会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明专利
    • Horizontal type continuous casting machine
    • 卧式连续铸造机
    • JPS6195747A
    • 1986-05-14
    • JP21589484
    • 1984-10-15
    • Ishikawajima Harima Heavy Ind Co LtdNippon Kokan Kk
    • FUJITA YONEAKIFUKUDA SHUZOOTSUKI MASAAKIKITAGAWA TORUTAZOE NOBUHIRO
    • B22D11/06
    • B22D11/0608
    • PURPOSE:To provide a horizontal type continuous casting machine which permits the simple and easy size setting of a casting mold by pressing the side faces on one side of the metallic blocks of upper, lower, right and left endless belts to the outside surfaces of the proximity blocks thereby forming the casting mold and changing optionally the width or thickness of the casting mold without exchanging the endless belts. CONSTITUTION:The end faces 19b, 20b, 21b, 22b on one side of the metallic blocks 15, 16, 17, 18 in the upper, lower, right and left endless belts 19, 20, 21, 22 are pressed to the outside surfaces 19a, 20a, 21a, 22a of the proximity metallic blocks to form the continuous casting mold. The mutual positions of the belts 19, 20, 21, 22 are changed, by which the size of the casting mold is changed and set as desired. The need for exchanging the belts 19, 20, 21, 22 is eliminated and the changing and setting of the mold size are made extremely simple and easy.
    • 目的:提供一种卧式连续铸造机,其通过将上,下,右和左环形带的金属块的一侧上的侧面按压到所述铸造模具的外表面,允许简单且容易地对铸模进行尺寸设定 接近块由此形成铸模,并且可选地改变铸模的宽度或厚度而不更换环形带。 构成:将上,下,右,左环形带19,20,21,22中的金属块15,16,17,18的一侧上的端面19b,20b,21b,22b按压到外表面 19a,20a,21a,22a,形成连续铸模。 改变带19,20,21,22的相互位置,根据需要改变和设定铸模的尺寸。 消除了对带19,20,21,22的更换的需要,并且使模具尺寸的改变和设置变得非常简单和容易。
    • 2. 发明专利
    • Method for dissipating wave of pouring basin in continuous casting machine
    • 连续浇注机排水波浪方法
    • JPS6138751A
    • 1986-02-24
    • JP16106984
    • 1984-07-31
    • Ishikawajima Harima Heavy Ind Co LtdNippon Kokan Kk
    • FUKASE HISAHIKOMATSUI KUNIOTAZOE NOBUHIROFUKUDA SHUZOOTSUKI MASAAKINISHIOKA SHINICHI
    • B22D11/06B22D11/10B22D11/11B22D11/112B22D11/116
    • B22D11/064
    • PURPOSE:To suppress the waving of a pouring basin and to produce a steel plate having good quality by applying horizontally a magnetic field to the surface of the surface of the pouring basin in a continuous casting machine and conducting electricity thereto in the horizontal direction and the direction intersecting orthogonally with the magnetic field. CONSTITUTION:This continuous casting machine produces the steel plate 5 by storing the molten steel 3 supplied from a nozzle 6 to form the pouring basin 8 above a pair of cooling rolls 1, 2 disposed to face each other apart at a prescribed spacing, rotating the rolls 1, 2 to move the solidified layer of the molten steel 3 formed atop the same and casting the steel plate. The magnetic field is formed forward and backward in the horizontal direction to the surface part of the above-mentioned pouring basin 8 by coils 7 provided before and behind the same and the electricity is conducted between a pair of electrodes 9 and 10 provided on the right and left in the direction intersecting orthogonally therewith to generate the electromagnetic force in the pouring basin 8 from above to below. The waving of the surface of the basin 8 is thus dissipated and the generation of defects such as double skins and cracks of the steel plate 5 is prevented.
