热词
    • 2. 发明专利
    • Spray coating facility
    • 喷涂设备
    • JP2014167171A
    • 2014-09-11
    • JP2014093082
    • 2014-04-28
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • NAGANO ICHIROMORI KAZUTAKAMEGA MASAHIKOTORIGOE TAIJIKAMIMURA YOSHIHISA
    • C23C4/12B05B7/20B05B7/22F01D5/28F01D9/02F01D25/00F02C7/00H05H1/32H05H1/42
    • PROBLEM TO BE SOLVED: To provide a spray coating facility for cleaning the inside of a spray coating booth.SOLUTION: A spray coating facility comprises: spray guns 11 and 71 for spraying spray coating powder to an object 1; a spray booth B, in which the object 1 and the spray guns are arranged; a suction fan 32 for sucking the gas in the spray booth; and a suction duct 31 opened in the spray booth B for introducing the gas in the spray booth into the suction fan. In the wall forming the spray coating booth B, in the wall 11 on the side of the spray guns with reference to the position, at which the object is arranged, there is formed a suction hole 39 for introducing air into the spray coating booth. Of the wall forming the spray coating booth B, in the wall on the opposite side of the spray guns with reference to the position, at which the object is arranged, a portion of a suction duct 31 on the opening side is formed, and an opening 31a is opened toward the spray guns 11 and 71.
    • 要解决的问题:提供一种用于清洁喷涂室内部的喷涂设备。解决方案:喷涂设备包括:喷枪11和71,用于将喷涂粉末喷涂到物体1上; 喷涂室B,其中物体1和喷枪布置在其中; 用于吸入喷雾室中的气体的吸风扇32; 以及在喷雾室B中开放的吸入管道31,用于将喷雾室中的气体引入吸入风扇。 在形成喷涂室B的壁上,相对于物体排列的位置,在喷枪侧的壁11中形成有用于将空气引入喷涂室中的抽吸孔39。 在形成喷涂室B的壁之间,在喷枪的相反侧的壁中,相对于物体排列的位置,形成开口侧的吸入管道31的一部分,并且 开口31a朝向喷枪11和71打开。
    • 3. 发明专利
    • Mold for precision casting and method for producing the same
    • 用于精密铸造的模具及其制造方法
    • JP2014076456A
    • 2014-05-01
    • JP2012224612
    • 2012-10-09
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • OGUMA HIDETAKAMORI KAZUTAKAOKADA IKUOSHIMOHATA SACHIO
    • B22C9/04
    • B22C3/00B22C7/02B22C9/04B22C9/06B22C9/061
    • PROBLEM TO BE SOLVED: To provide a mold for precision casting which generates no deformation even when held at a high temperature for a long time and a method for producing the same.SOLUTION: There is provided a mold for precision casting which is used for producing a casting and has a core having a shape corresponding to a cavity inside the casting and an outer mold having a shape corresponding to the outer peripheral surface of the casting, wherein the outer mold comprises: a prime layer (first dried film) 101A which is formed on the inner peripheral surface and is composed of a slurry film obtained by drying using a mold slurry for precision casting composed of monodispersed alumina (AlO) ultrafine particles having a particle diameter of 1.0 μm or less; slurry layers 102 which are formed outside the prime layer (first dried film) 101A and are composed of the mold slurry for precision casting; and a multi-layered back-up layer 105A which is obtained by forming a back-up layer (second dried film) 104-1 a plurality of times which is formed by drying stucco layers 103 in which a stucco material is adhered to the slurry layers 102.
