    • 1. 发明专利
    • Electrode plate for nonaqueous secondary battery and nonaqueous secondary battery using it
    • 非电源二次电池电极板和非正常二次电池使用
    • JP2008146894A
    • 2008-06-26
    • JP2006330202
    • 2006-12-07
    • Matsushita Electric Ind Co Ltd松下電器産業株式会社
    • SUMIHARA MASANORI
    • H01M4/02H01M4/04H01M4/13H01M4/139H01M4/36H01M4/62H01M10/05H01M10/052H01M10/0566
    • Y02E60/122
    • PROBLEM TO BE SOLVED: To provide a nonaqueous secondary battery having high reliability and capable of shutting off current with quick responsiveness to heat generation to avoid a situation causing heat generation even when sudden exothermic reaction is caused by an internal short circuit by installing a plurality of portions having an overcurrent shutting off function in an electrode plate, and fusing the plurality of portions having the overcurrent shutting off function when current less than short circuit current flows.
      SOLUTION: When thickness of an electrode mix layer on one side of an electrode plate 25 formed by applying electrode mix layers 23a, 23b containing electrode active materials 22a, 22b to a current collector 24, drying and pressing the electrode mix layers, is represented by T, particles 21a, 21b having a particle size of T/4 to T/2 are included in the electrode plate 25.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种具有高可靠性并且能够快速响应发热的关闭电流的非水二次电池,以避免即使当通过安装内部短路引起突然的放热反应时引起发热的情况 在电极板中具有过电流关闭功能的多个部分,并且当电流小于短路电流时,将具有过电流关断功能的多个部分熔合。 解决方案:通过将包含电极活性材料22a,22b的电极混合层23a,23b施加到集电体24上而形成的电极板25的一侧上的电极混合层的厚度,干燥并压制电极混合物层, 由T表示,电极板25中包含粒径为T / 4〜T / 2的粒子21a,21b。(C)2008,JPO&INPIT
    • 4. 发明专利
    • Non-aqueous secondary battery
    • 非水性二次电池
    • JP2007103356A
    • 2007-04-19
    • JP2006245209
    • 2006-09-11
    • Matsushita Electric Ind Co Ltd松下電器産業株式会社
    • SUMIHARA MASANORIMARUYAMA HIROSHI
    • H01M4/02H01M4/04H01M4/36H01M10/05H01M10/052H01M10/0566H01M10/0585H01M10/0587
    • Y02E60/122
    • PROBLEM TO BE SOLVED: To provide a non-aqueous secondary battery capable of maintaining high capacity and proper lifetime characteristics, while suppressing the occurrence of internal short circuiting of the non-aqueous secondary battery, since as a factor for internal short circuit, four short-circuiting modes are considered which consist of an exposed portion of a positive electrode current collector of a positive electrode plate and a surface of a negative electrode mixture of a negative electrode plate, the exposed portion of the positive electrode current collector and the exposed portion of the negative electrode current collector, the surface of the positive electrode mixture of the positive electrode plate and the surface of the negative electrode mixture of the negative electrode plate, and the surface of the positive electrode mixture of the positive electrode and the expoded portion of the negative electrode current collector.