    • 目的:为了抑制浇注盆的挥动,并且通过在连续铸造机中向倾倒盆的表面水平施加磁场并在水平方向上导通电力而制造具有良好质量的钢板,并且 方向与磁场正交相交。 构成:该连续铸造机通过储存从喷嘴6供给的钢水3来形成钢板5,以在规定间隔彼此分开配置的一对冷却辊1,2的上方形成倾倒盆8, 辊1,2移动形成在其上的钢水3的凝固层并浇铸钢板。 磁场通过设置在上述倾倒盆8的前后的线圈7在水平方向上向前和向后形成,并且在右侧设置的一对电极9和10之间传导电力 并且与正交相交的方向离开,从而从倾斜盆8的上方向下方产生电磁力。 因此,盆8的表面的波动被消散,并且防止了钢板5的缺陷如双面和裂纹的产生。
    • 3. 发明专利
    • Continuous casting method
    • 连续铸造方法
    • JPS6199545A
    • 1986-05-17
    • JP21871784
    • 1984-10-19
    • Ishikawajima Harima Heavy Ind Co LtdNippon Kokan Kk
    • OZEKI AKIYAHOSHIDA TATSUOSATO HIROAKIFUKUDA SHUZOOTSUKI MASAAKIFUKASE HISAHIKOMATSUI KUNIO
    • B22D11/06
    • B22D11/0631B22D11/0608
    • PURPOSE:To cast stably and continuously an ingot having a uniform surface by providing a molten metal pouring chamber formed with a molten metal outflow slit port between both side walls along a gate in a casting mold. CONSTITUTION:A casting mold 8 which is open in the upper part is formed of a U-shaped channel formed of the bottom wall 1 consisting of the endless belt and both side walls 3, 4 consisting of the endless belts and a gate 10 provided at one end of the U-shaped channel. The wall 1 and the walls 3, 4 are moved at the same speed in the same direction, by which the ingot is continuously cast in the mold 8. The molten metal pouring chamber 11 formed with the molten metal outflow slit port is provided between the walls 3 and 4 along the gate 7 in said mold 8.
    • 目的:通过在浇铸模具中沿浇口的两个侧壁之间设置熔融金属流出狭缝口,形成熔融金属浇注室,从而稳定连续铸造具有均匀表面的锭料。 构成:在上部开口的铸模8由由环形带构成的底壁1和由环形带构成的两个侧壁3,4形成的U形通道形成,并且设置在门10上 U形通道的一端。 壁1和壁3,4以相同的方向以相同的方向移动,通过该方向铸块连续铸造在模具8中。形成有熔融金属流出狭缝口的熔融金属浇注室11设置在 在模具8中沿门7的壁3和4。
    • 4. 发明专利
    • Continuous casting method
    • 连续铸造方法
    • JPS6199543A
    • 1986-05-17
    • JP21871584
    • 1984-10-19
    • Ishikawajima Harima Heavy Ind Co LtdNippon Kokan Kk
    • SATO HIROAKIKUNIOKA KAZUOOTSUKI MASAAKINISHIOKA SHINICHITSUCHIDA HIROSHITAKAHASHI SHUZO
    • B22D11/06B22D11/08
    • B22D11/0631B22D11/0608B22D11/08
    • PURPOSE:To cast stably and continuously an ingot having a uniform surface by advancing a gate for a specified period in synchronization with a bottom wall consisting of an endless belt and both side walls consisting of endless belts then retreating the gate to the home position. CONSTITUTION:A casting mold 8 which is open in the upper part is formed of a U-shaped channel formed of the bottom wall 1 consisting of the endless belt and both side walls 3, 4 consisting of the endless belts moving at the same speed in the same direction and a gate 7 provided at one end of the U-shaped channel. A molten metal is supplied into such mold 8 and the ingot is cast in the mold 8; at the same time, the ingot is continuously drawn in synchronization with the wall 1 and the walls 3, 4 from the mold 8 inside and is thus continuously cast. The gate 7 is advanced for the specified period in synchronization with the wall 1 and the walls 3, 4 and is then retreated to the home position.
