热词
    • 1. 发明专利
    • Plated steel sheet for can
    • 适用于CAN的钢板
    • JP2010242182A
    • 2010-10-28
    • JP2009093150
    • 2009-04-07
    • Nippon Steel Corp新日本製鐵株式会社
    • DATE HIROMITSUSHOJI HIROMASA
    • C23C28/00C23C22/22C23C22/50C25D5/26C25D5/48C25D7/04C25D11/36
    • PROBLEM TO BE SOLVED: To provide a plated steel sheet for can which is excellent in secondary adhesion and corrosion resistance of an organic coating film. SOLUTION: The plated steel sheet for can is a steel sheet continuously or intermittently having metal tin on a steel sheet surface or on an alloy layer containing iron and tin, and has a phosphate layer for 0.5-5.0 mg/m 2 as the amount of P on the metal tin and/or on the alloy layer, and further has a silica-zirconia treatment layer containing the oxide of Zr and/or the hydroxide of Zr for 2-15 mg/m 2 as the amount of Zr and the oxide of Si and/or the hydroxide of Si for 2-15 mg/m 2 as the amount of Si, for which the total the amount of Zr and the amount of Si is 5-30 mg/m 2 , on the phosphate layer. COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供一种有机涂膜的二次粘合性和耐腐蚀性优异的罐用电镀钢板。 解决方案:用于罐的镀覆钢板是在钢板表面上或在含有铁和锡的合金层上连续或间歇地具有金属锡的钢板,并且具有0.5-5.0mg / m 2的磷酸盐层 > 2 作为金属锡和/或合金层上的P量,并且还含有含有Zr的氧化物和/或Zr的氧化物的二氧化硅 - 氧化锆处理层,其含量为2-15mg / 作为Si的量,作为Si的量,作为Zr的量和Si的氧化物和/或Si的氢氧化物为2-15mg / m 2 SP / 2,其中 在磷酸盐层上总共Zr的量和Si的量为5-30mg / m 2 SPF。 版权所有(C)2011,JPO&INPIT
    • 2. 发明专利
    • Metal (hydro)oxide coated metallic material
    • 金属(HYDRO)氧化物涂层金属材料
    • JP2009299145A
    • 2009-12-24
    • JP2008155876
    • 2008-06-13
    • Nippon Steel Corp新日本製鐵株式会社
    • SHOJI HIROMASAFUDA MASAHIRO
    • C23C26/00B32B9/00C23C22/34C23C28/00C25D9/08
    • PROBLEM TO BE SOLVED: To provide a metallic material having a coating layer which is small in environmental load and is highly corrosion resistant, and is high in adhesion in the case of forming an organic resin-based coating layer.
      SOLUTION: The metal (hydro)oxide coated metallic material having a film consisting of one or both of the oxide and hydroxide of two to four of metal elements selected from the following (a) to (c) groups and containing one or more of the metal elements selected from the at least (a) group: wherein, (a) group includes Ti. Zr, Hf, (b) group includes V, Nb, Ta, and (c) group includes Si.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供具有环境负荷小且耐腐蚀性高的涂层的金属材料,并且在形成有机树脂基涂层的情况下具有高粘附性。 解决方案:具有由选自以下(a)至(c)组的两至四个金属元素中的一种或两种氧化物和氢氧化物组成的膜的金属(氢氧化物)涂覆的金属材料,并且包含一个或多个 更多选自至少(a)组的金属元素:其中,(a)基团包括Ti。 Zr,Hf,(b)组包括V,Nb,Ta和(c)基团包括Si。 版权所有(C)2010,JPO&INPIT
    • 7. 发明专利
    • Metal oxide and/or metal hydroxide coated conductive material
    • 金属氧化物和/或金属氢氧化物涂层导电材料
    • JP2008214758A
    • 2008-09-18
    • JP2008110762
    • 2008-04-21
    • Nippon Steel Corp新日本製鐵株式会社
    • SHOJI HIROMASASUGIURA TSUTOMU
    • C23C22/34C23C22/68C25D9/04C25D9/10
    • C25D9/04C23C22/34C23C22/68
    • PROBLEM TO BE SOLVED: To provide a method for production of various oxide and/or hydroxide coatings with various functions and constructions on metal materials from aqueous solutions, and metal materials having such coatings.
