会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明专利
    • Motor control device
    • 电机控制装置
    • JP2010178488A
    • 2010-08-12
    • JP2009017760
    • 2009-01-29
    • Honda Motor Co Ltd本田技研工業株式会社
    • FUKUI TAKAHIROOKAMURA AKIHIROTAKAHASHI YUTAKAHARADA ATSUSHIOKAMOTO MASAKI
    • H02P6/08H02P21/00H02P27/04
    • PROBLEM TO BE SOLVED: To provide a motor control device which suppresses a decrease in the maximum output power of a motor that is caused by the fluctuation of power voltage in a motor driving circuit or the effect of individual irregularities of motor performance. SOLUTION: The motor control device includes a power control unit 100 which sets a larger upper limit leading angle θa_lmt, which is the upper limit of a current leading angle, as an output voltage Vpin from a battery 60 lowers, and an upper limit output setting unit 40 which sets a smaller upper limit output power of the motor 70 as the output voltage Vpin from the battery 60 lowers and sets an upper limit torque Tr_lmt corresponding to the upper limit output power and the rotation speed MOT_rpm of the motor 70, and a controller 1 which generates control signals UH, UL, VH, VL, WH, and WL to a PDU 50 so that the current leading angle does not exceed the upper limit leading angle θa_lmt and an output torque of the motor 70 does not exceed the upper limit torque Tr_lmt. COPYRIGHT: (C)2010,JPO&INPIT
    • 要解决的问题:提供一种电动机控制装置,其抑制由电动机驱动电路中的电力电压的波动引起的电动机的最大输出功率的降低或电动机性能的各种不规则的影响。 电动机控制装置包括功率控制单元100,其将来自电池60的输出电压Vpin设定为作为电流前导角的上限的较大上限前导角θa_lmt下降,并且上部 限制输出设定单元40,其设定作为电池60的输出电压Vpin的电动机70的较小上限输出功率下降,并且设定与电动机70的上限输出功率和转速MOT_rpm相对应的上限转矩Tr_lmt 以及控制器1,其向PDU 50产生控制信号UH,UL,VH,VL,WH和WL,使得当前引导角不超过上限引导角θa_lmt,并且电动机70的输出转矩不 超过上限转矩Tr_lmt。 版权所有(C)2010,JPO&INPIT
    • 3. 发明专利
    • Releasing agent for casting and casting method using the same
    • 使用其铸造和铸造方法的释放剂
    • JP2004154833A
    • 2004-06-03
    • JP2002323599
    • 2002-11-07
    • Honda Motor Co Ltd本田技研工業株式会社
    • HARADA ATSUSHI
    • B22C3/00B22C9/06
    • PROBLEM TO BE SOLVED: To provide a releasing agent reducing an oxide film which is formed on the surface of molten metal in casting.
      SOLUTION: A reducing agent (calcium hydride: CaH
      2 ) in a releasing agent 6 is decomposed into Ca and H
      2 by the remaining heat of a mold and the heat of the molten metal. These Ca and H
      2 are combined with oxygen in the cavity to become CaO and H
      2 O respectively. Thus, oxygen in the cavity is consumed so that MgO and Al
      2 O
      3 are hard to be formed. Even if some amount of oxygen left in the cavity is reacted with Mg or Al existing in the molten metal to become an oxide film of MgO or Al
      2 O
      3 , these MgO and Al
      2 O
      3 are reduced, as shown in the following formulas, so that the film is eliminated and fluidity is secured. Namely, the formulas are MgO + Ca → Mg + CaO and Al
      2 O
      3 + 3Ca → 2Al + 3CaO.
      COPYRIGHT: (C)2004,JPO
    • 解决方案:提供一种还原在铸造中形成在熔融金属表面上的氧化膜的脱模剂。 解决方案:脱模剂6中的还原剂(氢化钙:CaH 2 )通过模具的剩余热分解为Ca和H 2 ,并且 熔融金属的热量。 这些Ca和H 2 与空腔中的氧气分别成为CaO和H 2 O。 因此,空腔中的氧被消耗,使得难以形成MgO和Al 2 SB 3 O 3。 即使留在空腔中的一定量的氧气与存在于熔融金属中的Mg或Al反应,成为MgO或Al O 3 的氧化膜,这些MgO 并且如下式所示,还原Al 2 O 3 SB 3,从而消除膜并确保流动性。 即,式为MgO + Ca→Mg + CaO和Al 3 SB 3 + 3Ca→2Al + 3CaO。 版权所有(C)2004,JPO