    • The present invention discloses a fiber treatment agent containing an ester compound represented by the formula (1):

              R 1 -O-((EO) l -(PO) m )-(EO) n -CO-R 2      (1)

      wherein, R 1 represents a hydrocarbon group containing 8 to 24 carbon atoms; R 2 represents an alkyl, alkenyl or cycloalkyl group having 7 to 23 carbon atoms; EO represents an ethyleneoxy group; PO represents a propyleneoxy group; l and n each represent an average reacted mole number of ethyleneoxy groups, 1 ranging from 0 to 15 and n ranging from 1 to 20; m represents an average reacted mole number of propyleneoxy groups, ranging from 0.5 to 20; and ((EO) l -(PO) m ) and (EO) n are arranged in block in this order, while (EO) l and (PO) m in ((EO) l -(PO) m ) may be arranged at random or in block.
    • 本发明公开了含有式(1)表示的酯化合物的纤维处理剂:ƒ€ƒ€ƒ€ƒ€ƒR1 -O - ((EO)l - (PO)m ) - (EO)n -CO-R 2€ƒ€ƒ€ƒ(1)其中,R 1表示含有8至24个碳原子的烃基; R 2表示碳原子数为7〜23的烷基,链烯基或环烷基; EO表示乙烯氧基; PO表示丙烯氧基; 1和n各自表示乙烯氧基的平均反应摩尔数,1为0至15,n为1至20的范围; m表示丙烯氧基的平均反应摩尔数,范围为0.5至20; 和((EO)1-(PO)m)和(EO)n以这种顺序排列,而((EO)1-(PO)m)中的(EO)1和(PO) 随机或封闭。
    • 8. 发明公开
    • Manufacturing method for polyester yarn
    • Verfahren zur Herstellung von Polyestergarnen
    • EP1514959A1
    • 2005-03-16
    • EP03019582.0
    • 2003-09-03
    • NAN YA PLASTICS CORPORATION
    • Jen, Zo-Chun
    • D01F6/62D01D5/088D01D5/16D06M15/53D06M13/165D02J13/00D02J1/22D02G1/00D02J3/00D01G3/00
    • D01F6/62Y10T428/2913Y10T428/2929Y10T428/2969
    • Provide a manufacturing method for polyester yarn excellent in yarn transferring, packaging and loosing with no white powder occurred when weaving, which is heating polyester polymer of inherent viscosity (IV) 0.5∼0.7 and melting point of 245∼265°C to melt, filter and extruding in constant amount by direct spin drawing of monofilament yarn or combining multi-tow of filaments, then splitting to obtain polyester yarn having high denier in monofilament, characterized in comprising the following steps :

      a. uniformly spinning said constant amount extruded polyester melt through spinneret orifices to obtain the filament tows, passing said spun fiiament tows under spinneret to uniformly cooled to solidify in the quenching air tube, wherein said quenching air tube is equipped with chilling water tubular coil to keep the temperature of quenching air at 10∼15°C;
      b. oiling said cooled filament tows, then texturing by the godet roller of direct spin drawing machine, wherein the surface of said godet roller are treated by chrome plating to make the surface roughness of first heating roller in Ra0.025 to 0.1 µm and the surface roughness of second heating roller in Ra0.1 to 0.5 µm ;
      c. drawing said filament tows between said first heating roller and second heating roller with drawing ratio of 3.5∼5 times on the basis of the initial length of said filament tows, the temperature of said first heating roller was set at 85∼105°C, while the temperature of said second heating roller was set at 130∼160°C ;
      d. obtaining spin drawing yarn (SDY) of d.p.f. 5d∼55d by using said conditions, EO/PO ( ethylene oxide / propylene oxide) content of spinning finish in oiling is set at 50%∼90%.

      Polyester yarn of d.p.f. 5d∼55d excellent in yarn transferring, packaging and loosing with no white powder occurred when weaving manufactured by this invention has higher modulus itself, can avoid streak and speckle in weaving, which is suitable in elastic supporter of shoe material, printing mesh, bridal dress etc.
    • 提供纺织时不会发生白色粉末的纱线转移,包装和松动性优异的聚酯纱线的制造方法,其是特性粘度(IV)为0.5〜0.7,熔点为245〜265℃的加热聚酯聚合物熔融,过滤 并通过单纱的直接纺丝或单丝的多丝纤维直接挤出,然后分离得到单丝的高旦数的聚酯纱,其特征在于包括以下步骤:a。 通过喷丝孔将所述恒定量的挤出聚酯熔体均匀地纺丝以获得丝束,将所述纺丝丝束在喷丝头下方通过淬火空气管均匀冷却固化,其中所述淬火空气管装备有冷却水管状线圈,以保持 淬火空气温度为10℃15℃; 湾 将所述冷却的丝束牵引,然后通过直接旋转拉伸机的导丝辊进行加捻,其中所述导丝辊的表面通过镀铬处理以使第一加热辊的表面粗糙度在Ra0.025至0.1μm,表面 第二加热辊的粗糙度在Ra0.1〜0.5μm; C。 在所述第一加热辊和第二加热辊之间,以所述丝束的初始长度为基准,拉伸比为3.5〜5倍的拉丝倍数,将所述第一加热辊的温度设定在85℃〜105℃,同时 所述第二加热辊的温度设定在130〜160℃; 天。 得到d.p.f的纺丝纱线(SDY) 通过使用上述条件,5d类似55d,上油中的纺丝整理剂的EO / PO(环氧乙烷/环氧丙烷)含量为50%,相当于90%。 聚酯纱线d.p.f. 5d类型55d优良的纱线转移,包装和松脱,无白色粉末发生,本发明制造的编织本身具有较高的模量,可以避免织造上的条纹和斑点,适用于鞋材,印花网,新娘礼服的弹性支撑