      SOLUTION: The positive electrode plate 11 and the negative electrode plate 7 have portions formed, where paint of a mixture is not coated on the current collector. An insulator layer 10, on which a paint of an insulator is coated and dried, is formed on at least either the surface of the negative electrode mixture 7a facing the exposed portion of the positive electrode current collector 5b, or the surface of the exposed portion of the positive electrode current collector 5b facing the negative electrode mixture 7a, and the exposed portion is protected.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供能够保持高容量和适当寿命特性的非水二次电池,同时抑制非水二次电池的内部短路的发生,因为作为内部短路的因素 考虑了四个短路模式,其包括正极板的正极集电体的暴露部分和负极板的负极混合物的表面,正极集电体的暴露部分和 负极集电体的露出部分,正极板的正极合剂的表面和负极板的负极混合物的表面以及正极的正极混合物的表面和被喷射的 部分负极集电体。 解决方案:正极板11和负极板7具有形成的部分,其中混合物的涂料未涂覆在集电体上。 在与正极集电体5b的暴露部分相对的负极混合物7a的至少任一个表面或露出部分的表面上形成绝缘体层10,在其上涂覆和干燥绝缘体的涂料, 的正极集电体5b面对负极混合物7a,并且暴露部分被保护。 版权所有(C)2007,JPO&INPIT
    • 6. 发明专利
    • Manufacturing method of positive plate for nonaqueous secondary battery
    • 非正式二次电池正极板的制造方法
    • JP2005340071A
    • 2005-12-08
    • JP2004159169
    • 2004-05-28
    • Matsushita Electric Ind Co Ltd松下電器産業株式会社
    • FUKUNAGA MASAOKURODA AKIRAKASHIWAGI KOKUKIYOSUZUKI GOHEISUMIHARA MASANORI
    • H01M10/05H01M4/131H01M4/1391H01M4/36H01M4/62H01M4/04H01M4/02
    • Y02P70/54
    • PROBLEM TO BE SOLVED: To provide a positive plate capable of increasing capacity by reducing binding material and thickening agent, extending life by reducing irregularity of coating weight and improving high temperature keeping properties by reducing conductive material by using an even dispersal effect of electrode plate structuring materials by improving a mixing method of the conductive material, the binding material and the thickening agent which are structuring materials other than an active material contributing to battery capacity and a large capacity nonaqueous secondary battery using the positive plate. SOLUTION: In the electrode panel structured by mixing and dispersing the active material A, the conductive material B, the rubber particle binding material C having acrylate units and the thickening agent D of water soluble polymer with water, the active material A and the conductive material B is moistened with water solution of the thickening agent D as a first mixing and then the binding material C and water are added and mixed. In the above procedure, the binding material C is 0.2 to 1.4 pts.wt. of the active material A and the conductive material B is 1.0 to 2.5 pts.wt. of the active material A. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:通过减少粘结材料和增稠剂来提供能够增加容量的正极板,通过减少涂层重量的不均匀性延长使用寿命,并通过使用均匀的分散效应减少导电材料来改善高温保持性能 电极板结构材料,通过改善导电材料,粘结材料和增稠剂的混合方法,所述导电材料,结合材料和增稠剂是构成不同于有助于电池容量的活性材料的结构材料和使用正极板的大容量非水二次电池。 解决方案:在通过混合和分散活性材料A,导电材料B,具有丙烯酸酯单元的橡胶颗粒粘合材料C和水溶性聚合物的增稠剂D与水的活性材料A和 作为第一次混合,用增稠剂D的水溶液润湿导电材料B,然后加入并混合粘结材料C和水。 在上述步骤中,粘合材料C为0.2〜1.4重量份。 的活性物质A和导电材料B为1.0〜2.5重量份。 的活性物质A.版权所有(C)2006,JPO&NCIPI
    • 8. 发明专利
    • Electrode plate for non-aqueous secondary battery, its manufacturing method, and non-aqueous secondary battery
    • 非水性二次电池电极板及其制造方法和非水性二次电池
    • JP2007328977A
    • 2007-12-20
    • JP2006158189
    • 2006-06-07
    • Matsushita Electric Ind Co Ltd松下電器産業株式会社
    • SUMIHARA MASANORI
    • H01M4/02H01M4/04H01M4/13H01M4/131H01M4/139H01M4/1391H01M4/62H01M10/05H01M10/052H01M10/058H01M10/0587
    • Y02P70/54
    • PROBLEM TO BE SOLVED: To provide a nonaqueous secondary battery which is superior in productivity, small in battery capacity unevenness and superior in life characteristics since places of different active material densities are formed at least at one electrode plate of the positive electrode plate and the negative electrode plate that is compressed to a specified thickness.
