    • 1. 发明专利
    • Dissimilar metal bonded joint, and method of manufacturing the same
    • DISSIMILAR金属粘结接头及其制造方法
    • JP2013130238A
    • 2013-07-04
    • JP2011279731
    • 2011-12-21
    • Nippon Steel & Sumitomo Metal Corp新日鐵住金株式会社Furukawa-Sky Aluminum Corp古河スカイ株式会社
    • SAKIYAMA TATSUYAMIYAZAKI YASUNOBUOKADA TOSHIYA
    • F16B5/02B21D39/03B21J15/14F16J15/14
    • B21J15/025F16B5/045F16B19/1054
    • PROBLEM TO BE SOLVED: To provide a dissimilar metal bonded joint and a method of manufacturing the same, allowing reliably preventing dissimilar metal corrosion at the joint of dissimilar metals.SOLUTION: The dissimilar metal bonded joint includes: a first metal member 1; a second metal member 2 which is superimposed on the first metal member 1 and made of different dissimilar metal from the first metal member 1; a mechanical joint part 4 which fastens the first and second metal members 1, 2; and a seal layer 5 formed between the joint surfaces 1a, 2a of the first and second metal members 1, 2. A first annular projection 1bsurrounding the mechanical joint part 4 and a second annular projection 1bsurrounding the first annular projection 1bare provided to the joint surfaces 1a, 2a of the first metal member 1 or the second metal member 2. The seal layer 5 is formed between the first and second metal members 1, 2 between the first and second annular projections 1b, 1b.
    • 要解决的问题:为了提供异种金属接合接头及其制造方法,允许可靠地防止异种金属接头处的异种金属腐蚀。解决方案:异种金属接合接头包括:第一金属构件1; 第二金属构件2,其从第一金属构件1叠加在第一金属构件1上并由不同的异种金属制成; 紧固第一和第二金属构件1,2的机械接合部4; 以及密封层5,其形成在第一和第二金属构件1,2的接合表面1a,2a之间。围绕机械接合部分4的第一环形突起和围绕第一环形突起1b的第二环形突起设置在接合表面 第一金属构件1或第二金属构件2的1a,2a。密封层5形成在第一和第二环形突起1b,1b之间的第一和第二金属构件1,2之间。
    • 2. 发明专利
    • Joining method of aluminum plate material
    • 铝板材的接合方法
    • JP2013056349A
    • 2013-03-28
    • JP2011194939
    • 2011-09-07
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社Nippon Steel & Sumitomo Metal Corp新日鐵住金株式会社
    • OKADA TOSHIYASAKIYAMA TATSUYAICHIYAMA YASUTOMO
    • B23K9/23B23K9/16B23K9/167C22C21/00C22C21/02C22C21/06
    • PROBLEM TO BE SOLVED: To provide an inexpensive joining method of a thickness-different aluminum joined sheet in which the smoothness of the surface is excellent, the bond strength is high, and there is not the defect.SOLUTION: The joining method of an aluminum plate material is a method that joins two or more aluminum plate materials that have 0.5-3.0 mm of a thickness and in which the thicknesses of adjacent aluminum plate materials are different, and is characterized in that the two or more aluminum plate materials are an aluminum alloy that includes: less than Mg:6.0 mass%; and a remainder consisting of Al and inevitable impurities. A thin plate material thickness t1 and a thick plate material thickness t2 satisfy 1.0≤t2/t1
    • 要解决的问题:为了提供一种廉价的接合方法,其中表面的平滑度优异的粘结强度高,不存在缺陷的厚度不同的铝接合片的接合方法。 解决方案:铝板材料的接合方法是连接两个或多个厚度为0.5-3.0mm并且相邻铝板材料的厚度不同的铝板材料的方法,其特征在于 两种以上的铝板材料是铝合金,其包括:小于Mg:6.0质量%; 剩余部分由Al和不可避免的杂质组成。 薄板材厚度t1和厚板材厚度t2满足1.0≤t2/ t1 <1.3,电极间距离至多为1.0mm,He为纯度的75-100%,5-15升/分钟 使用流量作为保护气体,并且不使用填充金属。 薄板材料和厚板材的平均板厚中的每个单位板厚度的热输入量假定为2,500-12,000(J / cm 2),两个板的端面相互对接,并且对接部 通过直流直流TIG焊接方法连接。 版权所有(C)2013,JPO&INPIT
    • 3. 发明专利
    • Rotary joining tool for friction stir joining and friction stir joining method using the same
    • 旋转加工工具用于摩擦接合和摩擦加工方法
    • JP2013000761A
    • 2013-01-07
    • JP2011132746
    • 2011-06-15
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社Nippon Steel & Sumitomo Metal Corp新日鐵住金株式会社
    • SAKAI TOSHIROOKADA TOSHIYASAKIYAMA TATSUYAICHIYAMA YASUTOMO
    • B23K20/12
    • PROBLEM TO BE SOLVED: To provide a rotary joining tool easy in control, comparatively inexpensive, affording favorable joining strength and used for joined members of different plate thicknesses, and to provide a friction stir joining method using the same.SOLUTION: Provided are the rotary joining tool for friction stir joining adapted to friction-stir-join the joined members of different plate thicknesses, wherein an upper base part, an upper shoulder, a lower base part, a lower shoulder and a probe between the shoulders are configured to be integrally rotatable, surfaces of the upper shoulder and the lower shoulder define a convex curve toward an abutment part, one or more grooves are formed in the convex curve so as to run from an outer periphery to the center and to flow the plasticized joined members into it, the abutment part of the joined members is nipped between the upper shoulder and the lower shoulder so as to set the probe parallel with abutment faces, and the probe moves along the abutment part while rotating with the upper base part and the lower base part out of contact with the joined members. A method of manufacturing the same is also provided.
