    • 1. 发明专利
    • JPH05249264A
    • 1993-09-28
    • JP5468091
    • 1991-03-19
    • MITSUBISHI HEAVY IND LTDMITSUBISHI ATOMIC POWER IND
    • TSUNODA HIDEOIOKI KIMIHIRO
    • G21B1/11G21B1/00G21B1/17
    • PURPOSE:To improve the integrity of heat structure by mixing metal with ceramic and composing an armor block part by means of a mixed material obtained by continuously changing its composition ratio. CONSTITUTION:An armor tile block 7 is composed of a part 4 of 100% copper, a mixed material part 5 obtained by mixing ceramic such as with tin copper and an armor tile 2 composed of carbon material such as C/C composite material, and a hole for putting through a metal-made cooling tube 1 is provided in the part 4. Compositional ratio of the part 5 indicates that copper is high in the side near the part 4 and ceramic such as tin is continuously heightened as it approches to the tile 2. And the adhesion between materials is heightened through an active metal-thin inserted material 6 such as TiC in the boundary part between the tile 2 and the part 5. Next, the cooling tube 1 is put through the hole of the part 4 and a contact face is vacuum-brazed and fixed for connection. Thereby keeping of residual stress and thermal stress is suppressed and the thermal structural integrity of the material is heightened.
    • 3. 发明专利
    • Crucible for melting metal and its manufacturing method
    • 用于熔炼金属及其制造方法
    • JP2009243723A
    • 2009-10-22
    • JP2008088799
    • 2008-03-28
    • Kenji AbikoMitsubishi Heavy Ind Ltd三菱重工業株式会社兼次 安彦
    • TSUNODA HIDEOABIKO KENJI
    • F27B14/10C04B35/057C21C7/00
    • PROBLEM TO BE SOLVED: To provide a crucible for melting metal and its manufacturing method for preventing erosion, and obtaining a robust modified layer to prevent separation of the modified layer simultaneously with separating work of molten steel attached to an inner surface, by forming uniform CaO-ZrO 2 eutectic structure not by surface coating of zirconia powder, but uniformly coating CaO with zirconia precipitating from liquid by molding and baking CaO as a raw material by using liquid zirconium chelate as a binder. SOLUTION: In this crucible for melting metal mainly composed of calcium oxide (CaO) used in a vacuum melting furnace, the powder of CaO as the raw material is molded and baked while using the liquid zirconium chelate as the binder to precipitate uniform CaO-ZrO 2 eutectic structure on CaO as aggregate. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种用于熔融金属的坩埚及其防止侵蚀的制造方法,并获得坚固的改性层,以防止与附着在内表面上的钢水分离工作同时分离改性层,由 通过氧化锆粉末的表面涂覆形成均匀的CaO-ZrO 2 共晶结构,但是通过使用液体锆螯合物作为粘合剂,通过模制和焙烧CaO作为原料,均匀地涂覆含有通过液体沉淀的氧化锆的CaO。 解决方案:在用于熔化主要由真空熔化炉中使用的氧化钙(CaO)组成的金属的坩埚中,以使用液体锆螯合物作为粘合剂的CaO作为原料的粉末进行成型和烘烤,以使均匀 CaO-ZrO 2 / SB共晶结构在CaO作为骨料。 版权所有(C)2010,JPO&INPIT
    • 5. 发明专利
    • Large sized ceramic surface plate and xy stage device
    • 大尺寸陶瓷表面板和XY阶段设备
    • JP2007075965A
    • 2007-03-29
    • JP2005268956
    • 2005-09-15
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • TSUNODA HIDEOTAZANE YOICHIKATO HITOSHIUENO DAIJIKONDO MASARU
    • B25H7/02C04B35/14
    • PROBLEM TO BE SOLVED: To provide a large sized ceramic surface plate which reduces the weight even if it is the large surface plate and an XY stage device using it. SOLUTION: The large sized ceramic surface plate 10 is composed of: a crossbeam 13 which supports a ceramic plain plate 11 by joining at least two or more ceramic plain plate 11 made of a ceramic material to abut to a ceramic plain plate joining body 12 and the joining part of the ceramic plain plate joining body 12; and the ceramic plain plate 11 so as to cover the space of at least four corners at the other end surface side of the crossbeam 13. The large sized ceramic surface plate is extremely precise, is reduced in weight, and responds to the enlargement of the ceramic surface plate. COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供一种大型陶瓷表面板,其即使是大的表面板也能减轻重量,并且使用XY平台装置。 < P>解决方案:大型陶瓷表面板10由以下部分组成:横梁13,其通过将由陶瓷材料制成的至少两个以上的陶瓷平板11接合而邻接陶瓷平板接合的陶瓷平板11 主体12和陶瓷平板接合体12的接合部分; 和陶瓷平板11,以覆盖横梁13的另一端面侧的至少四个角部的空间。大尺寸的陶瓷表面板非常精确,重量减轻,并且响应于 陶瓷表面板。 版权所有(C)2007,JPO&INPIT
    • 6. 发明专利
    • Conveying device, coating device and coating method
    • 输送装置,涂布装置和涂布方法
    • JP2006232419A
    • 2006-09-07
    • JP2005045624
    • 2005-02-22
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • TSUNODA HIDEOTAZANE YOICHI
    • B65G39/02B05B13/02B05C13/02B05D3/00
    • PROBLEM TO BE SOLVED: To apply coating to a steel plate at high treatment efficiency without generating a flaw as much as possible.
