    • 11. 发明专利
    • Coke-extruding apparatus
    • 咖啡挤出装置
    • JP2008007529A
    • 2008-01-17
    • JP2006176130
    • 2006-06-27
    • Jfe Steel KkJfeスチール株式会社
    • KAMEZAKI SHUNICHIISHINO KAZUNARISHIMAMURA TAKAHIROTAKAHASHI TAMOTSUUCHIDA TETSUOTANAKA HITOSHIKIKUCHI SHINTAROFUKUSHIMA YASUHIRO
    • C10B33/08C10B41/02
    • PROBLEM TO BE SOLVED: To provide a coke-extruding apparatus having an adequate structure, capable of avoiding the collision between a vibration exciter for applying vibration to coke lumps and a ram driving apparatus, etc., for driving a ram as a coke-extruding apparatus capable of extruding coke lumps while applying vibration to coke lumps when extruding the coke lumps from a carbonizing chamber by pressing a ram head of ram top to the coke lumps in the carbonizing chamber of a coke oven.
      SOLUTION: The coke extruding apparatus 11 comprises a vibration exciter 22b for vibrating a vibrating plate provided on a ram head 22 on the outside of a ram 20, and a connecting part 30 capable of carrying out connection and separation between the vibration exciter 28 and the ram 20.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种具有足够结构的焦炭挤出装置,其能够避免用于将振动施加到焦炭块上的振动激励器与冲击器驱动装置等之间的碰撞,以用于驱动冲头作为 焦炭挤出装置,其能够通过将压头顶部的压头压入焦炭炉的碳化室中的焦炭块而从碳化室挤出焦炭块时对焦炭块施加振动,同时挤出焦炭块。 解决方案:焦炭挤出装置11包括用于振动设置在冲头20外部的冲头22上的振动板的振动激励器22b和能够执行振动激励器之间的连接和分离的连接部分30 28和公羊20.版权所有(C)2008年,JPO&INPIT
    • 13. 发明专利
    • Exhaust heat recovering method and exhaust heat recovering device
    • 废热回收方法和排除热回收装置
    • JP2009006395A
    • 2009-01-15
    • JP2007229919
    • 2007-09-05
    • Jfe Steel KkJfeスチール株式会社
    • SHIMAMURA TAKAHIROKUBO NORIKOKAMEZAKI SHUNICHI
    • B22D11/055F28F13/18
    • PROBLEM TO BE SOLVED: To provide a method where, when an object to be cooled such as a high temperature product, a high temperature stock and a high temperature part in equipment is cooled by a heat medium such as cooling water and air, the difference in temperature of the heat medium before and after the cooling is widen without damaging cooling capacity, thus the calorie obtained by the heat medium is made easy to be recovered, and the heat of the object is recovered.
      SOLUTION: In the exhaust heat recovering method, an object 1 to be cooled is cooled by a heat medium 4 flowing through a flow passage 2 provided for the object 1, and the heat of the heat medium after the cooling is utilized. In the exhaust heat recovering device, a porous metal body 3 is arranged in contact with the heat transfer face of the flow passage, the heat medium is passed through the inside of the porous metal body, so as to widen the temperature difference in the heat medium before and after the cooling, and thereafter, the heat of the heat medium is utilized.
      COPYRIGHT: (C)2009,JPO&INPIT
    • 要解决的问题:提供一种方法,其中当诸如高温产品的待冷却物体,设备中的高温部件和高温部件由诸如冷却水和空气的热介质冷却时 冷却之前和之后的热介质的温度差加宽而不损坏冷却能力,因此易于回收热介质获得的热量,并且回收对象的热量。 解决方案:在废热回收方法中,待冷却的物体1被流过设置在物体1上的流路2的热介质4冷却,利用冷却后的热介质的热量。 在废热回收装置中,多孔金属体3配置成与流路的传热面接触,使热介质通过多孔金属体的内部,从而加热热量的温度差 介质在冷却之前和之后,然后利用热介质的热量。 版权所有(C)2009,JPO&INPIT
    • 15. 发明专利
    • Coke extrusion method and coke manufacturing method
    • 咖啡挤出方法和焦化制造方法
    • JP2008007541A
    • 2008-01-17
    • JP2006176340
    • 2006-06-27
    • Jfe Steel KkJfeスチール株式会社
    • FUKUSHIMA YASUHIROKIKUCHI SHINTAROTANAKA HITOSHIUCHIDA TETSUOSHIMOYAMA IZUMIKAMEZAKI SHUNICHIISHINO KAZUNARISHIMAMURA TAKAHIRO
    • C10B33/10C10B41/02
    • PROBLEM TO BE SOLVED: To provide a coke extrusion method that exactly lessens an extrusion load thereby to reduce damages of a coke oven wall when a coke lump is extruded from a carbonization chamber of a coke oven, and a coke manufacturing method.