    • 要解决的问题:提供即使在长时间保持高温下也不产生变形的精密铸造用模具及其制造方法。本发明提供一种精密铸造用模具,其用于制造 铸件,具有与铸件内部的空腔相对应的形状的芯体和具有与铸件的外周面相对应的形状的外模具,其中,外模具包括:主层(第一干燥膜)101A, 形成在内周面上,由使用由使用粒径为1.0μm以下的单分散氧化铝(AlO)超微粒子构成的精密铸造用模浆料进行干燥而得到的浆料膜构成。 浆料层102,其形成在初始层(第一干燥膜)101A的外侧,并且由用于精密铸造的模具浆料构成; 以及多层备用层105A,其通过多次形成后备层(第二干燥膜)104-1而获得,所述多层后处理层通过干燥其上附着灰泥材料的灰泥层103而形成 层102。
    • 5. 发明专利
    • Carbide tool manufacturing method
    • 碳化工具制造方法
    • JP2012024850A
    • 2012-02-09
    • JP2010162429
    • 2010-07-20
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • KIKUCHI TAIJIMORI KAZUTAKA
    • B23B27/14B22F1/00B22F3/02B23F21/16B23P15/28C22C1/05
    • PROBLEM TO BE SOLVED: To provide a carbide tool manufacturing method for manufacturing a tool made of a carbide alloy and having a further enhanced temperature characteristic.SOLUTION: The carbide tool manufacturing method includes the steps of mixing tungsten carbide and a binder at a predetermined ratio, adding a solvent thereto and kneading it, drying and granulating the mixture with a spray dryer, and manufacturing the carbide tool by press-forming and sintering the raw material powder thus obtained. Powder with a diameter of 1 to 3 μm is used as the tungsten carbide and powder consisting of cobalt is used as the binder, the cobalt having a specific surface area of 30 to 60 m/g.
    • 解决的问题:提供一种用于制造由碳化物合金制成的工具并具有进一步提高的温度特性的硬质合金刀具制造方法。 解决方案:碳化物刀具的制造方法包括以预定比例混合碳化钨和粘合剂,向其中加入溶剂并捏合,用喷雾干燥器干燥并造粒混合物,并通过压制 形成并烧结由此获得的原料粉末。 使用直径为1〜3μm的粉末作为碳化钨,使用由钴组成的粉末作为粘合剂,钴的比表面积为30〜60μm 2 / g以下。 版权所有(C)2012,JPO&INPIT
    • 6. 发明专利
    • Thermal spraying device
    • 热喷涂装置
    • JP2011168840A
    • 2011-09-01
    • JP2010033895
    • 2010-02-18
    • Mitsubishi Heavy Ind Ltd三菱重工業株式会社
    • NAGANO ICHIROTANIGAWA HIDETSUGUMEGA MASAHIKOUEDA YASUTOSHIYUASA ATSUSHIKOJIMA KATSUHISATORIGOE TAIJIKAMIMURA YOSHIHISAMORI KAZUTAKA
    • C23C4/00
    • PROBLEM TO BE SOLVED: To provide a thermal spraying device recovering non-welded thermal spray particles at high concentration, easily selecting and reusing the thermal spray particles and enhancing a utilization ratio of the thermal spray particles.
      SOLUTION: The thermal spraying device includes a first encircling body 9 forming a first internal space 11 encircling a peripheral part of a thermal spraying object 5 so that the thermal spray particles discharged from a thermal spraying gun 3 are passed, a first exhaust system 13 sucking and exhausting an atmosphere of the first internal space 11, a cyclone 27 provided in the first exhaust system 13 and selecting thermal spray particles, a second encircling body 43 forming a second internal space 45 encircling a peripheral part of the first encircling body 9 and a second exhaust system 47 sucking and exhausting an atmosphere of the second internal space 45, wherein the pressure of the atmosphere of the second internal space 45 is made lower than that of the atmosphere of the first internal space 11.
      COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题:提供一种以高浓度回收非焊接热喷雾颗粒的热喷涂装置,容易选择和重新使用热喷雾颗粒并提高热喷雾颗粒的利用率。 解决方案:热喷涂装置包括第一环绕体9,其形成围绕热喷涂体5的周边部分的第一内部空间11,使得从热喷枪3排出的热喷雾颗粒通过,第一排气 系统13吸入和排出第一内部空间11的气氛,设置在第一排气系统13中并选择热喷雾颗粒的旋风分离器27,形成围绕第一环绕体的周边部分的第二内部空间45的第二环绕体43 9和第二排气系统47吸引和排出第二内部空间45的气氛,其中使第二内部空间45的气氛的压力低于第一内部空间11的气氛的压力。 :(C)2011,JPO&INPIT