热词
    • 1. 发明专利
    • Wind-welding method
    • 风焊方法
    • JPS5930472A
    • 1984-02-18
    • JP14066582
    • 1982-08-13
    • Ishikawajima Harima Heavy Ind Co Ltd
    • MINODA KAZUYUKITANIYAMA NARIAKI
    • B23K9/02B23K33/00
    • B23K33/00
    • PURPOSE:To reduce the generation rate of undercut and incomplete fusion, by wind-welding a corner of the end part of a member by chamfering, R-finishing or groove-cutting. CONSTITUTION:A corner of the end part of a member 1 in case of wind-welding is brought to chamfering of >=2C, or R-finishing of >=2R. Or with respect to a corner of the member 1 and a range of about 50mm. for the corner, edge preparation of about 45 deg. is executed. In this way, generation of undercut and generation of incomplete fusion of a padding welding route part are prevented, the workability is improved and the reliability is raised.
    • 目的:为了减少底切和不完全融合的发生率,通过倒角,R精加工或切槽来对构件端部的角进行风焊。 构成:风切割时,构件1的端部的一个角部进行> = 2C的倒角或> = 2R的R精加工。 或者相对于构件1的角部和约50mm的范围。 为角落,边缘准备约45度。 被执行。 这样,防止了衬底焊接路径部分的底切产生和不完全融合的产生,提高了可加工性,提高了可靠性。
    • 2. 发明专利
    • T SHAPED JOINT
    • JPS632585A
    • 1988-01-07
    • JP14417586
    • 1986-06-20
    • ISHIKAWAJIMA HARIMA HEAVY IND
    • NAKAMUTA HIROSHITANIYAMA NARIAKI
    • B23K33/00B23K9/02
    • PURPOSE:To restrain the area occupied by a depositing metal smaller, to reduce the amount of a filler metal and shorten the welding time by forming the soft toe part becoming the weld zone with its projection in advance at both sides of one end of a bone member. CONSTITUTION:The soft toe part 7 becoming the weld zone onto a skin plate 2 is formed with its projection in advance at both sides of one end of a skelton member 6. The soft toe part 7 has the 1st inclined face 7a inclining so as to increase the plate thickness of the skelton member 6 gradually toward the one end and the 2nd inclined face 7b forming a groove in the space with the skin plate 2 with its inclining so as to reduce the plate thickness of the skelton member 6 gradually toward the one end from the tip of this inclined face 7a, and the cross sectional shape makes an about triangular shape. An adequate R is made on the part (A) connecting to the side face 6a of the bone member 6 by the 1st inclined face 7a and the generation of stress concentration is prevented. The angle theta for the skin plate 2 of the 2nd inclined face 7b is 0 deg.
    • 5. 发明专利
    • WELD LINE PROFILING DEVICE
    • JPS6349369A
    • 1988-03-02
    • JP19022786
    • 1986-08-13
    • ISHIKAWAJIMA HARIMA HEAVY IND
    • TANIYAMA NARIAKITEJIMA AKIO
    • B23K9/127B23K9/02
    • PURPOSE:To perform the fillet welding along a weld line at a high speed by detecting a welding current or the arc voltage of two welding wires and comparing the values to detect a deviation of torches from the weld line and sliding the torches to correct the deviation. CONSTITUTION:The welding currents flowing between the tips of the respective welding wires 8 and 8', and base metal 1 are detected by ammeters 13 and 14 respectively the these detected currents are sent to a comparison computing element 15. The comparison computing element 15 compares the detected currents and in case the difference between both the detected currents is positive or negative, a slide motor 7 is rotated normally or rotated reversely by a normal and reverse rotation commanding device 17 to slide and move a sliding device 6. The welding torches 4 and 4' are moved in a direction to cross at right angles with the weld line 2 together with the welding wires 8 and 8' and stopped at the position where intervals between the tips of the respective welding wires 8 and 8' and the base metal 1 become equal. The tips of the welding wires 8 and 8' are advanced along the weld line 2 without weaving to perform the fillet welding at the high speed by performing the above-mentioned control continuously.