    • 1. 发明专利
    • Production method of precursor fiber for obtaining carbon fiber having high strength and high elastic modulus
    • 用于获得具有高强度和高弹性模量的碳纤维的前置纤维的生产方法
    • JP2010185163A
    • 2010-08-26
    • JP2010005744
    • 2010-01-14
    • Japan Exlan Co LtdToyobo Co Ltd日本エクスラン工業株式会社東洋紡績株式会社
    • NISHIMURA HIROKAZUABE YUKIHIROHIRAO KOICHIYAMAGUCHI SHINSUKESAKURA DAISUKEWATANABE YOSHIHIRO
    • D01F6/18D01F6/54D01F9/22
    • PROBLEM TO BE SOLVED: To provide a production method of a precursor fiber capable of producing a carbon fiber with high strength and high elastic modulus.
      SOLUTION: The production method of the precursor fiber for carbon fiber comprises (1) a step of preparing a carbon nanotube-dispersed liquid by dispersing and dissolving the carbon nanotube and a polyacrylonitrile-based polymer in at least one kind of organic solvents selected from a group consisting of dimethylformamide, dimethylacetamide, N-methyl-2-pyrrolidone and dimethylsulfoxide, (2) a step of condensing the carbon nanotube dispersed liquid, (3) a step of preparing a carbon-nanotube-containing polyacrylonitrile-based polymer by coagulating the condensed carbon nanotube-dispersed liquid in a poor solvent, filtering and drying, (4) a step of preparing a spinning dope by dissolving the carbon nanotube-containing polyacrylonitrile-based polymer in an aqueous solution of rhodan salt, (5) a step of obtaining a coagulated yarn by a wet or dry/wet spinning, from the spinning dope and (6) a step of obtaining the precursor fiber of carbon fiber by drawing the coagulated yarn.
      COPYRIGHT: (C)2010,JPO&INPIT
    • 解决的课题:提供能够制造高强度,高弹性模量的碳纤维的前体纤维的制造方法。 解决方案:碳纤维前体纤维的制造方法包括(1)通过将碳纳米管和聚丙烯腈类聚合物分散溶解在至少一种有机溶剂中来制备碳纳米管分散液体的步骤 选自由二甲基甲酰胺,二甲基乙酰胺,N-甲基-2-吡咯烷酮和二甲基亚砜组成的组,(2)将碳纳米管分散液冷凝的工序,(3)制备含碳纳米管的聚丙烯腈系聚合物 (4)通过将含碳纳米管的聚丙烯腈类聚合物溶解在硫酸盐的水溶液中而制备纺丝原液的步骤,(5)通过将碳纳米管分散液冷凝在不良溶剂中,过滤和干燥, 从纺丝原液通过湿式或干式/湿式纺丝获得凝固丝的步骤,(6)通过拉伸凝固丝来获得碳纤维前体纤维的步骤。 版权所有(C)2010,JPO&INPIT
    • 5. 发明专利
    • Method for producing high-strength polyacrylonitrile-based carbon fiber
    • 生产高强度聚丙烯腈基碳纤维的方法
    • JP2011026750A
    • 2011-02-10
    • JP2010006039
    • 2010-01-14
    • Japan Exlan Co LtdToyobo Co Ltd日本エクスラン工業株式会社東洋紡績株式会社
    • NISHIMURA HIROKAZUHIRAO KOICHIYAMAGUCHI SHINSUKEWATANABE YOSHIHIRO
    • D01F9/22
    • PROBLEM TO BE SOLVED: To provide a method for producing a carbon fiber, by which the carbon fiber not having a difference between the structures of inner and outer layers and having a high tensile strength and a high tensile elastic modulus can simply be produced. SOLUTION: The method for producing the carbon fiber comprises preparing a spinning dope comprising a polyacrylonitrile-based polymer and carbon nanotubes dispersed in