    • 4. 发明公开
    • POLYPHENYLENE SULFIDE RESIN COMPOSITION AND METHOD FOR MANUFACTURING SAME
    • EP3330309A1
    • 2018-06-06
    • EP16832803.7
    • 2016-07-22
    • Toray Industries, Inc.
    • TAKAO, HidenobuKAIHO, ShuHORIUCHI, Shunsuke
    • C08G75/0209C08L81/02
    • C08G75/0209C08K3/08C08K2003/0818C08L81/02
    • A polyphenylene sulfide resin composition including a polyphenylene sulfide resin (a) of 90 to 50% by weight and a polyphenylene sulfide resin (b) and/or a polyphenylene sulfide resin (c) of the total of 10 to 50% by weight blended with the polyphenylene sulfide resin (a), relative to the total of the polyphenylene sulfide resins (a) to (c) as 100% by weight, in which the polyphenylene sulfide resin composition has a change rate of viscosity of 1.5 times or less when the composition is heated at 320°C for 5 hours. Polyphenylene sulfide resin (a): a polyphenylene sulfide resin having a weight average molecular weight of 50,000 or more and having a weight reduction ratio ΔWr of 0.18% or less when the resin is heated, in which the ratio is represented by the below-mentioned Equation (1); Polyphenylene sulfide resin (b): a polyphenylene sulfide resin having a weight average molecular weight of less than 50,000 and an alkaline earth metal content of less than 200 ppm, and having an increase rate of molecular weight of 5.0% or less when the resin is heated at 320°C for 10 minutes together with 0.5% by weight 2-(3,4-epoxycyclohexyl)ethyltrimethoxysilane added thereto; Polyphenylene sulfide resin (c): a polyphenylene sulfide resin containing 200 to 800 ppm of an alkaline earth metal (d) and having a weight reduction ratio ΔWr of more than 0.18% when the resin is heated, in which the ratio is represented by the below-mentioned Equation (1): ΔWr = (W1 - W2) / W1 × 100(%) --- (1) (wherein ΔWr is a weight reduction ratio (%), which is a value determined from a sample weight (W1) at 100°C reached and a sample weight (W2) at 330°C reached in thermogravimetric analysis carried out under a non-oxidizing atmosphere at normal pressure at a temperature raising rate of 20°C/minute); A PPS resin composition that has a smaller viscosity change during melt residence and generates a smaller amount of gas when heated is provided.