    • 1. 发明专利
    • Preparation of zinc shots for blasting
    • 用于喷砂的锌合金制备
    • JPS58222177A
    • 1983-12-23
    • JP10370282
    • 1982-06-16
    • Nippon Mining Co Ltd
    • AKAGI SUSUMUYOSHIKAWA KOUSUKEOOKURA TAKAHIKO
    • B24C11/00B01J2/02B01J2/06B22F9/08B24D3/00C09K3/14
    • PURPOSE: To prepare small-sized zinc shots suitale for blasting consistently with good yield, by allowing molten zinc to drop through a nozzle from a sump into water under controlled conditions of temperature and depth of molten metal, nozzle size, distance between nozzle and surface of water, temperature of water, etc.
      CONSTITUTION: A ceramic nozzle 15 with an orifice diameter of 0.3W0.6mm is provided at the bottom of a sump 13 in a tank 10 which is divided into a molten metal pouring chamber 12 and the sump 13 and a molten zinc heated to 540W 600°C is supplied to the tnak 10 so that the depth of the molten metal may be 30W60cm. Then the molten zinc is allowed to drop through the nozzle 15 into a water tank 1 which is filled with water at 30W50°C to such a level that the distance from the bottom end of the nozzle 15 to the surface of water may be 10mm or smaller. The molten zinc is allowed to cool and solidify and the zinc shots thus formed are led into a taking-up chamber 13 along an inclined bottom wall 4 and are taken out into a collecting container 5.
      COPYRIGHT: (C)1983,JPO&Japio
    • 目的:为了准备小尺寸的锌合金喷丸,可以以良好的产量进行喷砂,通过使熔融锌在熔融金属的温度和深度,喷嘴尺寸,喷嘴和表面之间的距离的受控条件下,通过喷嘴从水槽中滴入水中 水,温度等。构成:孔径为0.3-0.6mm的陶瓷喷嘴15。 设置在容器10的底部,该容器10被分为熔融金属浇注室12和贮槽13,并且加热到540-600℃的熔融锌被供应到塔尼克10,使得深度 熔融金属可以是30-60cm。 然后使熔融的锌通过喷嘴15落入一个水箱1中,该水箱1填充了30-50℃的水,使得从喷嘴15的底端到水面的距离可以 为10mm。 或更小。 使熔融的锌冷却固化,并将这样形成的锌射流沿着倾斜的底壁4引入卷取室13,并且被取出到收集容器5中。