会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 43. 发明专利
    • Large furnace opening hole brick in converter and lining structure of furnace opening hole in converter using this
    • 大转炉开关孔在转炉中使用转炉和炉内结构开关孔
    • JP2005336515A
    • 2005-12-08
    • JP2004153874
    • 2004-05-24
    • Kurosaki Harima CorpSumitomo Metal Ind Ltd住友金属工業株式会社黒崎播磨株式会社
    • KUBO YOSHIKAZUYOSHIDA HIROSHITANAKA MASAHITOEGAMI MASAYUKINAGAO KUNITAKASHIROMOTO HIROSHIMASUDA KAZUHIKO
    • C21C5/44
    • Y02P10/212
    • PROBLEM TO BE SOLVED: To provide a furnace opening hole brick and a lining structure using this brick, with which the brick in the furnace opening hole part in a converter is difficult to fall down and the lining work is simple, and the number and time of repairing of the furnace opening hole brick can be reduced. SOLUTION: The lining has large resistance to the oxygen-blowing and the shock of scrap-chute and difficult-to-crack, by which the number of constituting pieces of the bricks in the circumferential direction in the furnace opening hole, that is, the divided number is small and the thickness is large, and the lining work is performed with these bricks. Further, even in the case of developing the crack on the brick, this cracked position is a part of the tip end part, and since the brick is large-type, the brick is not fallen down. In the lining structure 10 from the furnace opening hole part 1 to the constricting part, the uppermost step bricks 2 and the second step bricks 3 from the upper part, are formed as the large-sized bricks. COPYRIGHT: (C)2006,JPO&NCIPI
    • 要解决的问题:为了提供一种使用这种砖的炉开孔砖和衬里结构,转炉中的炉开孔部分中的砖难以落下并且衬里工作简单,并且 可以减少炉孔孔砖的修理次数和时间。 解决方案:该炉衬具有较大的耐吹氧能力和废料溜槽的冲击,并且难以开裂,通过这种方式,炉膛孔中圆周方向的砖构件数量, 是,分割数小,厚度大,衬里工作是用这些砖进行的。 此外,即使在砖上发生裂纹的情况下,该裂纹位置是前端部的一部分,并且由于砖是大型砖,所以砖不会下落。 在从炉开孔部1到收缩部的衬里结构体10中,形成有来自上部的最上层步骤砖2和第二阶梯砖3作为大尺寸砖。 版权所有(C)2006,JPO&NCIPI
    • 44. 发明专利
    • COARSE AGGREGATE CONTINUOUS BLEND TECHNIQUE TO UNSHAPED REFRACTORY
    • JP2001215086A
    • 2001-08-10
    • JP2000025446
    • 2000-02-02
    • SUMITOMO METAL INDINTOCAST JAPAN KK
    • KUBO YOSHIKAZUYASUI SEIICHI
    • B28C5/38F27D1/16
    • PROBLEM TO BE SOLVED: To solve the problem where a coarse aggregate cannot be blended with an unshaped refractory in an industrial scale since a continuous-type kneading mixer for blending the coarse aggregate with the unshaped refractory has not been considered at all. SOLUTION: A continuous-type kneading mixer 3 is equipped with conveyance kneading, dispersion mixing, and ejection parts 7, 8, and 9. At the conveyance kneading part 7, the unshaped refractory is carried while being kneaded for changing into sol. At the dispersion mixing part 8, in the unshaped refractory being changed into the sol, a turning flow generation blade 19 that has an external diameter for forming space where the coarse aggregate can be turned around a rotary shaft 11, and a conveyance kneading member 13 that carries the unshaped refractory being changed into the sol where the coarse aggregate is dispersed for blending are fitted onto the outer- periphery surface of the rotary shaft 11, at the same time, a fall-throwing device 16 of the coarse aggregate is provided, and the coarse aggregate is nearly uniformly dispersed to the unshaped refractory being changed into the sol for mixing. At the ejection part 9, the unshaped refractory being changed into the sol where the coarse aggregate is dispersed for mixing is allowed to fall into a mold for throwing via a slanting surface 9a.