      SOLUTION: The coke extrusion method comprises monitoring extrusion force during extrusion when the coke lump 11 in the carbonization chamber 10 in the coke oven is extruded from the carbonization chamber using an extrusion apparatus 20 and extruding the coke lump while applying oscillation thereto from the back surface by an oscillator 23 when the extrusion force is at least 40% of the maximum extrusion force. It is preferable that the coke lump is extruded with oscillation applied when the extrusion force is at least 20% of the maximum extrusion force, that the extrusion force is monitored by measuring the load current value of the driving force of the extrusion apparatus, and that application of oscillation is terminated when the extrusion force falls below the predetermined value after application of oscillation.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种当从焦化炉的碳化室挤出焦炭块和焦炭制造方法时,精确地减小挤出负荷从而减少焦炉壁的损坏的焦炭挤出方法。 解决方案:焦炭挤出方法包括当使用挤出装置20从碳化室将焦化炉中的碳化室10中的焦炭块11挤出时挤出焦炭块,同时向其中施加振荡,从而监测挤压期间的挤压力 当挤出力为最大挤压力的至少40%时,通过振荡器23的后表面。 优选的是,当挤出力为最大挤压力的至少20%时,焦炭块被挤压,通过测量挤压装置的驱动力的负载电流值来监测挤出力,并且 在施加振荡之后挤出力降至预定值以下时,停止施加振动。 版权所有(C)2008,JPO&INPIT
    • 16. 发明专利
    • Coke extrusion method and coke manufacturing method
    • 咖啡挤出方法和焦化制造方法
    • JP2008007540A
    • 2008-01-17
    • JP2006176339
    • 2006-06-27
    • Jfe Steel KkJfeスチール株式会社
    • FUKUSHIMA YASUHIROKIKUCHI SHINTAROTANAKA HITOSHIUCHIDA TETSUOSHIMOYAMA IZUMIKAMEZAKI SHUNICHIISHINO KAZUNARISHIMAMURA TAKAHIRO
    • C10B33/08
    • PROBLEM TO BE SOLVED: To provide a coke extrusion method that exactly lessens an extrusion load thereby to reduce damages of a coke oven wall when a coke lump is extruded from a carbonization chamber of a coke oven, and a coke manufacturing method. SOLUTION: The coke extrusion method comprises monitoring extrusion force during extrusion when the coke lump in the carbonization chamber in the coke oven is extruded from the carbonization chamber using an extrusion apparatus and extruding the coke lump while applying oscillation thereto in the case that the extrusion force reaches a predetermined value or gets higher. It is preferable that the predetermined value of the extrusion force is set to 20-50% based on the maximum extrusion force, that the extrusion force is monitored by measuring the load current value of the driving apparatus of the extrusion apparatus, that application of oscillation is terminated when the extrusion force falls below the predetermined value after application of oscillation, that the extrusion apparatus has a ram head to be pushed against the coke lump for extruding the coke lump from the carbonization chamber with the oscillation being applied to the coke lump by oscillating the ram head. COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种当从焦化炉的碳化室挤出焦炭块和焦炭制造方法时,精确地减小挤出负荷从而减少焦炉壁的损坏的焦炭挤出方法。 解决方案:焦炭挤出方法包括当使用挤出装置从焦化炉中的碳化室中挤出焦炭炉中的焦炭块并挤出焦炭块同时在其中进行振荡时,在挤出期间监测挤出力, 挤出力达到预定值或变高。 优选地,基于最大挤压力将挤压力的预定值设定为20-50%,通过测量挤出装置的驱动装置的负载电流值来监测挤出力,施加振荡 当挤压力在施加振动之后下降到预定值以下时,终止挤出装置,挤出装置具有被压靠在焦炭块上的压头,用于从碳化室挤出焦炭块,同时将振荡施加到焦炭块上 振动压头。 版权所有(C)2008,JPO&INPIT
    • 17. 发明专利
    • Coke extruding method and coke producing method
    • 咖啡挤出方法和焦炭生产方法
    • JP2008007538A
    • 2008-01-17
    • JP2006176337
    • 2006-06-27
    • Jfe Steel KkJfeスチール株式会社
    • KIKUCHI SHINTAROFUKUSHIMA YASUHIROTANAKA HITOSHIUCHIDA TETSUOSHIMOYAMA IZUMIKAMEZAKI SHUNICHIISHINO KAZUNARISHIMAMURA TAKAHIRO
    • C10B33/10C10B41/02
    • PROBLEM TO BE SOLVED: To provide a coke extruding method and a coke producing method capable of surely reducing the extruding load in the extrusion of a coke block out of a carbonization chamber of a coke oven and reducing the damage of the coke oven wall.
