    • 2. 发明专利
    • High workability steel plate for carburizing
    • 高效的钢板加固
    • JP2010235977A
    • 2010-10-21
    • JP2009082728
    • 2009-03-30
    • Nisshin Steel Co Ltd日新製鋼株式会社
    • TAKEDA KIMIYOSHITAGASHIRA SATOSHIKATAGIRI YUKIOSUZAKI TSUNETOSHI
    • C22C38/00C21D1/06C21D9/32C21D9/40C21D9/46C22C38/38C22C38/58
    • PROBLEM TO BE SOLVED: To provide a steel plate having excellent workability and carburization hardening property, even in the steel plate having 3-15 mm plate thickness to be used for a gear, the outer ring of a bearing, a pulley, and the like. SOLUTION: A high workability steel plate for carburizing, has a component composition composed of, by mass%, 0.10-0.40% C, 0.02-0.40% Si, 1.00-2.00% Mn, ≤0.02% P, ≤0.02% S, 0.20-0.70% Cr, 0.0003-0.005% B, 0.03-0.20% Ti and further, when necessary, one or two kinds of 0.20-2.00% Ni and 0.10-0.80% Mo and the balance Fe with inevitable impurities. The steel plate has a structure such that a structural phase occupying ≥1% area ratio is only ferrite phase and cementite phase, and the number of the particles having ≥0.2 μm in the cementite phase is ≤1,500 pieces/10,000 μm 2 , and in addition to it, Ti carbide particles having 20-100 nm particle diameter are dispersed in the range of 4,000-20,000 pieces/10,000 μm 2 , and the steel plate shows hardness of COPYRIGHT: (C)2011,JPO&INPIT
    • 要解决的问题为了提供一种具有优异的可加工性和渗碳硬化性能的钢板,即使在用于齿轮的板厚度为3-15mm的钢板中,轴承的外圈,滑轮, 等等。 解决方案:用于渗碳的高可加工性钢板,具有以质量%计含有0.10-0.40%C,0.02-0.40%Si,1.00-2.00%Mn,≤0.02%P,≤0.02%的组分组成的组分组合物, S,0.20-0.70%Cr,0.0003-0.005%B,0.03-0.20%Ti,此外,如果需要,可以使用一种或两种0.20-2.00%的Ni和0.10-0.80%的Mo,余量为Fe和不可避免的杂质。 钢板具有这样的结构,使得占据面积比为1%的结构相仅为铁素体相和渗碳相,渗碳体相中≥0.2μm的粒子数为≤1,500个/10,000μm 2 除此之外,具有20-100nm粒径的Ti碳化物颗粒分散在4,000-20,000片/10,000μm 2 的范围内,并且钢板显示硬度 <180 HV。 版权所有(C)2011,JPO&INPIT
    • 3. 发明专利
    • Middle and high carbon steel sheet with high-strength superior in stampability
    • 具有高强度中高耐磨性的中高碳钢板
    • JP2006291236A
    • 2006-10-26
    • JP2005108955
    • 2005-04-05
    • Nisshin Steel Co Ltd日新製鋼株式会社
    • KATAGIRI YUKIOSUZUKI MASAHITOINOUE MAKOTOHIRAMATSU TERUSHI
    • C22C38/00C22C38/06C22C38/50
    • PROBLEM TO BE SOLVED: To provide a middle and high carbon steel sheet with high-strength which has high strength and superior stampability and is suitable for parts for various machine structures.
