    • Metallic material having excellent metal dusting resistance
    • 金属材料具有优异的金属耐腐蚀性
    • JP2007186727A
    • 2007-07-26
    • JP2006003479
    • 2006-01-11
    • Sumitomo Metal Ind Ltd住友金属工業株式会社
    • NISHIYAMA YOSHITAKAOTSUKA NOBUO
    • C22C38/00C22C38/58
    • PROBLEM TO BE SOLVED: To provide a material having excellent metal dusting resistance which is suitable as the material for a cracking furnace, a reforming furnace or the like in petroleum refining, a petrochemical plant or the like.
      SOLUTION: The metallic material has a composition containing, by mass, 0.01 to 0.4% C, 0.01 to 2.5% Si, 0.01 to 2.5% Mn, 15 to 35% Cr, 20 to 65% Ni, 0.05 to 20% Cu, ≤0.1% S, ≤0.25% N, ≤0.02% O (oxygen) and one or more selected from >0.05 to 0.3% P, 0.001 to 1% Sb and 0.001 to 0.5% Bi, and the balance Fe. The metallic material may comprise one or more selected from ≤10% Co, ≤3% Mo, ≤6% W, ≤1% Ti, ≤2% Nb, ≤0.1% B, ≤1.2% Zr, ≤0.5% Hf, ≤0.1% Mg, ≤0.1% Ca, ≤0.8% Al, ≤0.15% Y, ≤0.15% La and ≤0.15% Ce as well.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供一种适用于石油炼制,石油化工厂等中的裂解炉,重整炉等的材料,具有优异的耐金属粉尘性的材料。 解决方案:金属材料具有以质量计含有0.01至0.4%的C,0.01至2.5%的Si,0.01至2.5%的Mn,15至35%的Cr,20至65%的Ni,0.05至20% Cu,≤0.1%S,≤0.25%N,≤0.02%O(氧)和选自0.05〜0.3%P,0.001〜1%Sb和0.001〜0.5%Bi的一种或多种,​​余量为Fe。 金属材料可以包括选自≤10%Co,≤3%Mo,≤6%W,≤1%Ti,≤2%Nb,≤0.1%B,≤1.2%Zr,≤0.5%Hf中的一种或多种, ≤0.1%Mg,≤0.1%Ca,≤0.8%Al,≤0.15%Y,≤0.15%La和≤0.15%Ce。 版权所有(C)2007,JPO&INPIT
    • 12. 发明专利
    • Austenitic stainless steel
    • 奥氏体不锈钢
    • JP2006291290A
    • 2006-10-26
    • JP2005113402
    • 2005-04-11
    • Sumitomo Metal Ind Ltd住友金属工業株式会社
    • NISHIYAMA YOSHITAKAOTSUKA NOBUO
    • C22C38/00C22C38/58
    • C22C38/42C22C38/001C22C38/005F28F21/083
    • PROBLEM TO BE SOLVED: To provide austenitic stainless steel having scale peeling resistance that, even if it is subjected to a heating-cooling cycle of repeating heating at high temperature and cooling to room temperature, the peeling of protective oxidized scale formed on the steel surface can be suppressed, and suitably usable even in a high temperature humidified gas environment heated to high temperature, particularly, to ≥1,023 K. SOLUTION: The austenitic stainless steel has a composition comprising 0.01 to 0.15% C, 0.01 to 3% Si, 0.01 to 2% Mn, 0.1 to 2.5% Cu, 23 to 30% Cr, 16 to 25% Ni, 0.005 to 0.20% Al, 0.001 to 0.40% N, ≤0.04% P and ≤0.01% S, further comprising one or more kinds selected from Y and Ln group metals by 0.005 to 0.1% in total, and the balance Fe with inevitable impurities, and in which the number of inclusions composed of Y and the La group in the surface of the steel is ≤5×10 -3 pieces/μm 2 . COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:为了提供具有防垢剥离性的奥氏体不锈钢,即使经受在高温下重复加热并冷却至室温的加热 - 冷却循环,也会形成在 钢表面可以被抑制,即使在加热到高温的高温加湿气体环境中也是适用的,特别是≥1,023K。