      SOLUTION: There are provided specifically a method for production of a metal oxide and/or metal hydroxide coated metal material characterized by immersing a metal material or electrolyzing a conductive material in an aqueous treatment solution at pH 2 to 7 containing metal ion and fluorine ion in a 4-fold molar ratio with respect to the metal ion, and/or containing a complex ion comprising at least a metal ion and a fluorine ion in a 4-hold molar ratio with respect to the metal ion, to form on the surface of the metal material a metal oxide and/or metal hydroxide coating containing the metal ion, as well as a metal oxide and/or metal hydroxide coated metal material characterized by having a metal oxide and/or metal hydroxide coating produced by the method.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种用于生产具有各种功能和结构的各种氧化物和/或氢氧化物涂层的方法,所述各种功能和结构在水溶液中的金属材料和具有这种涂层的金属材料上。 具体地说,提供一种金属氧化物和/或金属氢氧化物涂覆的金属材料的制造方法,其特征在于将金属材料浸渍或电解导电材料到含有金属离子的pH为2〜7的水溶液中, 氟离子相对于金属离子为4倍摩尔比,和/或含有相对于金属离子具有4-保持摩尔比的至少金属离子和氟离子的复合离子,以形成 金属材料的表面是含有金属离子的金属氧化物和/或金属氢氧化物涂层,以及金属氧化物和/或金属氢氧化物涂覆的金属材料,其特征在于具有通过该方法制备的金属氧化物和/或金属氢氧化物涂层 。 版权所有(C)2008,JPO&INPIT
    • 8. 发明专利
    • Surface-treated metal sheet, surface treatment agent for metal, and method for manufacturing surface-treated metal sheet
    • 表面处理金属片,金属表面处理剂,以及制造表面处理金属片的方法
    • JP2008138254A
    • 2008-06-19
    • JP2006325648
    • 2006-12-01
    • Nippon Steel Corp新日本製鐵株式会社
    • SHOJI HIROMASA
    • C25D9/08C25D11/00
    • PROBLEM TO BE SOLVED: To provide a surface-treated metal sheet which does not contain chromium and has superior adhesiveness to a paint film, superior corrosion resistance, and further, superior weldability, and to provide a manufacturing method therefor. SOLUTION: The surface-treated metal sheet comprises a metal layer (A) of which the metal excludes chromium, and a layer (B) formed of a hydroxide or an oxide of a metal (b) which excludes chromium and a metal (a), or a mixture of the hydroxide and the oxide, on the metal layer (A). The layer (B) also includes the metal (a) which is the same type as the metal layer (A). The surface treatment agent for the metal and the method for manufacturing the surface-treated metal sheet are disclosed. COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种不含铬的表面处理金属片,并且对涂膜具有优异的粘附性,优异的耐腐蚀性,并且还具有优异的焊接性,并提供其制造方法。 解决方案:表面处理金属片包括其中金属不含铬的金属层(A)和由不含铬和金属的金属(b)的氢氧化物或氧化物形成的层(B) (a),或氢氧化物和氧化物的混合物在金属层(A)上。 层(B)还包括与金属层(A)相同类型的金属(a)。 公开了金属用表面处理剂及表面处理金属板的制造方法。 版权所有(C)2008,JPO&INPIT
    • 9. 发明专利
    • Treating solution excellent in surface treating reactivity
    • 在表面处理反应中处理优异的溶液
    • JP2007113047A
    • 2007-05-10
    • JP2005304296
    • 2005-10-19
    • Nippon Steel Corp新日本製鐵株式会社
    • KIMURA MASAOTANAKA YUKIMOTOSHOJI HIROMASA
    • C23C20/08
    • PROBLEM TO BE SOLVED: To provide a treating solution for depositing a surface film of excellent quality in an extensive process condition.
      SOLUTION: The treating solution is used for a process for depositing one or more kinds of oxide, hydroxide and oxyhydroxide of a metal element M (hereinafter, referred to as "oxides or the like") from a treating solution containing fluoro complex ions of one or more kinds of metal element M to be selected from Ti, Si and Zr on a surface of a material to be treated. The total molar concentration of the oxides or the like of the metal element M in the treating solution is ≥10
      -4 mol/L and ≤1 mol/L, and the mean grain size of the oxides is ≤5 μm. The treating solution is excellent in surface treating reactivity.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供一种用于在广泛的工艺条件下沉积出优质品质的表面膜的处理溶液。 解决方案:处理溶液用于从含有氟络合物的处理溶液中沉积金属元素M(以下称为“氧化物等”)的一种或多种氧化物,氢氧化物和羟基氧化物的方法 在待处理材料的表面上选择Ti,Si和Zr中的一种或多种金属元素M的离子。 处理液中的金属元素M的氧化物等的总摩尔浓度为≥10×SP> -4 / mol / L,≤1mol/ L,氧化物的平均粒径为 ≤5μm。 处理溶液的表面处理反应性优异。 版权所有(C)2007,JPO&INPIT
    • 10. 发明专利
    • Steel sheet having excellent penetration property on tig welding
    • 在TIG焊接上具有优异的穿透性能的钢板
    • JP2004285395A
    • 2004-10-14
    • JP2003078136
    • 2003-03-20
    • Nippon Steel Corp新日本製鐵株式会社
    • INOUE YUJISHOJI HIROMASA
    • B23K9/167B23K9/23B23K103/16C23C26/00
    • PROBLEM TO BE SOLVED: To provide a steel sheet in which deep penetration can be obtained even under ordinary TIG (Tungsten Inert Gas) welding conditions and to which TIG welding of high efficiency can be performed by obviating a stage of applying active flux on the welding.
      SOLUTION: The steel sheet is constituted so as to be coated with a film consisting of one or more kinds selected from titanium oxide, zirconium oxide, chromium oxide, molybdenum oxide, silicon oxide and iron oxide in ≥0.05 μm by the total film thickness by using a liquid phase deposition method (LPD method) where at least a part of its surface is brought into contact with a treatment solution containing the metal ions of oxide to be formed and fluorine ions to form an oxide film on the surface. Thus, the film has high adhesion with the steel sheet, has uniform film thickness, and is not peeled on TIG welding operation.