      SOLUTION: The middle and high carbon steel sheet with high-strength has a metallurgical structure in which carbides with an average particle diameter of 0.30 μm or smaller are dispersed in a matrix consisting of ferritic crystal grains with an average grain size of 2.0 μm or smaller; contains C in an amount of 0.30 to 1.00 mass%; and is thermally refined into the hardness of 250 HV. Specifically, the steel sheet has a composition comprising 2.0 mass% Si or less, 1.0 mass% Mn or less, 0.03 mass% P or less, 0.02 mass% S or less, 0.1 mass% acid-soluble Al or less in addition to 0.30-1.00 mass% C, and the balance substantially Fe; and may also further include one or more elements of 2.0 mass% Cr or less, 0.5 mass% Mo or less, 0.3 mass% Cu or less, 2.0 mass% Ni or less and 0.10 mass% Ti or less.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供具有高强度和优异的冲压性的高强度的中高碳钢板,适用于各种机械结构的部件。 解决方案:具有高强度的中高碳钢板和高碳钢板具有冶金结构,其中平均粒径为0.30μm或更小的碳化物分散在由平均粒径为2.0的铁素体晶粒组成的基体中 μm以下; 含有0.30〜1.00质量%的C; 并被热精炼成250HV的硬度。 具体地说,钢板的组成包括2.0质量%以下,1.0质量%以下,0.03质量%以下,0.02质量%以下,0.1质量%以下的酸溶性Al以下,0.30以下 -1.00质量%C,余量基本为Fe; 还可以包含2.0质量%以下Cr,0.5质量%以下,0.3质量%以下Cu,2.0质量%以下,0.10质量%Ti以下的1种以上的元素。 版权所有(C)2007,JPO&INPIT
    • 7. 发明专利
    • Steel sheet for rotor core of high-speed ipm motor, method of manufacturing the same, rotor core of ipm motor, and ipm motor
    • 高速IPM电机转子芯钢,其制造方法,IPM电机转子芯和IPM电机
    • JP2013076161A
    • 2013-04-25
    • JP2012147416
    • 2012-06-29
    • Nisshin Steel Co Ltd日新製鋼株式会社
    • IWAZU TOMONAGAKATAGIRI YUKIOFUJIWARA SUSUMU
    • C22C38/00C21D8/12C22C38/06C22C38/58H01F1/16H01F1/18
    • PROBLEM TO BE SOLVED: To provide a steel sheet for a rotor core which, when the steel sheet is used as a rotor core of an IPM motor, does not cause lowering of a reluctance torque of the IPM motor, and has high yield strength and high proportional limit capable of coping with high-speed rotation.SOLUTION: The steel sheet for a rotor core of a high-speed IPM motor having a yield strength of 780 N/mmor more, a proportional limit of 600 N/mmor more, and a magnetic flux density Bof 1.65 T or more, is obtained by: cold-rolling a hot-rolled steel sheet having a component composition including >0.03-0.90 mass% of C, 0-3.0 mass% of Si, 0.05-2.5 mass% of Mn, ≤0.05 mass% of P, ≤0.02 mass% of S, 0.005-0.20 mass% of acid soluble Al, 0.001-0.020 mass% of N, and the balance Fe with inevitable impurities, to adjust the final rolling rate to 10% or more; and then heating the resultant cold-rolled sheet at a temperature range of from 200 to 500°C.
    • 要解决的问题:提供一种用于转子铁心的钢板,当钢板用作IPM电动机的转子铁芯时,不会导致IPM电动机的磁阻转矩降低,并且具有高的 屈服强度和高比例极限能够应对高速旋转。 解决方案:屈服强度为780N / mm 2 的高速IPM电机的转子铁心用钢板,比例限制为600N / mm 2 以上,磁通密度B 8000 为1.65T以上,通过以下方式获得:冷轧 组成成分为:C:0.03〜0.90质量%,Si:0.3〜3.0质量%,Mn:0.05〜2.5质量%,P:0.05质量%,P:0.02质量%以下的成分组成的热轧钢板, 0.005-0.20质量%的酸溶性Al,0.001-0.020质量%的N,余量为Fe与不可避免的杂质,将最终轧制速率调整到10%以上; 然后在200〜500℃的温度范围内加热得到的冷轧板。 版权所有(C)2013,JPO&INPIT
    • 9. 发明专利
    • High carbon steel sheet having excellent machinability
    • 高碳钢板具有优异的机械性能
    • JP2006283175A
    • 2006-10-19
    • JP2005108223
    • 2005-04-05
    • Nisshin Steel Co Ltd日新製鋼株式会社
    • KATAGIRI YUKIOSUZUKI MASAHITOHIRAMATSU TERUSHI
    • C22C38/00C22C38/06C22C38/58
    • PROBLEM TO BE SOLVED: To provide a high-carbon steel sheet which is machined to product shapes of machine parts and parts for automobiles, etc., by improving machinability without depending on deposition of graphite and addition of free-cutting elements.
      SOLUTION: The high-carbon steel sheet contains 0.6 to 1.5mass% C, ≤1.0mass% Si, 0.1 to 2.0mass% Mn, ≤0.02mass% S, ≤0.03mass% P, and 0.005 to 0.20mass% Al, has an area rate of 40 to 80% and lamella spacing of ≥0.4 μm and is made into a mixed structure of pearlite, ferrite+spherical or bar-shaped cementite. If necessary, one or two or more of ≤2.5mass% Ni,≤2.0 mass% Cr, ≤1.0mass% Mo and/or one or two or more of ≤0.07mass% Ti, ≤0.07mass% Nb, ≤0.4mass% V. and ≤0.07mass% B may be incorporated therein.
      COPYRIGHT: (C)2007,JPO&INPIT
    • 要解决的问题:提供一种通过提高机械加工性而不依赖于石墨沉积并添加自由切削元件而加工成机械零件和汽车零件形状的高碳钢板。