    • 目的:通过与由环形带组成的底壁和由环形带组成的两个侧壁同步地将门推进一定时间段来稳定地连续铸造具有均匀表面的锭,然后将门退回原位。 构成:在上部开口的铸模8由由环形带构成的底壁1和由以相同速度移动的环形带组成的两个侧壁3,4形成的U形通道形成, 相同的方向和设置在U形通道的一端的门7。 将熔融金属供给到这种模具8中,铸锭铸造在模具8中; 同时,铸锭与壁1和壁3,4同步地从模具8内部连续拉出并因此连续铸造。 门7与壁1和壁3,4同步前进指定的时间段,然后退回原位。
    • 5. 发明专利
    • Continuous casting method
    • 连续铸造方法
    • JPS6199544A
    • 1986-05-17
    • JP21871684
    • 1984-10-19
    • Ishikawajima Harima Heavy Ind Co LtdNippon Kokan Kk
    • KITAGAWA TORUNISHIOKA SHINICHISATO HIROAKIFUKUDA SHUZOOTSUKI MASAAKIFUKASE HISAHIKOMATSUI KUNIO
    • B22D11/06
    • B22D11/0608B22D11/0631
    • PURPOSE:To cast stably and continuously an ingot having a uniform surface by forming a vertical groove of a narrow width between both side walls in the corner part on the surface of a gate faced to the inside of a casting mold toward the height direction thereof. CONSTITUTION:A casting mold 8 which is open in the upper part is formed of a U-shaped channel formed of the bottom wall 1 consisting of the endless belt and both side walls 3, 4 consisting of the endless belts and a gate 10 provided at one end of the U-shaped channel. The wall 1 and the walls 3, 4 are moved at the same speed in the same direction by which the ingot is continuously cast in the mold 8. The vertical groove 11 of the narrow width is formed between the walls 3 and 4 in the corner part of the surface 10a of the gate 10 faced to the mold 8 toward the height direction thereof.
    • 目的:通过在浇铸模内侧的浇口表面的拐角部分的两个侧壁的高度方向上形成宽度窄的垂直槽,稳定地连续铸造出具有均匀表面的铸块。 构成:在上部开口的铸模8由由环形带构成的底壁1和由环形带构成的两个侧壁3,4形成的U形通道形成,并且设置在门10上 U形通道的一端。 壁1和壁3,4以相同的方向以相同的方向移动,通过该方向,铸锭连续铸造在模具8中。窄的宽度的垂直槽11形成在角部的壁3和4之间 门10的表面10a的一部分朝向模具8的高度方向。
    • 6. 发明专利
    • Continuous casting method
    • 连续铸造方法
    • JPS6199542A
    • 1986-05-17
    • JP21871484
    • 1984-10-19
    • Ishikawajima Harima Heavy Ind Co LtdNippon Kokan Kk
    • SATO HIROAKIFUKUDA SHUZOOTSUKI MASAAKIKITAGAWA TORUTSUCHIDA HIROSHITAKAHASHI SHUZO
    • B22D11/06
    • B22D11/0608B22D11/0631
    • PURPOSE:To cast stably and continuously an ingot having a uniform surface characteristic by moving intermittently a bottom wall consisting of an endless belt and both side walls consisting of endless belts at a specified pitch. CONSTITUTION:A casting mold 8 which is open in the upper part is formed of a U-shaped channel formed of the bottom wall 1 consisting of the endless belt and both side walls 3, 4 consisting of the endless belts moving at the same speed in the same direction and a gate 7 provided at one end of the U-shaped channel. A molten metal is supplied into such mold 8 and the ingot is cast in the mold 8; at the same time, the ingot is continuously drawn in synchronization with the wall 1 and the walls 3, 4 from the mold 8 inside and is thus continuously cast. The wall 1 and the walls 3, 4 are intermittently moved at a specified pitch.
    • 目的:通过间歇地移动由环形带构成的底壁和以规定间距由环形带组成的两个侧壁,能够稳定且连续地铸造具有均匀表面特性的铸锭。 构成:在上部开口的铸模8由由环形带构成的底壁1和由以相同速度移动的环形带组成的两个侧壁3,4形成的U形通道形成, 相同的方向和设置在U形通道的一端的门7。 将熔融金属供给到这种模具8中,铸锭铸造在模具8中; 同时,铸锭与壁1和壁3,4同步地从模具8内部连续拉出并因此连续铸造。 壁1和壁3,4间隔地以特定的间距移动。
    • 7. 发明专利
    • Continuous casting machine
    • 连续铸造机
    • JPS6195748A
    • 1986-05-14
    • JP21589584
    • 1984-10-15
    • Ishikawajima Harima Heavy Ind Co LtdNippon Kokan Kk
    • FUKUDA SHUZOSATO HIROAKIOTSUKI MASAAKIHOSHIDA TATSUOFUKAI TOSHIYUKI
    • B22D11/06
    • B22D11/0688
    • PURPOSE:To provide a titled continuous casting machine which cools satisfactorily the metallic blocks of at least a pair of endless belts moving synchronously in the same direction with an extremely simple and inexpensive installation by cooling the outside metallic blocks of said metallic blocks with water from the top and bottom surface sides. CONSTITUTION:The top and bottom surfaces of the outside metallic block arrays 24b 25b of the endless belts 24, 25 consisting of the metallic blocks and moving synchronously in the same direction are cooled by the cooling water injected from the cooling water nozzles 38, 45 of cooling means 31, 32. The water is discharged 40, 46. The blocks 24b, 25b are satisfactorily cooled by and with the extremely simple method and inexpensive installation.
