    • 4. 发明专利
    • JPH05337741A
    • 1993-12-21
    • JP33931292
    • 1992-12-18
    • FUJIKURA LTD
    • TAKAYAMA TERUYUKITOMINAGA HARUOOGURA YOSHIOYAMAGUCHI TETSUO
    • B23H7/08C23C10/24H01B5/02H01B13/00
    • PURPOSE:To provide the manufacture of a electrode wire for wire electrodischarge machining that is high in strength against high temperature, less in the frequency of disconnection even if removal rate is increased and able to enhance the efficiency of electrodischarge machining operations. CONSTITUTION:Zincing is applied to the outer circumferential surface of a copper covered steel wire 11 made up of covering copper on the steel wire at a covering rate of 10-70% and, after a zinc layer is formed there, it is subjected to heat treatment in an inert atmosphere so as to get zinc alloyed with the ground copper to the full as this zinc layer vanishes into nothing, through which it comes to a thickness of 1-15mum, where such a concentration gradient as making zinc density become high toward an outer layer from the copper ground is set thereon, thereby forming a copper- zinc alloyed layer 12 which has an outer layer 13 of 55-65% in zinc density at the outer surface side, an intermediate layer 14 of 40-48% in zinc density at the intermediate part and an inner layer 15 of less than 40% in zinc density at the inner surface side, respectively. With this constitution, a removal rate is increasable and, what is more, such a wire electrodischarge machining electrode wire as excellent even in economical efficiency is thus securable.
    • 9. 发明专利
    • MANUFACTURE OF OXIDE CRYSTALLINE WIRE MATERIAL
    • JPH03246826A
    • 1991-11-05
    • JP4494590
    • 1990-02-26
    • FUJIKURA LTD
    • AOYANAGI MAMORUTOMINAGA HARUOKUROSAKA AKITO
    • H01B12/04H01B13/00
    • PURPOSE:To enable obtaining a high strength sintered body of oxide without any use of a molding assistant such as a caking agent by sealing oxide powder wetted with moisture to the predetermined level in a rubber tube, and freezing the powder after molding under pressure for maintaining the shape of the compact of the oxide powder. CONSTITUTION:Oxide powder wetted up to 3wt.% or more of moisture is sealed in a rubber tube and then molded under pressure. The compact so obtained is immersed and frozen in a solvent at a temperature equal to or below liquid nitrogen temperature, together with the rubber tube. The compact after the separation of the rubber tube is heated up to 800 deg.C or higher for sintering. An oxide sintered body material 1 obtained after the separation of the rubber tube is made to have a diameter of 1.0mm or more. This material 1 is locally heated and the liquid of a fused portion 3 is solidified to obtain a wire material 11 having a diameter of 0.5mm or less. According to the aforesaid construction, the oxide can be sintered without any addition of a molding assistant and the oxide crystalline wire material 11 can be continuously manufactured without any any break at a low cost.