解决方案:奥氏体不锈钢具有0.01至0.15%的C,0.01 至3%Si,0.01〜2%Mn,0.1〜2.5%Cu,23〜30%Cr,16〜25%Ni,0.005〜0.20%Al,0.001〜0.40%N,≤0.04%P,≤0.01%S 进一步包含选自Y和Ln族金属中的一种或多种,​​总计为0.005至0.1%,余量为Fe与不可避免的杂质,其中由钢中的Y和La基组成的夹杂物的数量 ≤5×10 -3 个/μm 2 。 版权所有(C)2007,JPO&INPIT
    • 14. 发明专利
    • Austenitic stainless steel, stainless steel product and method of manufacturing the same
    • 奥氏体不锈钢,不锈钢产品及其制造方法
    • JP2011236465A
    • 2011-11-24
    • JP2010108475
    • 2010-05-10
    • Sumitomo Metal Ind Ltd住友金属工業株式会社
    • ADACHI KAZUHIKOSEKI AKIRANISHIYAMA YOSHITAKAFUJISAWA KAZUYOSHIFUKUMURA YUICHISHIBUYA MASAYUKI
    • C22C38/00C21D9/46C22C38/58
    • PROBLEM TO BE SOLVED: To provide austenitic stainless steel which has oxidation resistance property and high-temperature strength, facilitates manufacturing of raw materials and processing to products by forming and welding, can be used for a large range of fields and exhibits excellent economy.SOLUTION: The austenite stainless steel has a chemical composition including: 0.05-0.20% ofC, less than 1.0% of Si, 2.0% or less of Mn, 0.04% or less of P, 0.01% or less of S, 20.0-30.0% of Cr, 10.0-15.0% of Ni, 0.10-0.42% of N, 0.0010-0.01% of B, 0.01-0.10% of La+Ce, 0.01-0.20% of sol.Al, Fe for balance and impurities. The C concentration at a surface layer in the thickness direction is higher than that at the center in the thickness direction by 0.03% or more, and/or the N concentration at the surface layer in the thickness direction is higher than that at the center in the thickness direction by 0.03% or more.
    • 要解决的问题:为了提供具有耐氧化性和高温强度的奥氏体不锈钢,通过成型和焊接便于原料的制造和加工成产品,可用于大范围的领域并且显示出优异的 经济。 解决方案:奥氏体不锈钢的化学组成包括:0.05-0.20%的C,小于1.0的Si,2.0%以下的Mn,0.04%以下的P,0.01%以下的S,20.0 -30.0%的Cr,10.0-15.0%的Ni,0.10-0.42%的N,0.0010-0.01%的B,0.01-0.10%的La + Ce,0.01-0.20%的sol.Al,Fe的余量和杂质 。 厚度方向的表面层的C浓度比厚度方向中央处的C浓度高0.03%以上,和/或厚度方向的表面层的N浓度高于中心的浓度 厚度方向为0.03%以上。 版权所有(C)2012,JPO&INPIT
    • 17. 发明专利
    • Steel tube with excellent steam oxidation resistance
    • 具有优异的蒸汽氧化电阻的钢管
    • JP2009068079A
    • 2009-04-02
    • JP2007238636
    • 2007-09-14
    • Sumitomo Metal Ind Ltd住友金属工業株式会社
    • NISHIYAMA YOSHITAKAMIYAHARA HITOSHIKAWAKAMI TADASHI
    • C22C38/00C21D7/06C22C38/18C22C38/58
    • PROBLEM TO BE SOLVED: To provide a steel tube having excellent steam oxidation resistance and suitable as a material used for boilers in power generation facilities, tubing and various heat exchangers, etc.