      SOLUTION: A coke block is extruded from a carbonization chamber of a coke oven with an extruding device while applying vibration to the coke block when the bottom temperature of the combustion chamber adjacent to the carbonization chamber is ≤1000°C. As an alternative, the coke block is extruded under application of vibration when the bottom temperature of the combustion chamber adjacent to the carbonization chamber is ≥1300°C, the bottom temperature difference between two combustion chambers adjacent to the carbonization chamber is ≥100°C, the setting time exceeds 180 min, the water content of coal is ≤6.0 mass% or the content of coal having particle diameter of ≤3 mm is ≤68 mass%.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 待解决的问题:提供一种焦炭挤出方法和焦炭生产方法,其能够可靠地降低焦炭块的挤出中的挤出负荷,并减少焦炉的碳化室 壁。 解决方案:当与碳化室相邻的燃烧室的底部温度≤1000℃时,将焦炭块从具有挤出装置的焦化炉的碳化室挤出,同时向焦炭块施加振动。 作为替代方案,当邻近碳化室的燃烧室的底部温度≥1300℃时,在施加振动的情况下挤压焦炭块,与碳化室相邻的两个燃烧室之间的底部温度差为≥100℃ ,凝固时间超过180分钟,煤的含水量≤6.0质量%,或者粒径≤3毫米的煤的含量≤68质量%。 版权所有(C)2008,JPO&INPIT
    • 19. 发明专利
    • Slag removing device
    • SLAG移除装置
    • JP2007262546A
    • 2007-10-11
    • JP2006092727
    • 2006-03-30
    • Jfe Steel KkJfeスチール株式会社
    • KAMEZAKI SHUNICHIISHINO KAZUNARI
    • C21C5/46C21C1/06C21C7/00
    • PROBLEM TO BE SOLVED: To provide a slag removal device with which in the case of removing the slag floated up on molten metal from a molten metal vessel of a refining furnace or ladle, etc., holding the molten metal, such as molten iron, molten steel, the greater part of slag can be removed several times in operations, with a simple constitution, even in the case of the molten metal vessel having deep depth, such as a converter.
      SOLUTION: In the slag removal device 1, the slag 12 existing on the surface of the molten metal 11 held in the molten metal vessel 8, is scraped out from a slag-exhausting hole 9 with a scraping plate 4 fit to the tip end part of a supporting arm 3 so as to be reciprocatively shiftable in the horizontal direction, wherein the scraping plate is composed of a metal plate which is elastically deformable and even in the case of contacting with the slag-exhausting hole, this metal plate can pass through while being elastically deformed.
      COPYRIGHT: (C)2008,JPO&INPIT
    • 要解决的问题:提供一种除渣装置,其在将熔融金属从熔融金属容器中移出的熔渣中的熔融金属从熔融金属容器中取出的情况下,将熔融金属(例如 铁水,钢水,大部分炉渣可以在操作中多次去除,即使在具有深度的熔融金属容器(如转炉)的情况下,结构简单。 解决方案:在除渣装置1中,存在于熔融金属容器8中的熔融金属11的表面上存在的渣12从排渣孔9被刮出,刮板4适合 支撑臂3的前端部能够在水平方向上往复移动,其中刮板由可弹性变形的金属板构成,即使在与排渣孔接触的情况下,该金属板 可以通过而弹性变形。 版权所有(C)2008,JPO&INPIT
    • 20. 发明专利
    • Recycle system for used automobiles, using network
    • 使用汽车的循环系统,使用网络
    • JP2003303231A
    • 2003-10-24
    • JP2002106752
    • 2002-04-09
    • Jfe Steel KkJfeスチール株式会社
    • KAMEZAKI SHUNICHIWAKIMOTO KAZUMASAMIZUKAMI HIDEAKIIWASAKI KATSUHIRO
    • B09B3/00B09B5/00G06Q30/06G06Q50/00G06Q50/10G06F17/60
    • Y02P90/84
    • PROBLEM TO BE SOLVED: To provide a technique for recycling smoothly used automobiles, scattered all over the country. SOLUTION: This system includes a center server 3 communicable with each other via a network 2, a taker terminal 75, an advanced disassembling enterprise terminal 76, a conventional disassembling enterprise terminal 77, and a shredder enterprise terminal 78, and the center server 73 is provided with a database 81 for storing rewritably information about transaction of the scraped automobile of a taker, information about advanced disassembling of an advanced disassembling enterprise, information about conventional disassembling of a conventional disassembling enterprise, and information as to shredder treatment of a shredder enterprise, and a means for retrieving the taker, the advance disassembling enterprise, the conventional disassembling enterprise, and the shredder enterprise fit to a required condition from the data base 81 to transmits a retrieved result to a request terminal and to transmit required information to the terminals of the taker, the advanced disassembling enterprise, the conventional disassembling enterprise, and the shredder enterprise retrieved therein. COPYRIGHT: (C)2004,JPO
    • 要解决的问题:提供一种分散在全国各地平稳使用的汽车回收技术。 解决方案:该系统包括通过网络2彼此通信的中心服务器3,接收者终端75,高级拆卸企业终端76,传统拆卸企业终端77和粉碎企业终端78,以及中心 服务器73设置有数据库81,用于存储关于接受者的被刮取汽车的交易的可重写信息,关于先进拆卸企业的高级拆卸的信息,关于传统拆卸企业的常规拆卸的信息,以及关于破碎机处理的信息 粉碎机企业,以及从数据库81检索接收者,提前拆解企业,传统拆解企业和符合要求条件的破碎机企业的手段,将检索结果发送到请求终端,并将所需信息发送到 接待员的终端,先进的拆装公司 传统拆解企业,拆包企业等。 版权所有(C)2004,JPO