    • 目的:提供一种标称的连续铸造机,其使用至少一对环形带的金属块通过非常简单且廉价的装置以相当的方向同时冷却金属块的外部金属块, 顶面和底面两侧。 构成:由金属块组成的环形带24,25的外侧金属块组件24b 25b的顶面和底面由相同方向同步移动,由从冷却水喷嘴38,45注入的冷却水冷却 冷却装置31,32。水被排出40,46。块24b,25b通过非常简单的方法和廉价的安装令人满意地冷却。
    • 8. 发明专利
    • Cooling device for block type continuous casting machine
    • 块式连续铸造机的冷却装置
    • JPS6195745A
    • 1986-05-14
    • JP21589284
    • 1984-10-15
    • Ishikawajima Harima Heavy Ind Co LtdNippon Kokan Kk
    • OTSUKI MASAAKIINAMOTO KINYAHOSHIDA TATSUOSATO HIROAKIOGAWA AKIRA
    • B22D11/06
    • B22D11/0688
    • PURPOSE:To provide a titled device which circulates cooling water by making effective use of an installation space and to improve the durability of a cooling system by connecting the self-sealing joints in the cooling water inlets and outlets of the metallic blocks of an endless belt to the self-sealing joints of a driving shaft to face said joints. CONSTITUTION:Water paths 45 of the adjacent plural metallic blocks 22 of the endless belt are connected to the equal-pitch inlets and outlets 50, 52 of the self-sealing joints 51a, 53a of headers 46, 47 moving synchronously with the endless belt by means of pipes 48, 49. The equal-pitch self-sealing joints 51b, 53b of the driving shaft 28 of the endless belt are provided by the air pressures 59, 65 from swivel joints 57, 63 during the time when the joints rotated from the position M to N to make joint-to-joint connection, thus feeding water 58 to the water paths 45 and discharging 74 the same therefrom. The space in the endless belt is effectively utilized and since there is no part to be excessively deformed by the use of the conventional flexible hoses, the durability is improved.
    • 目的:提供一种通过有效利用安装空间来循环冷却水并通过连接环形带的金属块的冷却水入口和出口中的自密封接头来提高冷却系统的耐久性的标题装置 到驱动轴的自密封接头以面对所述接头。 构成:环形带的相邻多个金属块22的水路45连接到与环形带同步移动的集管46,47的自密封接头51a,53a的等间距入口和出口50,52 管道48,49的装置。环形带的驱动轴28的等间距自密封接头51b,53b由关节旋转时的旋转接头57,63的空气压力59,65提供。 位置M到N进行关节连接,从而将水58与水路45和排出口74相同。 有效利用环形带中的空间,并且由于通过使用常规柔性软管不会使部分过度变形,所以耐久性提高。
    • 9. 发明专利
    • Continuous casting device
    • 连续铸造装置
    • JPS61140353A
    • 1986-06-27
    • JP26287684
    • 1984-12-14
    • Ishikawajima Harima Heavy Ind Co LtdNippon Kokan Kk
    • KITAGAWA TORUNISHIOKA SHINICHIHOSHIDA TATSUOFUKUDA SHUZOOTSUKI MASAAKITSUCHIDA HIROSHITAKAHASHI SHUZO
    • B22D11/06
    • B22D11/0637B22D11/0608
    • PURPOSE:To produce a continuous casting ingot having a uniform surface and inside compsn. in a continuous casting mold constituted of a bottom wall, both side walls and gate formed of metallic blocks into an endless state by providing a heating mechanism near the surface of the gate facing the mold. CONSTITUTION:The casting mold 8 is constituted by attaching the refractory gate 7 to one end of the U-shaped space constituted of the bottom wall 1 and the both side walls 3, 4 formed of the many metallic blocks 2, 5, 6. A molten metal D is poured therein and the bottom wall 1 and both side walls 3, 4 are respectively moved in directions A, B, C. The molten metal is drawn out as the continuous casting ingot 9 toward the direction E. The heating element is provided near the surface of the gate 7 facing the mold 8 to heat said surface to 600-1,200 deg.C, by which the solidified shell 9b of the molten metal is generated on the inside surface 7a without being connected to the solidified shell 9a generated on the bottom wall 1 and both side walls 3, 4. The instability at the solidification initiation point on the gate 7 side according to the drawing out of the ingot 9 is obviated and the stable production of the ingot having no defects such as breakout is made possible.
