    • Method for manufacturing sealing material
    • 密封材料的制造方法
    • JP2003327434A
    • 2003-11-19
    • JP2002137195
    • 2002-05-13
    • Nippon Electric Glass Co Ltd日本電気硝子株式会社
    • MATSUDA TOSHIFUMIKATO MITSUOCHIMURA YOSHIKIHAYASHI MASAAKI
    • C03B5/225C03B5/16C03C8/04C03C8/10H01J9/26
    • C03C3/072C03C3/064C03C3/066C03C3/074C03C8/04C03C8/10
    • PROBLEM TO BE SOLVED: To provide a method for manufacturing a sealing material by which method foaming from the sealing material is suppressed in spite of sealing of a device in a vacuum and the degradation in the airtightness of the device, the degradation in the sealing strength of the sealed sections, etc., are averted. SOLUTION: The method for manufacturing the powdery sealing material P composed of the powder glass manufactured by crushing regulated to attain a softening point of 200 to 900°C as a chief material has a process step of heating the powder glass to a maximum temperature of 100°C to a temperature of (the glass softening point of the powder glass - 30°C) in a refractory vessel 20 by using a vacuum reduced pressure heating furnace 10 and a process step of holding the powder glass at the prescribed temperature for the prescribed time under a reduced pressure of ≤10 4 Pa. COPYRIGHT: (C)2004,JPO
    • 解决问题的方案:提供一种制造密封材料的方法,其中即使在真空中密封装置并且器件的气密性降低,也可以抑制从密封材料发泡的方法, 密封部等的密封强度得以避免。 解决方案:制造由粉碎玻璃制成的粉末状密封材料P的方法为通过粉碎调节以达到软化点为200-900℃为主要材料的方法具有将粉末玻璃加热到最大程度的工艺步骤 温度为100℃,通过使用真空减压加热炉10在耐火容器20中的温度(粉末状玻璃的玻璃软化点-30℃)和保持粉末状玻璃的规定温度的工序 在≤10 4 Pa的减压下规定时间。 版权所有(C)2004,JPO
    • 3. 发明专利
    • Filler powder, and powder and paste for sealing
    • 填充粉末,粉末和密封剂
    • JP2006137635A
    • 2006-06-01
    • JP2004328325
    • 2004-11-12
    • Nippon Electric Glass Co Ltd日本電気硝子株式会社
    • CHIMURA YOSHIKIIZEKI JUNICHI
    • C04B35/628C03C8/24C04B35/00H01J5/02H01L23/10
    • PROBLEM TO BE SOLVED: To provide a filler powder for use in a sealing glass having a coefficient of thermal expansion which matches that of an article to be sealed, having an outstanding fluidity and enabling airtight sealing, and to provide a powder and a paste for sealing prepared by mixing a sealing glass powder with the filler powder. SOLUTION: The filler powder is prepared by coating one or more ceramic filler powders selected from the group consisting of cordierite, willemite, alumina, zircon, tin oxide, β-eucryptite, KZr 2 (PO 4 ) 3 , NbZr(PO 4 ) 3 , Na 0.5 Nb 0.5 Zr 1.5 (PO 4 ) 3 , K 0.5 Nb 0.5 Zr 1.5 (PO 4 ) 3 , Ca 0.5 Zr 2 (PO 4 ) 3 and WO 4 Zr 2 (PO 4 ) 2 with a fire resistant fine powder. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供一种用于密封玻璃的填料粉末,该密封玻璃的热膨胀系数与要密封的物品的热膨胀系数匹配,具有优异的流动性并且能够进行气密密封,并且提供粉末和 通过将密封玻璃粉末与填料粉末混合制备的用于密封的浆料。 解决方案:通过涂覆一种或多种选自堇青石,硅锌矿,氧化铝,锆石,氧化锡,β-锂辉石,KZr 2(PO)的陶瓷填料粉末制备填料粉末 SB SB 3,SBZ 3,NbZr(PO 4 )3 SB,Nb < SB> 0.5 Zr 1.5 (SB <4> SB> 3 ,K 0.5 Zr 1.5 (SB <4> SB> 3)SB <3> SB (PO 4 3&lt; SB&gt; 4&lt; SB&gt; 2&lt; SB&gt; 2 具有耐火细粉。 版权所有(C)2006,JPO&NCIPI
    • 10. 发明专利
    • Glass tablet, method for producing the same, and glass tablet-integrated exhaust pipe
    • 玻璃板,其制造方法和玻璃板一体化排气管
    • JP2011105596A
    • 2011-06-02
    • JP2011026705
    • 2011-02-10
    • Nippon Electric Glass Co Ltd日本電気硝子株式会社
    • CHIMURA YOSHIKIIZEKI JUNICHI
    • C03C8/24H01J11/46H01J11/48H01J11/54H01J29/86
    • PROBLEM TO BE SOLVED: To provide a glass tablet having high fluidity, a method for producing the glass tablet, and a glass tablet-integrated exhaust pipe.
      SOLUTION: The glass tablet is a ring-like glass tablet comprising a glass powder and a filler powder, and do not substantially contain PbO. The method for producing the glass tablet includes steps of: uniformly mixing a glass powder containing substantially no PbO with a filler power; adding a vehicle having good thermal decomposition property to the mixture powder to prepare granules; press-forming the granules; and calcining the product. The tablet-integrated exhaust pipe is obtained by sticking the glass tablet comprising the glass powder and the filler powder containing substantially no PbO to the outer peripheral face at the tip end of the exhaust pipe made of glass.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供一种具有高流动性的玻璃片,一种玻璃片的制造方法和一种玻璃片一体式排气管。 解决方案:玻璃片是包含玻璃粉末和填料粉末的环状玻璃片,基本不含有PbO。 制造玻璃片的方法包括以下步骤:将基本上不含PbO的玻璃粉与填充剂均匀混合; 向混合物粉末中加入具有良好热分解性能的载体以制备颗粒; 压制成型颗粒; 并煅烧产品。 片剂一体化排气管是将包含玻璃粉末的玻璃片和基本上不含PbO的填料粉末粘贴到由玻璃制成的排气管的前端的外周面而获得的。 版权所有(C)2011,JPO&INPIT