the polyacrylonitrile-based polymer, spinning and drawing the spinning dope to produce a carbon fiber precursor, and then subjecting the precursor to a fire-resisting treatment and a carbonization treatment. In the method. the fire-resisting treatment is performed by irradiating the carbon fiber precursor with energy rays. The carbon fiber is characterized in that Ro/Ri is 0.5-2.0, wherein Ro and Ri are the G/D ratios of the outermost layer and innermost layer of the fiber, respectively, determined with Raman spectrum. COPYRIGHT: (C)2011,JPO&INPIT
    • 待解决的问题:提供一种碳纤维的制造方法,通过该方法,内外层结构不具有高拉伸强度和高拉伸弹性模量的碳纤维可简单地 产生的。 解决方案:制备碳纤维的方法包括制备包含聚丙烯腈基聚合物的纺丝原液和分散在聚丙烯腈类聚合物中的碳纳米管,纺丝和拉伸纺丝原液以制备碳纤维前体, 耐火处理和碳化处理的前体。 在该方法中。 通过用能量射线照射碳纤维前体来进行耐火处理。 碳纤维的特征在于Ro / Ri为0.5-2.0,其中Ro和Ri分别是用拉曼光谱测定的纤维的最外层和最内层的G / D比。 版权所有(C)2011,JPO&INPIT
    • 6. 发明专利
    • Antistatic acrylic fiber and method for producing the same
    • 防静电丙烯纤维及其制造方法
    • JP2003064580A
    • 2003-03-05
    • JP2001255471
    • 2001-08-27
    • Japan Exlan Co Ltd日本エクスラン工業株式会社
    • WATANABE YOSHIHIRO
    • D06M13/463D06M13/11D06M101/28
    • PROBLEM TO BE SOLVED: To obtain an antistatic acrylic fiber having excellent durability against dyeing, washing, etc., of antistatic performances and to provide a method for producing the same.
      SOLUTION: An antistatic agent composed of a specific cationic functional group-containing polymer and an insolubilizing agent compose of a glycidyl group-containing compound are stuck to the surface of acrylic fiber under specific conditions. Consequently the acrylic fiber prevents reduction of antistatic performances even by dyeing and repeated washing, is widely usable for clothing and has durable antistatic durability since the antistatic agent and the insolubilizing agent are firmly stuck to the surface of the fiber.
      COPYRIGHT: (C)2003,JPO
    • 要解决的问题:为了获得抗静电性能的耐染色,洗涤等优异的抗静电丙烯酸纤维,并提供其制造方法。 解决方案:由特定的含阳离子官能团的聚合物组成的抗静电剂和由含缩水甘油基的化合物组成的不溶解剂在特定条件下粘附在丙烯酸纤维的表面上。 因此,丙烯酸纤维即使通过染色和反复洗涤也能防止抗静电性能的降低,因此可广泛用于衣服,并且由于抗静电剂和不溶解剂牢固地粘附在纤维的表面上,因此具有耐久的抗静电性。
    • 7. 发明专利
    • Stainproof fiber structural product
    • 防污纤维结构产品
    • JP2007046178A
    • 2007-02-22
    • JP2005229539
    • 2005-08-08
    • Japan Exlan Co Ltd日本エクスラン工業株式会社
    • WATANABE YOSHIHIRO
    • D01F8/04
    • Y02A50/235
    • PROBLEM TO BE SOLVED: To provide a highly stainproof fiber structural product in view of such problems involved in conventional these products as the decline in stainproofness durability, constituent fibers' functions and physical properties, and processability, etc., although for metal oxide microparticles with photocatalytic activity, the activity has been studied to utilize as the stainproofness of such products so far.