    • 要解决的问题:为了提供易于控制的旋转接合工具,比较便宜,提供了良好的接合强度并且用于不同板厚度的接合部件,并且提供了使用该旋转接合工具的摩擦搅拌接合方法。 解决方案:提供用于摩擦搅拌接合的旋转接合工具,其适于摩擦搅拌连接不同板厚度的接合部件,其中上基部,上肩部,下基部,下肩部和 肩部之间的探针被构造成可一体旋转,上肩部和下肩部的表面限定朝向邻接部分的凸曲线,在凸曲线中形成一个或多个凹槽,以从外周向中心延伸 并且将塑化的连接部件流入其中,将接合部件的抵接部分夹在上肩部和下肩部之间,以将探针平行于邻接面设置,并且探头沿着抵接部件移动,同时旋转 上基部和下基部与接合部件脱离接触。 还提供了一种制造该方法的方法。 版权所有(C)2013,JPO&INPIT
    • 4. 发明专利
    • Method of forming aluminum alloy sheet
    • 形成铝合金板的方法
    • JP2013230483A
    • 2013-11-14
    • JP2012103458
    • 2012-04-27
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社Nippon Steel & Sumitomo Metal Corp新日鐵住金株式会社
    • NOGUCHI OSAMUOKADA TOSHIYATAKADA TAKESHI
    • B21D22/20
    • PROBLEM TO BE SOLVED: To provide a method of performing press forming by suppressing the rupture of a tailored blank which is obtained by butt welding of aluminum alloy sheets which are different in at least one of plate thickness and strength.SOLUTION: A tailored blank 20 is prepared by butt-welding two or more aluminum alloy sheets which are different in at least one of a sheet thickness and strength. When forming the tailored blank 20, the tailored blank 20 is heated so that the material temperature of the base metal 24 of the tailored blank 20 becomes 100-250°C in a state that the heat affected zone 23 of the tailored blank 20 by butt welding is not higher than 80°C, and the heat affected zone 23 is situated between a punch 15 and a die 16 to perform press forming.
    • 要解决的问题:提供一种通过抑制由板材厚度和强度中的至少一种不同的铝合金板的对接而获得的定制坯料的破裂来进行冲压成形的方法。解决方案:定制的坯料20 是通过对板材厚度和强度中的至少一种不同的两种以上的铝合金板进行对焊而制备的。 当形成定制的坯料20时,将定制的坯料20加热,使得定制坯料20的母材金属24的材料温度在定制的坯料20的热影响区域23的对接状态下变为100-250℃ 焊接不高于80℃,并且热影响区23位于冲头15和模具16之间以进行冲压成形。
    • 5. 发明专利
    • Joining method of aluminum alloy material and dissimilar metal material
    • 铝合金材料和金属材料的接合方法
    • JP2013116483A
    • 2013-06-13
    • JP2011264846
    • 2011-12-02
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社
    • MURASE TAKASHIYANAGAWA YUTAKAOKADA TOSHIYA
    • B23K20/00B23K20/16B23K20/233B23K35/363C22C9/00C22C9/04C22C14/00C22C19/03C22C21/02C22C21/12C22C23/02C22C38/00
    • PROBLEM TO BE SOLVED: To provide a new joining method capable of achieving high reliability, excellent joining performance and small material deformation in joining, in a joining method of an aluminum alloy material and a dissimilar metal material.SOLUTION: The joining method of the aluminum alloy material and the dissimilar metal material is used for joining one joining member being the aluminum alloy material and the other joining member being the dissimilar metal material. In the method, the other joining member is the dissimilar metal material having higher solid phase line temperature than the aluminum alloy, and is joined at a temperature where a ratio of a liquid phase mass generated in the aluminum alloy material to the total mass of the aluminum alloy material is 5 to 35%. The one joining member breaks an oxidized film of the surface of the aluminum alloy material by adjustment of Mg concentration of the aluminum alloy material or use of a flux so as to contrive secure joining.
