    • Method for preventing corrosion of cast iron pipe
    • 防止铸钢管腐蚀的方法
    • JP2005342717A
    • 2005-12-15
    • JP2005178068
    • 2005-06-17
    • Dainippon Toryo Co LtdKurimoto Ltd大日本塗料株式会社株式会社栗本鐵工所
    • SAITO MASAHIKODEGUCHI TAKAAKIKAJIWARA YOSHIHISAMICHIURA YOSHISADAYAMADA YOSHIOTAME SHINICHIRO
    • F16L58/08B05D5/00B05D7/14C23C4/08C23C28/00F16L58/10
    • C23C28/00
    • PROBLEM TO BE SOLVED: To provide a method for preventing corrosion of a cast iron pipe by using a coating material which can be coated on the surface of white rust produced in outdoor temporary placing and on white rust produced in steam curing.
      SOLUTION: This method for preventing corrosion of cast iron pipe comprises the steps of (1) thermally spraying zinc, zinc-aluminum pseudoalloy, or zinc-aluminum alloy to form a thermal spray coating layer onto the outer surface of a cast iron pipe, (2) coating an aqueous two-component epoxy emulsion coating material having a solid content of not less than 5% by weight and comprising a first component of an epoxy resin having an epoxy equivalent of 475 to 1,800 and a second component of an amine curing agent having an active hydrogen equivalent (on a solid basis) of 160 to 600 onto the outer surface of the cast iron pipe to form an epoxy resin film, and (3) coating an acrylic emulsion coating material having a solid content of not less than 15% by weight on the epoxy resin film to form an acrylic resin film.
      COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:提供一种通过使用可涂覆在户外临时放置产生的白锈表面上的涂层材料和在蒸汽固化中产生的白锈来防止铸铁管的腐蚀的方法。 解决方案:这种防止铸铁管腐蚀的方法包括以下步骤:(1)热喷锌,锌铝合金或锌铝合金,以在铸铁外表面上形成热喷涂层 管,(2)涂布固体含量不小于5重量%的水性双组分环氧乳液涂料,其包含环氧当量为475至1,800的环氧树脂的第一组分和第二组分 具有160至600的活性氢当量(基于固体)的胺固化剂在铸铁管的外表面上形成环氧树脂膜,和(3)涂覆固体含量不高的丙烯酸乳液涂料 在环氧树脂膜上小于15重量%,形成丙烯酸树脂膜。 版权所有(C)2006,JPO&NCIPI
    • 9. 发明专利
    • Corrosion prevention coating on ferrous substrate and corrosion prevention method
    • 腐蚀性防腐涂料和腐蚀防治方法
    • JP2003286559A
    • 2003-10-10
    • JP2002092907
    • 2002-03-28
    • Kurimoto Ltd株式会社栗本鐵工所
    • KAJIWARA YOSHIHISASAITO MASAHIKOMICHIURA YOSHISADAKITAGAWA MASAYOSHI
    • C23C4/08C23C4/04C23F13/00
    • PROBLEM TO BE SOLVED: To provide a more perfect coating for preventing corrosion on the surface of a ferrous substrate. SOLUTION: This corrosion prevention coating comprises the first corrosion prevention layer consisting of Zn, a Zn-Al quasi-alloy, or a Zn-Al alloy formed on the surface of the substrate with thermal spraying, and the second corrosion prevention layer consisting of Al+Al 2 O 3 or an Al alloy + Al 2 O 3 , which is formed with thermal spraying and adheres to the first corrosion prevention layer. Then, the coating hardly causes such corrosion as to initiate from the second layer, because of having extremely high hardness due to the second layer, having an excellent impact resistance due to the whole composite coating, and hence rarely causing surface damages, even if the passivity on the surface is broken; does not cause corrosion in the ferrous substrate due to a sacrificial anode action of the inner layer; and revives the passivity in the broken part during the action by self-restoring. COPYRIGHT: (C)2004,JPO
    • 要解决的问题:提供一种更完美的涂层,用于防止铁基底表面的腐蚀。 解决方案:该防腐蚀涂层包括由热喷涂形成在基材表面上的Zn,Zn-Al准合金或Zn-Al合金构成的第一防腐层,第二防腐层 由Al + Al 2 3 或由Al合金+ Al 2 SBO 3组成的Al合金+ 热喷涂并粘附到第一防腐层。 然后,由于由于第二层而具有极高的硬度,因此整个复合涂层具有优异的耐冲击性,因此很少引起表面损伤,所以涂层几乎不引起从第二层引发的腐蚀,因此即使 被动的表面被打破了; 由于内层的牺牲阳极作用,不会在铁基材中引起腐蚀; 并在自我恢复的行动中恢复被破坏的被动。 版权所有(C)2004,JPO
    • 10. 发明专利
    • Apparatus for recovering coating material in powder coating
    • 用于在粉末涂料中回收涂料的装置
    • JP2003284979A
    • 2003-10-07
    • JP2002092264
    • 2002-03-28
    • Kurimoto Ltd株式会社栗本鐵工所
    • DEGUCHI TAKAAKIKAJIWARA YOSHIHISASAITO MASAHIKOMICHIURA YOSHISADA
    • B05B15/04B05B5/08B05B15/12B05D3/00B05D7/24
    • PROBLEM TO BE SOLVED: To provide an apparatus for recovering a powder coating material which sucks and recovers a floating part of the powder coating material sprayed on a pipe body heated and rotated in a coating booth before heat curing.
      SOLUTION: In the apparatus for recovering the coating material in powder coating in which the pipe body 16 heated and rotated is relatively charged in the coating booth 10, the coating booth is formed from a circulating endless filter belt 11 and a suction mouth 17 is arranged on the back face of the endless filter belt 11. Concretely, the endless filter belt 11 circulates over the top face, the depth face and the bottom face of the pipe body 16, and a port opening 19 for taking the pipe body 16 in and out is provided in this side, and the port opening 19 is adjustable in accordance with the size of the pipe body 16.
      COPYRIGHT: (C)2004,JPO
    • 要解决的问题:提供一种用于回收粉末涂料的装置,该粉末涂料在热固化之前吸收和回收喷涂在涂覆室中加热和旋转的管体上的粉末涂料的浮动部分。 解决方案:在用于回收在涂层室10中相对地加热和旋转的管体16的粉末涂料中的涂料的回收装置中,涂覆室由循环的环形过滤带11和吸嘴 17设置在环形过滤带11的背面。具体地,环形过滤带11在管体16的顶面,深度面和底面上循环,并且用于吸取管体 16的入口和出口设置在该侧,并且端口19可根据管体16的尺寸进行调节。版权所有(C)2004,JPO