      SOLUTION: The conveying device comprising a projection roller 14 and a foaming roller 15 rotatably supported and supporting the steel plate W from a lower surface side is provided on a coating device 10. The projection roller 14 is made to a structure having a plurality of pins 22 arranged on a peripheral surface of a roller body 21 with a gap in a circumferential direction and having a ball rollably retained at a distal end of the pin 22. The foaming roller 15 is made to a structure having a foaming layer 32 comprising a porous metal material provided on a peripheral surface of the roller body 31 over a circumferential direction. The steel plate W in which front and back surface are coated with a shop primer comprising zinc-rich paint by a coating spray 12 is conveyed by the projection roller 14 and the foaming roller 15.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:以高处理效率将涂层涂覆到钢板上,而不会产生尽可能多的缺陷。 解决方案:在涂覆装置10上设置有包括从下表面侧可旋转地支撑并支撑钢板W的突出辊14和发泡辊15的输送装置。突出辊14制成具有 多个销22布置在辊主体21的周向周向表面上,周向具有间隙,并且具有可滚动地保持在销22的远端的球。发泡辊15被制成具有发泡层32的结构 包括在圆周方向上设置在辊主体31的周面上的多孔金属材料。 前面和后表面涂有包含富锌涂料的涂料喷涂12的车间底漆的钢板W由凸出辊14和发泡辊15输送。(C)2006,JPO&NCIPI
    • 7. 发明专利
    • Dimming device and method for manufacturing the same
    • 调试装置及其制造方法
    • JP2005316180A
    • 2005-11-10
    • JP2004134557
    • 2004-04-28
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • TSUNODA HIDEOKOBAYASHI KATSUAKIOKADA TOMOAKI
    • G02F1/155G02F1/15
    • PROBLEM TO BE SOLVED: To provide a dimming device which has superior transparency, which is made compact and further which is mass-produced at a low cost, and to provide a method for manufacturing the same.
      SOLUTION: The dimming device is constructed by laminating flexible first and second substrates 11, 12 placed facing each other, and a first grid electrode 13, an electrolyte layer 14, an electrochromic (EC) film 15, and a second grid electrode 16 between the first and second substrates 11, 12, and by arranging an insulating section 17 between the first and second grid electrodes 13, 16. By making the insulating section 17 interposed in between the first and second conductive grid electrodes 13, 16, contact between the first grid electrode 13 and the electrochromic (EC) film 15 is prevented.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 解决的问题:提供一种具有优异的透明度的调光装置,该调光装置被紧凑且进一步以低成本批量生产,并提供其制造方法。 解决方案:调光装置通过层叠彼此面对的柔性第一和第二基板11,12以及第一栅极13,电解质层14,电致变色(EC)膜15和第二栅极电极 16,并且通过在第一和第二栅电极13,16之间布置绝缘部分17.通过将绝缘部分17插入在第一和第二导电栅电极13,16之间进行接触 在第一栅极13和电致变色(EC)膜15之间被防止。 版权所有(C)2006,JPO&NCIPI
    • 9. 发明专利
    • Superheater tube of marine boiler
    • 海水锅炉超级管
    • JP2003083505A
    • 2003-03-19
    • JP2001276768
    • 2001-09-12
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • YAMAMOTO HIDEKUNITAKEUCHI DAISUKETSUNODA HIDEOMATSUMOTO HIROTOSHI
    • F22B37/04C22C38/00F22B37/10F22G3/00
    • PROBLEM TO BE SOLVED: To provide a superheater tube of a marine boiler.
      SOLUTION: The superheater tube of the marine boiler in the first invention is composed of a high temperature corrosion resistant material, and the superheater tube of the marine boiler in the second invention has the superheater tube body and a high temperature corrosion resistant coating layer formed on the outer surface of the superheater tube body. In the superheater tube of the marine boiler in the second invention, it is desirable that the superheater tube body is made of steel containing Cr of 2 to 2.5% pts.wt., and the coating layer is made of steel containing Cr of 18% pts.wt. and Ni of 8% pts.wt, and also the superheater tube body is made of steel containing Cr of 2 to 2.5% pts.wt., and the coating layer is made of an alloy comprising Cr of 50% pts.wt. and Ni of 50% pts.wt.
      COPYRIGHT: (C)2003,JPO
    • 要解决的问题:提供船用锅炉的过热器管。 解决方案:第一发明的船用锅炉的过热器管由耐高温材料构成,第二发明的船用锅炉的过热器管具有过热器管体和高温耐腐蚀涂层 过热器管体的外表面。 在第二发明的船用锅炉的过热器管中,期望过热器管体由含有2〜2.5重量%的Cr的钢制成,涂层由含有18重量%的Cr的钢制成, 重量 和8重量%的Ni,过热器管体由含有2〜2.5重量%的Cr的钢制成,涂层由含有50重量%的Cr的合金制成。 和Ni为50%重量