    • 要解决的问题:提供一种在铝合金材料和异种金属材料的接合方法中能够实现高可靠性,优异的接合性能和接合时材料变形小的新的接合方法。 解决方案:铝合金材料和异种金属材料的接合方法用于将作为铝合金材料的一个接合构件和作为异种金属材料的另一个接合构件接合。 在该方法中,另一方的接合部件是与铝合金相比具有较高的固相线温度的异种金属材料,并且在铝合金材料中产生的液相质量比与 铝合金材料为5〜35%。 一个接合构件通过调节铝合金材料的Mg浓度或使用助焊剂来破坏铝合金材料表面的氧化膜,从而实现牢固的接合。 版权所有(C)2013,JPO&INPIT
    • 7. 发明专利
    • Method for manufacturing flat metal plate
    • 制造平板金属板的方法
    • JP2010234432A
    • 2010-10-21
    • JP2009086879
    • 2009-03-31
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社
    • SAKAI TOSHIROOKADA TOSHIYA
    • B21D1/02B23K20/12B23K31/00
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a flat metal plate capable of manufacturing a wide flat metal plate having the high flatness by butting and welding an end face of one flat metal plate to an end face of the other flat metal plate.
      SOLUTION: A second straightening step is executed, while a reversely-warped part 6 as indicated in Fig.5 by a dotted line C is present by a first straightening step, to the behavior of a flat aluminum plate 3 in the straightening step, and the entire flat aluminum plate 3 can be as flat as possible by the first straightening step. Further, the reversely-warped part 6 is eliminated by the second straightening step as much as possible to industrially manufacture the joined flat aluminum plate having the flatness equivalent to that of a glass tray of the flat aluminum plate used in one piece.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 解决的问题:提供一种制造平板金属板的方法,该平板金属板能够通过将一个平板金属板的端面对接和焊接到另一个平面的端面来制造具有高平坦度的宽扁平金属板 金属板。 解决方案:执行第二矫直步骤,而通过第一矫直步骤存在如图5中虚线C所示的反向弯曲部分6,在平直铝板3的矫正中的行为 整个平板铝板3可以通过第一矫正步骤尽可能平坦。 此外,通过第二矫直工序尽可能地消除了反向翘曲部分6,以在工业上制造具有与一块使用的扁平铝板的玻璃托盘的平坦度相当的平坦度的接合扁平铝板。 版权所有(C)2011,JPO&INPIT
    • 8. 发明专利
    • Method for joining aluminum alloy material, method for manufacturing aluminum alloy joined body, and aluminum alloy joined body
    • 接合铝合金材料的方法,制造铝合金加工体的方法和铝合金接合体
    • JP2013116474A
    • 2013-06-13
    • JP2011264013
    • 2011-12-01
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社
    • FUJITA KAZUKOMURASE TAKASHIOKADA TOSHIYA
    • B23K20/00B23K20/16B23K20/233C22C21/06C22C21/12C22F1/00C22F1/04
    • PROBLEM TO BE SOLVED: To provide a novel joining method applicable to 2000-type aluminum alloy material, and an aluminum alloy joined body of high strength, and a method for manufacturing the same.SOLUTION: In the method for joining aluminum alloy materials with the content of Mg being regulated to, by mass, ≤0.5%, aluminum alloy materials are joined with each other in the non-oxidizing atmosphere while flux is applied between the joined members at the temperature in which the mass ratio of the liquidus generated in the aluminum alloy to the total mass of the aluminum alloy materials of one joined member is 5-35%, and on the other hand, the mass ratio of the liquidus generated in the aluminum alloy materials to the total mass of the aluminum alloy materials of the other joined member is ≤35%. There are provided the method for manufacturing the aluminum alloy joined body using the aluminum alloy materials joined thereby, and the aluminum alloy joined body manufactured thereby.