      SOLUTION: The steel tube with excellent steam oxidation resistance contains 8 to 28 mass% Cr and has a worked layer in the inner surface thereof and satisfies inequality α≥0.5 (wherein α is represented by equation α={Hv
      20 -Hv
      t/2 }/Hv
      t/2 ). In the equation, Hv
      20 and Hv
      t/2 denote a Vickers hardness in a position at a depth of 20 μm from the inner surface of the steel tube and a Vickers hardness in a position at a depth of t/2 (where (t) is wall thickness of the steel tube) from the inner surface of the steel tube, respectively.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供具有优异的耐蒸汽抗氧化性的钢管,适合用作发电设备,管道和各种热交换器等中的锅炉的材料。解决方案:具有优异蒸汽的钢管 抗氧化性含有8〜28质量%的Cr,并且在其内表面具有加工层,并且满足不等式α≥0.5(其中α由等式α=äHv Hv 2 / SB)/ Hv t / 2 )。 在该方程式中,Hv 20 和Hv t / 2 表示在距离钢管内表面20μm深度的位置的维氏硬度,维氏硬度 在钢管的内表面分别在t / 2深度(其中(t)是钢管的壁厚)的位置。 版权所有(C)2009,JPO&INPIT
    • 18. 发明专利
    • Metallic material having excellent metal dusting resistance
    • 金属材料具有优异的金属耐腐蚀性
    • JP2008214734A
    • 2008-09-18
    • JP2007058088
    • 2007-03-08
    • Sumitomo Metal Ind Ltd住友金属工業株式会社
    • NISHIYAMA YOSHITAKAOTSUKA NOBUO
    • C22C38/00C22C19/05C22C38/60
    • PROBLEM TO BE SOLVED: To provide a metallic material having excellent metal dusting resistance and, e.g., suitable as the stock for a cracking furnace, a reforming furnace, a heating furnace or a heat exchanger in petroleum refining plant, a petrochemical plant or the like.
      SOLUTION: The metallic material having metal dusting resistance has a composition comprising, by mass, 0.01 to 0.4% C, 0.01 to 1.0% Si, 0.01 to 2.5% Mn, 15 to 35% Cr, 20 to 70% Ni, 0.05 to 20% Cu, ≤0.1% S, >0.8 to 4.0% Al, ≤0.1% N, ≤0.02% O (oxygen), >0.05 to 0.3% P, one or more selected from 0.001 to 1% Sb and 0.001 to 0.5% Bi, and the balance Fe with impurities. The material may comprise one or more selected from ≤10% Co, ≤3% Mo, ≤6% W, ≤2% Ti, ≤2% Nb, ≤0.1% B, ≤1.2% Zr, ≤0.5% Hf, ≤0.1% Mg, ≤0.1% Ca, ≤0.15% Y, ≤0.15% La, ≤0.15% Ce and ≤0.15% Nd as well.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供具有优异的耐金属粉尘性的金属材料,例如适合作为石油炼制厂中的裂解炉,重整炉,加热炉或热交换器的原料,石化厂 或类似物。 解决方案:具有金属防尘性的金属材料具有质量分数为0.01〜0.4%,Si:0.01〜1.0%,Mn:0.01〜2.5%,Cr:15〜35%,Ni:20〜70% 0.05〜20%的Cu,≤0.1%的S,> 0.8〜4.0%的Al,≤0.1%的N,≤0.02%的O(氧),> 0.05〜0.3%的P,选自0.001〜1%的Sb和0.001 至0.5%Bi,余量为Fe与杂质。 该材料可以包括选自≤10%Co,≤3%Mo,≤6%W,≤2%Ti,≤2%Nb,≤0.1%B,≤1.2%Zr,≤0.5%Hf,≤ 0.1%Mg,≤0.1%Ca,≤0.15%Y,≤0.15%La,≤0.15%Ce和≤0.15%Nd。 版权所有(C)2008,JPO&INPIT
    • 19. 发明专利
    • Stainless steel having carburization resistance and calking resistance, and stainless steel pipe thereof
    • 具有耐高温和耐腐蚀性的不锈钢及其不锈钢管
    • JP2005048284A
    • 2005-02-24
    • JP2004182433
    • 2004-06-21
    • Sumitomo Metal Ind Ltd住友金属工業株式会社
    • NISHIYAMA YOSHITAKAYAMADERA YOSHIMI
    • C22C38/00C22C38/18C22C38/58
    • PROBLEM TO BE SOLVED: To provide a stainless steel pipe used as a cracking furnace pipe for an ethylene plant, and to provide a method for improving the carburization resistance and calking resistance of the pipe when used for it.
      SOLUTION: The stainless steel pipe comprises a main body made of a base metal containing, by mass%, 20-35% Cr, and a surface layer part having a Cr-deficient layer. The Cr-deficient layer contains 10% or higher Cr, and has a thickness of 20 μm or thinner. The stainless steel may further have an oxidized scale layer mainly containing 50% or more Cr on the outer side of the Cr-deficient layer. The thickness of an oxidized scale layer is 0.1 to 15 μm. Furthermore, the stainless steel may have the second oxidized scale layer mainly containing 50% or more Si, in between the above oxidized scale layer and the Cr-deficient layer.
      COPYRIGHT: (C)2005,JPO&NCIPI