    • C08F297/08C08F210/06
    • PROBLEM TO BE SOLVED: To obtain a polypropylene-based polymer that is formed at a polypropylene copolymerization stage and forms no solvent-soluble component causing reduction in physical properties. SOLUTION: The propylene-based copolymer is a polymer comprising a part (D sol ) soluble in n-decane at a room temperature and a part (D insol ) insoluble in n-decane at a room temperature and obtained from propylene (M P ) and one or more kinds of olefins (M X ) selected from ethylene and a ≥4C α-olefin and simultaneously satisfies the following requirements of (1) the molecular weight distributions (Mw/Mn) of D sol and D insol measured by using GPC are both ≤4.0, (2) the mol concentration of skeleton derived from the olefins (M X ) in the D sol in the propylene-based polymer is 10-60 mol%, (3) the weight concentration of skeleton derived from the olefins (M X ) in the D insol in the propylene-based polymer is ≤2.0 wt.% and (4) the intrinsic viscosity ([η](dl/g)) of the D sol in the propylene-based polymer is ≥1.5. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:获得在聚丙烯共聚阶段形成的聚丙烯类聚合物,不会形成导致物理性能降低的溶剂可溶性成分。 丙烯类共聚物是包含在室温下可溶于正癸烷的部分(D 溶胶)和部分(D insol )的聚合物, 在室温下不溶于正癸烷,得自丙烯(M SB SB)和一种或多种选自乙烯和≥4Cα的烯烃(M SB SB X) 同时满足以下要求:(1)通过使用GPC测量的D 溶胶和D sol 的分子量分布(Mw / Mn)均≤4.0, (2)丙烯类聚合物中的D 溶胶中衍生自烯烃(M X )的骨架的摩尔浓度为10-60摩尔%,(3) 基于丙烯的聚合物中的衍生自烯烃的骨架的重量浓度(M X )≤2.0重量%,(4)特性粘度 丙烯类聚合物中D 溶胶的([η](dl / g))≥1.5。 版权所有(C)2006,JPO&NCIPI