    • 1. 发明专利
    • Polishing jig device for slider assembly, and apparatus and method for polishing
    • 用于滑动组件的抛光装置,以及用于抛光的装置和方法
    • JP2011230218A
    • 2011-11-17
    • JP2010102030
    • 2010-04-27
    • Sae Magnetics (Hk) Ltd新科實業有限公司SAE Magnetics(H.K.)Ltd.
    • HARAKAWA OSAMUFUJII TAKASHIKURIBAYASHI MASAHIRO
    • B24B37/005B24B37/04B24B37/07B24B37/30B24B41/06G11B5/31G11B5/39G11B5/60
    • PROBLEM TO BE SOLVED: To uniformly polish a slider assembly, in which multiple slider arrays are arranged in the longitudinal direction, in the longitudinal direction of the slider assembly by a simple configuration.SOLUTION: A polishing jig 50a for the slider assembly, includes: a holding surface 58 for holding a surface to be polished of the slider assembly by allowing the surface to be polished to face a polishing surface of a polishing table; a pressure load receiver 56 for receiving a pressure load at which the surface to be polished is pressed on the polishing surface; multiple adjustment load receiving holes 60a-60g provided along the longitudinal direction for receiving an adjustment load for adjusting the pressure load in each position of the slider assembly arranged along the longitudinal direction; and missing parts 61a, 61b each provided between end receiving holes 60a, 60g and intermediate receiving holes 60b, 60f adjacent to the end receiving holes, positioned at a level between the adjustment load receiving holes and the holding surface, and penetrating through the polishing jig in the thickness direction of the jig.
    • 要解决的问题:为了通过简单的构造在滑块组件的纵向方向上均匀地抛光其中在纵向方向上布置多个滑块的滑块组件。 解决方案:用于滑块组件的抛光夹具50a包括:保持表面58,用于通过允许抛光表面面对抛光台的抛光表面来保持滑块组件的待抛光表面; 用于接收待抛光表面的压力负载的压力负载接收器56被压在抛光表面上; 沿着纵向方向设置的多个调节负载接收孔60a-60g,用于接收用于调节沿着纵向布置的滑块组件的每个位置的压力负载的调节负载; 以及各自设置在端部容纳孔60a,60g之间的缺损部分61a,61b和位于调节载荷接收孔和保持表面之间的水平面上的端部接收孔的中间接收孔60b,60f,并且穿过研磨夹具 在夹具的厚度方向上。 版权所有(C)2012,JPO&INPIT
    • 2. 发明专利
    • Method of manufacturing thin film magnetic head
    • 制造薄膜磁头的方法
    • JP2009217883A
    • 2009-09-24
    • JP2008059763
    • 2008-03-10
    • Sae Magnetics (Hk) Ltd新科實業有限公司SAE Magnetics(H.K.)Ltd.
    • HARAKAWA OSAMU
    • G11B5/31
    • PROBLEM TO BE SOLVED: To provide a method of manufacturing a thin film magnetic head by which high working efficiency and product efficiency are achieved, an intrusion phenomenon of a row bar and chipping thereof, damage to a polishing plate or the like can be avoided, moreover, polishing quantity can be surely detected from the start of polishing.
      SOLUTION: One plane 404 of the row bar 71 in a height direction Y is ground, and a slop 405 is formed which is angled in a direction where the height Y is decreased gradually from one plane 402 in a thickness direction Z where a reproducing element 100A and a recording element 100B are present toward the other one plane 401. Next, polishing in the direction of an arrow mark F1 from a side of the one plane 401 to the one plane 402 is performed for the slope 405, and relative positional deviation ΔY1 between the reproducing element 100A and the recording element 100B is corrected.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:为了提供一种制造高效率和产品效率的薄膜磁头的方法,排条的入侵现象和其碎裂,对抛光板等的损坏可以 此外,从抛光开始可以可靠地检测出抛光量。 解决方案:排列杆71在高度方向Y上的一个平面404被研磨,并且形成一个斜面405,其沿高度Y在厚度方向Z上从一个平面402逐渐减小的方向成角度, 向另一个平面401存在再现元件100A和记录元件100B。接下来,对于斜面405进行从一个平面401侧到一个平面402的箭头标记F1的方向的抛光,以及 再现元件100A与记录元件100B之间的相对位置偏差ΔY1被校正。 版权所有(C)2009,JPO&INPIT
    • 3. 发明专利
    • Methods of manufacturing coil and coil device
    • 制造线圈和线圈装置的方法
    • JP2010199291A
    • 2010-09-09
    • JP2009042379
    • 2009-02-25
    • Sae Magnetics (Hk) Ltd新科實業有限公司SAE Magnetics(H.K.)Ltd.
