7/00
    • D04H1/559B65H29/242B65H29/32B65H31/3054B65H2406/323D04H1/495D04H1/645D04H1/76
    • PROBLEM TO BE SOLVED: To provide a method for producing wet tissue that is used to produce bulky wet tissue.SOLUTION: The method for producing wet tissue, includes a step for preparing fiber sheets (11, 12), and post-processing steps (17, 18, 23, 25) comprising a step for folding the fiber sheets (17), a step for impregnating the fiber sheets with a chemical solution (18), a step for cutting the fiber sheets (23) and a step for laminating the fiber sheets (25), wherein a step for increasing the moisture content of the fiber sheets (13) and a step for spraying high-pressure steam onto the fiber sheets for which moisture content is increased (14) are contained between the step for preparing the fiber sheets (11, 12) and the post-processing steps (17, 18, 23, 25).
    • 待解决的问题:提供一种用于制造用于制造大体积湿纸巾的湿纸巾的方法。 解决方案:制造湿纸巾的方法包括制备纤维片(11,12)的步骤和包括用于折叠纤维片(17)的步骤的后处理步骤(17,18,23,25) ,用化学溶液(18)浸渍纤维片的步骤,切割纤维片(23)的步骤和层压纤维片(25)的步骤,其中增加纤维片材的含水量的步骤 (13),并且在用于制备纤维片(11,12)的步骤和后处理步骤(17,18)之间包含用于将高压蒸汽喷射到水分含量增加的纤维片材上的步骤(14) ,23,25)。 版权所有(C)2013,JPO&INPIT
    • 3. 发明专利
    • Method for producing nonwoven fabric
    • 生产非织造布的方法
    • JP2013076196A
    • 2013-04-25
    • JP2011218027
    • 2011-09-30
    • Uni Charm Corpユニ・チャーム株式会社
    • KONISHI TAKAYOSHIHIRAOKA TOSHIOHIKOSAKA TOSHIFUMIKAMEDA HANHO
    • D21H27/00D04H1/492
    • D21H23/50D21H27/002
    • PROBLEM TO BE SOLVED: To provide a method for producing a nonwoven fabric capable of providing a nonwoven fabric that is bulky and has flexibility.SOLUTION: The method for producing a nonwoven fabric includes steps of: forming a fiber sheet 24 on a substrate 18 by feeding a papermaking raw material containing water onto the substrate 18; drying the fiber sheet 24 (20); forming a region in which the water content is increased to a water content that is higher than the water content of the fiber sheet 24 dried by the step of drying the fiber sheet 24 on a part of the fiber sheet 24 dried by the step of drying (20) the fiber sheet 24 (23); and spraying a high-pressure steam to the region of the fiber sheet 24 in which the water content is increased (14).
    • 解决问题的方案:提供一种无纺布的制造方法,其能够提供体积大且柔软性的无纺布。 解决方案:无纺布的制造方法包括以下步骤:通过将含有水的造纸原料输送到基板18上而在基板18上形成纤维片24; 干燥纤维片24(20); 形成水分含量高于通过干燥纤维片24干燥的纤维片24的水分含量的区域,所述纤维片24在通过干燥步骤干燥的纤维片24的一部分上干燥 (20)纤维片24(23); 并向其中含水量增加的纤维片24的区域喷射高压蒸汽(14)。 版权所有(C)2013,JPO&INPIT