    • 要解决的问题:为了提供适用于2000型铝合金材料和高强度铝合金接合体的新型接合方法及其制造方法。 &lt; P&gt;解决方案:在铝的合金材料的接合方法中,Mg的含量以质量计≤0.5%进行调节,铝合金材料在非氧化性气氛中彼此接合,同时在连接 在铝合金中产生的液相线的质量比与一个接合部件的铝合金材料的总质量之间的温度下的成员为5-35%,另一方面,生成的液相线的质量比 铝合金材料与其他接合件的铝合金材料的总质量为≤35%。 提供了使用由此接合的铝合金材料制造铝合金接合体的方法,由此制造铝合金接合体。 版权所有(C)2013,JPO&INPIT
    • 9. 发明专利
    • Rotary joint tool for friction stir welding and method for friction stir welding using the same
    • 用于摩擦焊接的旋转接头工具及使用其的摩擦焊接方法
    • JP2012086267A
    • 2012-05-10
    • JP2011195524
    • 2011-09-08
    • Furukawa-Sky Aluminum CorpNippon Steel Corp古河スカイ株式会社新日本製鐵株式会社
    • SAKAI TOSHIROOKADA TOSHIYASAKIYAMA TATSUYAICHIYAMA YASUTOMO
    • B23K20/12
    • PROBLEM TO BE SOLVED: To provide a rotary joint tool in which control is easy, and also, cost is relatively low in friction stir welding for the members to be welded with different sheet thicknesses, and a method for friction stir welding with easy operation.SOLUTION: The rotary joint tool for friction stir welding is used for subjecting the butted parts of the metallic members to be welded with a level difference at the welding faces, and includes: an almost columnar base part; a shoulder part provided at the side of the members to be welded in the base part; and a probe hanging down concentrically with the base part from the surface of the shoulder part. The surface of the shoulder part forms a projecting curved face toward the butted parts, and, in which one or more grooves, provided in such a manner that the members to be welded plasticized by the rotation of the rotary joint tool flow-in to the inside, are formed from the outer circumference thereof to the center in the projecting curved face, and the probe is pushed parallelly to the butted faces of the butted parts, and further, the base part moves along the butted parts while rotating in a state of not being in contact with the members to be welded. The method for friction stir welding uses the same.
    • 要解决的问题:提供一种易于控制的旋转接头工具,并且对于待焊接的不同板厚的构件的摩擦搅拌焊接的成本相对较低,以及用于摩擦搅拌焊接的方法 操作方便 &lt; P&gt;解决方案:用于摩擦搅拌焊接的旋转接头工具用于使金属构件的对接部分在焊接面处焊接有水平差,并且包括:几乎为圆柱形的基部; 肩部,设置在待焊接部件的侧面的基部; 以及从肩部的表面与基部同心地悬挂的探针。 肩部的表面形成朝向对接部分的突出弯曲面,并且其中一个或多个凹槽设置成使得待被焊接的构件通过旋转接头工具的旋转而变形的构件流入 内部由其外周形成为突出弯曲面的中心,并且探头被平行地对准对接部的对接面,此外,基部沿着对接部移动,同时以 不与待焊接的部件接触。 摩擦搅拌焊接方法采用相同的方式。 版权所有(C)2012,JPO&INPIT
    • 10. 发明专利
    • Manufacturing method of aluminum plate
    • 铝板的制造方法
    • JP2009255095A
    • 2009-11-05
    • JP2008103754
    • 2008-04-11
    • Furukawa-Sky Aluminum Corp古河スカイ株式会社
    • OKADA TOSHIYASAKAI TOSHIROSHIBATA YASUO
    • B23K31/00B21D1/02B23K20/12B23K103/10
    • PROBLEM TO BE SOLVED: To industrially provide an aluminum plate joined with smoothness comparable to a conventionally used single sheet of glass tray.
      SOLUTION: In an aluminum plate (3) made into one sheet by joining an aluminum plate (1) and an aluminum plate (2), the side in which one place is warped in the joined part (4) is pressurized using an upper side pressing member such as a roller (6). Also, on the reverse side of the aluminum plate (3) having the warped place, a part corresponding to the place under the upper side pressing member is held by a lower side pressing fixed base (7). Thus, the warp is straightened out in the planar direction of the aluminum plate (3). Then, while the holding state of the aluminum plate (3) by the lower side pressing fixed base (7) is maintained, the upper side pressing member is successively moved along the joined part (4), pressurizing the side with the warp of the joined part (4) and improving the smoothness of the aluminum plate (3), in the manufacturing method.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:工业上提供与常规使用的单张玻璃托盘相当的平滑度的铝板。 解决方案:在通过连接铝板(1)和铝板(2)制成一片的铝板(3)中,在接合部分(4)中一个位置翘曲的一侧被加压,使用 诸如辊(6)的上侧按压构件。 此外,在具有翘曲位置的铝板(3)的背面,与下侧按压部件相对应的部分由下侧按压固定基座(7)保持。 因此,经线在铝板(3)的平面方向上被拉直。 然后,通过下侧按压固定基座(7)保持铝板(3)的保持状态,上侧按压部件沿着接合部(4)依次移动, (4),提高铝板(3)的平滑度。 版权所有(C)2010,JPO&INPIT