热词
    • 4. 发明专利
    • Control of desiliconation of molten iron
    • 控制铁矿石的分解
    • JPS58193307A
    • 1983-11-11
    • JP7688982
    • 1982-05-07
    • Kobe Steel LtdRiken Kogyo Kk
    • OONISHI TOSHIYASUTAKAGI WATARUKATSUTA JIYUNICHIROUTOZAWA ISAOICHIKAWA TADASHI
    • C21C1/04
    • C21C1/04
    • PURPOSE:To carry out desiliconation treatment of molten iron flowing down through a molten iron trough certainly in good efficiency, by measuring the silicon content in molten iron tapped from a shaft furnace by a thermoelectromotive force method to adjust the desiliconation condition of molten iron in the molten iron trough. CONSTITUTION:A skimmer is arranged in a course tapping molten iron from a shaft furnace through a molten iron trough to separate shaft furnace slag while the part of molten iron is sampled from the molten iron trough and poured into a casting mold to prepare a test piece. Subsequently, the thermoelectromotive force muV of the obtained test piece is measured and the silicon content in molten iron can be measured rapidly and accurately from a calibration curve; [%Si]=0.0573 X exp(muV/249). In the next step, a molten iron trough desiliconation condition such as the addition amount of a desiliconating agent is controlled corresponding to the above mentioned silicon content. By this method, proper desiliconation is carried out in good efficiency to make it possible to carry out succeeding out-furnace refining and converter refining in extremely good efficiency.
    • 目的:通过热电动势法测定从竖炉中抽出的铁水中的硅含量,通过测量铁水中的脱硅条件,对铁水槽中的铁水进行脱硅处理, 铁水槽 构成:撇渣器布置在从竖炉的铁水中通过铁水槽分离的铁水中,以分离竖炉炉渣,同时将铁水的一部分从铁水槽取样并倒入铸模中以制备试件 。 随后,测量所得测试件的热电动势muV,并且可以从校准曲线快速且准确地测量铁水中的硅含量; [%Si] = 0.0573×exp(muV / 249)。 在下一步骤中,对应于上述硅含量控制脱铁剂的添加量等铁水槽脱硅条件。 通过该方法,能够以良好的效率进行适当的脱硅,从而能够以极高的效率进行后续的精炼和转炉精炼。
    • 8. 发明专利
    • Electromagnetic stirring method of continuous casting billet of different steels
    • 连续铸钢不锈钢电磁搅拌方法
    • JPS59193743A
    • 1984-11-02
    • JP7037983
    • 1983-04-20
    • Kobe Steel Ltd
    • OONISHI TOSHIYASUWAKASUGI ISAMUOOKAMI MASAHIKOSUZUKI YASUO
    • B22D11/10B22D11/115B22D11/12
    • B22D11/115B22D11/122
    • PURPOSE:To prevent central segregaion of a continuous casting billet at the joint part and to improve the yield thereof by providing respectively electromagnetic stirrers near the water-cooled casting mold of a continuous casting device, the terminal part of solidification of the drawn billet and between said parts and operating the stirrers in accordance with a schedule. CONSTITUTION:A billet is drawn while all of the 1st-3rd electromagnetic stirrers 2a, 2b, 2c are operated during the time when the joint part of different kinds of steels moves by the length corresponding to the distance L (b-c) from the molten metal surface in a casting mold 1 to the 2nd stirrer 2b and to the 3rd stirrer 2c. The billet is drawn by stopping the 3rd stirrer 2c and operating the 1st and 2nd stirrers 2a, 2b during the time when the joint part of the different kinds of steels drawn by the length corresponding to the distance L (b-c) arrives at the 2nd stirrer 2b. The billet is drawn by operating only the 1st stirrer 2a during the time when said joint part moves to the 2nd-3rd stirrers 2b, 2c. The billet is drawn under stirring by the stirrers 2c, 2a after the joint part arrives at the stirrer 2c.
    • 目的:为了防止在连接部分连续铸造坯料的中心分离并通过在连续铸造装置的水冷铸造模具附近设置分别电磁搅拌器来提高其产量,拉伸坯料的凝固终端部分和 表示部件按照时间表操作搅拌器。 构成:当在不同种类的钢的接合部分移动相当于距离熔融金属的距离L(bc)的长度的时间期间,所有第1〜3电磁搅拌器2a,2b,2c全部被操作时, 在第1搅拌机2b和第3搅拌机2c的铸模1中的表面。 通过停止第三搅拌器2c并操作第一和第二搅拌器2a,2b,在对应于距离L(bc)的长度拉伸的不同种类的钢的接合部分到达第二搅拌器 2B。 在所述接合部移动到第2〜第3搅拌器2b,2c的时间期间,只通过操作第1搅拌器2a来抽出坯料。 在接头部分到达搅拌器2c之后,通过搅拌器2c,2a的搅拌下将钢坯拉伸。