      SOLUTION: This has a first process of coating and forming a place 3 in which the thickness of a mixture paint 2 of a positive electrode or the mixture paint 2 of a negative electrode becomes thin at least at one or more places of a current collector 1, and after the mixture paint 2 of the positive electrode or the mixture paint 2 of the negative electrode is dried, it is pressed to have a prescribed thickness, and the place 5 with different active material densities is formed at least at one or more places of the positive electrode plate 11 or the negative electrode plate 12.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种生产率优异,电池容量不均匀性和寿命特性优异的非水二次电池,因为在正极板的至少一个电极板上形成不同活性物质密度的位置 和被压缩到规定厚度的负极板。 解决方案:这具有第一种涂覆和形成位置3的方法,其中正极的混合物涂料2的厚度或负极的混合物涂料2的厚度至少在一个或多个位置变薄 集电体1,在将正极的混合物涂料2或负极的混合涂料2干燥之后,将其压制成规定的厚度,至少形成一个具有不同活性物质密度的位置5 或更多个正极板11或负极板12的位置。(C)2008,JPO&INPIT
    • 9. 发明专利
    • Manufacturing method of electrode plate for secondary battery
    • 二次电池电极板的制造方法
    • JP2007311280A
    • 2007-11-29
    • JP2006141173
    • 2006-05-22
    • Matsushita Electric Ind Co Ltd松下電器産業株式会社
    • SUMIHARA MASANORI
    • H01M4/04H01M4/02H01M4/139H01M4/62
    • Y02P70/54
    • PROBLEM TO BE SOLVED: To provide a high-quality and high-density electrode plate for a nonaqueous secondary battery by suppressing crease, disconnection and warpage of the electrode plate by pressing after removing an active material mix non-application region.
      SOLUTION: In this manufacturing method of this electrode plate for a secondary battery, a positive electrode mix coating 2 is applied in a discontinued form in the longitudinal direction of a strip-like collector 1 and dried in a state where non-application regions 3 are left at both ends in the width direction of the strip-like collector 1, and then the electrode plate is pressed to a predetermined thickness with at least the non-application regions 3 at both ends in the width direction of the strip-like collector 1 removed.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:为了通过在除去活性物质混合物非施加区域之后通过压制来抑制电极板的折痕,断开和翘曲来提供用于非水二次电池的高品质和高密度电极板。 解决方案:在这种二次电池用电极板的制造方法中,将正极混合涂层2沿带状集电体1的长度方向以中断的形式进行涂布,并在非应用状态下干燥 在带状集电体1的宽度方向上的两端留有区域3,然后将电极板按压至规定厚度,至少在带状集电体1的宽度方向上的两端的非施加区域3, 像收集器1一样。 版权所有(C)2008,JPO&INPIT
    • 10. 发明专利
    • Secondary battery
    • 二次电池
    • JP2005302635A
    • 2005-10-27
    • JP2004120171
    • 2004-04-15
    • Matsushita Electric Ind Co Ltd松下電器産業株式会社
    • SUMIHARA MASANORI
    • H01M2/02
    • Y02E60/12
    • PROBLEM TO BE SOLVED: To provide a secondary battery housed in an outer case having an identification means having high identification ability and effective than existing one for preventing imitation and copying, to solve problems that although batteries using imitation outer case material or batteries having different characteristics or different kinds can be charged with a regular dedicated charger, the safety of the battery in charging is not guaranteed. SOLUTION: At least one secondary battery is housed in the outer case material, and an identification label 2 for identifying an individual piece of the secondary battery is stuck on at least one portion on the surface of the outer case material. The identification label 2 has multilayer structure, and fragility working treatment is applied to at least one layer on the multilayer. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:为了提供容纳在外壳中的二次电池,具有识别装置,具有高的识别能力并且比现有的识别装置有效,用于防止仿制和复制,以解决尽管使用仿外壳材料或电池的电池的问题 具有不同特性或不同种类可以用常规专用充电器充电,电池在充电时的安全性不能保证。 解决方案:至少一个二次电池被容纳在外壳材料中,并且用于识别二次电池的单个片的识别标签2粘贴在外壳材料的表面上的至少一部分上。 识别标签2具有多层结构,并且脆性工作处理被应用于多层上的至少一层。 版权所有(C)2006,JPO&NCIPI