      SOLUTION: The stainproof fiber structural product comprises multilayer-structured fibers in such a way that porous layers and dense layers are alternately arranged, wherein stainproof fibers with metal oxide microparticles having photocatalytic activity contained in the dense layers are used at least part of this product.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供高度防污的纤维结构产品,鉴于传统这些产品中涉及的那些问题,因为防污性耐久性,组分纤维的功能和物理性能以及加工性等的降低,尽管对于金属 具有光催化活性的氧化物微粒,已经研究了活性作为迄今为止这种产品的防污性。 防污纤维结构产品包括多层结构纤维,使得多孔层和致密层交替布置,其中具有包含在致密层中的具有光催化活性的金属氧化物微粒的防污纤维使用至少部分 这个产品。 版权所有(C)2007,JPO&INPIT
    • 9. 发明专利
    • Volatile organic compound removing fiber
    • 挥发有机化合物去除纤维
    • JP2006265811A
    • 2006-10-05
    • JP2006011132
    • 2006-01-19
    • Japan Exlan Co Ltd日本エクスラン工業株式会社
    • WATANABE YOSHIHIROTANAKA KOICHI
    • D01F1/10A61L9/00A61L9/01B01J35/02B82Y5/00B82Y30/00D01D1/06D01F6/18D01F8/04D01F8/08D03D15/00D04H1/43
    • Y02A50/235
    • PROBLEM TO BE SOLVED: To provide a fiber containing metal oxide fine particles having photocatalytic activities, and capable of removing a volatile organic compound; and to provide a volatile organic compound-removing fiber structure having the volatile organic compound-removing fiber at least a part.
      SOLUTION: The volatile organic compound-removing fiber comprises the metal oxide fine particles having the photocatalytic activities, and has ≥80% rate of rejection of the volatile organic compound. Preferably, the metal oxide fine particle is titanium oxide, and has 10-100 nm particle diameter. The strand is a multilayered structural fiber having an alternately arranged porous layer and dense layer, and the metal oxide fine particles are contained in the dense layer. The volatile organic compound-removing fiber structure has the volatile organic material-removing fiber at least as a part.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供具有光催化活性的能够除去挥发性有机化合物的含有金属氧化物微粒的纤维, 并且提供至少一部分具有挥发性有机化合物去除纤维的挥发性有机化合物去除纤维结构体。 解决方案:挥发性有机化合物除去纤维包含具有光催化活性的金属氧化物细颗粒,并且具有≥80%的挥发性有机化合物的排斥率。 优选地,金属氧化物微粒是氧化钛,并且具有10-100nm的粒径。 该链是具有交替排列的多孔层和致密层的多层结构纤维,并且金属氧化物细颗粒包含在致密层中。 挥发性有机化合物去除纤维结构至少具有挥发性有机材料除去纤维。 版权所有(C)2007,JPO&INPIT
    • 10. 发明专利
    • Water-absorbing acrylic fiber and method for producing the same and fiber structure containing the fiber
    • 吸水性丙烯酸纤维及其制造方法和纤维的纤维结构
    • JP2003342831A
    • 2003-12-03
    • JP2002155263
    • 2002-05-29
    • Japan Exlan Co Ltd日本エクスラン工業株式会社
    • WATANABE YOSHIHIRO
    • D01F6/54D03D15/00
    • PROBLEM TO BE SOLVED: To provide water-absorbing acrylic fibers which have sufficient mechanical characteristics, sufficient antistaticity, an excellent water-absorbing speed and an excellent water absorption rate, to provide a method for producing the fibers, and to provide a fiber structure containing the fibers. SOLUTION: The water-absorbing acrylic fibers are obtained by spinning a spinning dope comprising a polymer mixture consisting of 95 to 99 wt.% of an acrylonitrile-based polymer containing acrylonitrile units in an amount of ≥80 wt.% and 1 to 5 wt.% of an acrylic antistatic resin containing acrylonitrile units in an amount of 10 to 70 wt.%, and has a water-absorbing speed of ≥0.15 g/g and a water absorption rate of ≥20 wt.%. COPYRIGHT: (C)2004,JPO
    • 要解决的问题:提供具有足够的机械特性,足够的抗静电性,优异的吸水速度和优异的吸水率的吸水性丙烯酸纤维,以提供纤维的制造方法,并提供一种 含有纤维的纤维结构。 吸水性丙烯酸纤维通过纺丝纺丝原液得到,该纺丝原液包含由95〜99重量%的丙烯腈系聚合物组成的聚合物混合物,丙烯腈系聚合物含有≥80重量%的丙烯腈单元,1重量% 至5重量%的含有10至70重量%的丙烯腈单元的丙烯酸类抗静电树脂,并且吸水速度≥0.15g/ g,吸水率≥20重量%。 版权所有(C)2004,JPO