    • Method of forming high performance thread forming screw
    • 形成高性能螺纹成形螺杆的方法
    • JP2012187638A
    • 2012-10-04
    • JP2012115545
    • 2012-05-21
    • Acument Intellectual Properties Llcアキュメント インテレクチュアル プロパティーズ エルエルシー
    • PRICE DAVID RSHATTUCK GARY
    • B21K1/46F16B25/04F16B33/02
    • F16B25/00B21K1/46C21D9/0093F16B25/0021F16B33/06
    • PROBLEM TO BE SOLVED: To provide a method of forming a thread forming screw, which can form threads in a workpiece having a surface hardness which exceeds HRC 23.SOLUTION: The method of forming a thread forming screw includes the steps of: cold upsetting an alloy wire to form a screw head, and then forming a screw thread part; carbon enriching the screw to at least a 0.48 carbon level, and then quenching and tempering the screw, wherein the screw is tempered such that the surface hardness does not exceed the core hardness by more than 3 Rockwell C points, and both the surface and core are at a Rockwell C33-C39 hardness; induction hardening the point; quenching and tempering the screw again, wherein the screw is tempered such that the lead threads and the first 3-4 full threads are at a Rockwell C56 minimum hardness, preferably to a depth of at least 0.008 inches, and the core is at the Rockwell C33-C39 hardness; and finally, applying a finish.
    • 要解决的问题:提供一种形成螺纹形成螺杆的方法,该螺纹形成螺杆可以在具有超过HRC 23的表面硬度的工件中形成螺纹。解决方案:形成螺纹形螺杆的方法包括 步骤:冷镦合金丝以形成螺丝头,然后形成螺纹部分; 碳将螺杆富集至少0.48碳水平,然后淬火和回火螺杆,其中螺杆被回火,使得表面硬度不超过芯部硬度超过3个洛氏C点,并且表面和芯部 处于洛氏C33-C39硬度; 感应淬火点; 再次对螺钉进行淬火和回火,其中螺杆被回火,使得引线和前3-4个全螺纹处于洛氏C56最小硬度,优选至少为0.008英寸的深度,并且芯在洛氏 C33-C39硬度; 最后应用完成。 版权所有(C)2013,JPO&INPIT