    • UEDA KUNIHIROYAMADA HIROKIHARAKAWA OSAMU
    • H01F41/04
    • H01P11/003G06K19/07779G06K19/07781H01F5/003H01F27/40H01F41/041H01F2017/006Y10T29/49016
    • PROBLEM TO BE SOLVED: To efficiently manufacture a thin type coil such as an antenna coil, and to easily cope with the manufacturing of a coil different in the number of turns. SOLUTION: The coil 9 is manufactured by sequentially carrying out steps of: forming a thin film 2 formed of a conductive material on one surface of a long-sheet-shaped flexible base 1; manufacturing an original roll of coils 4 by winding the flexible base 1 having the thin film 2 formed of the conductive material in a roll shape; manufacturing a wound body 6 by unwinding the flexible base 1 having the thin film 2 formed of the conductive material from the original roll of coils 4 and rewinding it around an outer periphery of a core 5; cutting out a coil intermediary body 7 by cutting the wound body 6 in a direction orthogonal to the length of the core 5; polishing a cut surface 7a of the coil intermediary body 7 cut out of the wound body 6; and attaching lead wires 8 to both ends of a winding part 7b formed of a conductive material in the coil intermediary body 7. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:为了有效地制造诸如天线线圈的薄型线圈,并且容易地应对不同匝数的线圈的制造。 解决方案:线圈9通过依次执行以下步骤制造:在长片状柔性基体1的一个表面上形成由导电材料形成的薄膜2; 通过将具有由导电材料形成的薄膜2的柔性基底1卷成卷状来制造原卷卷4; 通过从原卷绕线圈4展开具有由导电材料形成的薄膜2的柔性基座1并围绕芯5的外周重新卷绕来制造卷绕体6; 通过沿着与芯部5的长度正交的方向切割卷绕体6来切断线圈中间体7; 研磨从卷绕体6切出的线圈中间体7的切割面7a; 并将引线8连接在线圈中间体7中由导电材料形成的绕组部分7b的两端。(C)2010,JPO&INPIT
    • 4. 发明专利
    • Manufacturing method of slider
    • 滑块制造方法
    • JP2007207396A
    • 2007-08-16
    • JP2006028397
    • 2006-02-06
    • Shinka Jitsugyo Kk新科實業有限公司SAE Magnetics(H.K.)Ltd.
    • FUKUROI OSAMUHARAKAWA OSAMU
    • G11B5/60B24B7/22G11B21/21
    • PROBLEM TO BE SOLVED: To improve production efficiency by preventing warp of a bar when a slider is manufactured.
      SOLUTION: The manufacturing method of the slider has a step S1 for preparing a head element assembly formed by arranging many head elements to be the sliders, in which one of at least a reading element or a writing element is formed between a substrate and a protective film at least in one direction including a longitudinal direction, and a grinding step S2 in which the surface of the substrate side of the head element assembly is ground in the direction being orthogonal to the longitudinal direction.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:通过在制造滑块时防止棒的翘曲来提高生产效率。 解决方案:滑块的制造方法具有步骤S1,用于制备头部元件组件,该头部元件组件通过将许多头元件布置成滑块,其中至少一个读取元件或写入元件中的至少一个形成在基板 以及至少在包括纵向的一个方向上的保护膜,以及研磨步骤S2,其中头元件组件的基板侧的表面在与纵向正交的方向上被研磨。 版权所有(C)2007,JPO&INPIT