    • 目的:生产具有均匀表面和内部组成的连铸铸锭。 在通过在面对模具的门的表面附近提供加热机构的由底壁,两侧壁和由金属块形成的连续浇铸的连续浇铸模中,形成环状。 构成:通过将耐火门7安装在由底壁1和由许多金属块2,5,6形成的两个侧壁3,4构成的U形空间的一端构成铸造模8。 将熔融金属D倒入其中,底壁1和两个侧壁3,4分别在方向A,B,C上移动。熔融金属作为连续铸锭9朝向E方向被拉出。加热元件为 设置在门7的面对模具8的表面附近,以将所述表面加热到600-1200℃,由此熔融金属的凝固壳体9b在内表面7a上产生,而不与生成的凝固壳体9a相连 在底壁1和两个侧壁3,4上。根据铸锭9的拉出,门7侧的凝固起始点的不稳定性被消除,并且没有诸如突破的缺陷的锭的稳定生产是 成为可能
    • 10. 发明专利
    • Continuous casting method
    • 连续铸造方法
    • JPS6138747A
    • 1986-02-24
    • JP16106584
    • 1984-07-31
    • Ishikawajima Harima Heavy Ind Co LtdNippon Kokan Kk
    • FUKASE HISAHIKOMATSUI KUNIOTAZOE NOBUHIROKITAGAWA TORUSATO HIROAKIOTSUKI MASAAKI
    • B22D11/06
    • B22D11/0631B22D11/0697
    • PURPOSE:To prevent the generation of defects such as double skins and cracks in a deep channel endless track type continuous casting devide by injecting an inert gas or powder for suppressing waving to the free surface of the molten metal in a casting mold. CONSTITUTION:The molten metal 5 such as molten steel is poured from a nozzle 9 into the casting mold 4 of the deep channel type constituted of endless track mold walls 2, 3 and mold bottoms 6. The mold walls 2, 3 and bottoms 6 forming the mold 4 are moved endlessly to produce a steel ingot. A shielding plate 10 is provided in such a manner that the bottom end on the down stream side of the nozzle 9 contacts with the top surface of the molten steel 5 and the inert gas 12 such as N2 or powder such as glass powder is blown from plural nozzles 11 to the free surface of the molten steel 5 in the mold 4 on the down stream. The waving of the free surface of the molten steel 5 is suppressed and the free surface is eliminated upon solidification. The generation of detects such as double skins and cracks to the steel ingot as a result of the waving of the molten steel surface is thus prevented.
    • 目的:通过在铸模中注入惰性气体或粉末以抑制熔融金属的自由表面,防止在深沟道环形轨道式连续铸造中产生诸如双层皮和裂纹的缺陷。 构成:将熔融金属5(例如钢水)从喷嘴9注入到由环形轨道模具壁2,3和模底部6构成的深沟道型铸模4中。模具壁2,3和底部6形成 模具4不断地移动以产生钢锭。 以这样的方式设置屏蔽板10,使得喷嘴9的下游侧的底端与钢水5的上表面接触,并且诸如N 2的惰性气体12或诸如玻璃粉末的粉末从 多个喷嘴11连接到下游的模具4中的钢水5的自由表面。 钢筋5的自由表面的挥动受到抑制,固化时消除自由面。 因此防止了由于钢水表面的挥动而对钢锭产生诸如双面和裂纹的检测。