    • In a step of pressing a laminate 80, the laminate 80 is first pressed while being heated to a temperature lower than a melting point of a thermoplastic resin so as to elastically deform the thermoplastic resin and apply a pressure in a direction perpendicular to a laminating direction to thereby allow first and second conductive pastes 41 and 51 to tightly adhere to front and rear surface patterns 21 and 31. Next, the laminate 80 is pressed while being heated to a temperature equal to or higher than the melting point of the thermoplastic resin so as to fluidize the thermoplastic resin while allowing the thermoplastic resin to flow out from the laminate and apply a pressure in the direction perpendicular to the laminating direction to thereby allow the first and second conductive pastes 41 and 51 are solid-sintered. Since the first and second conductive pastes 41 and 51 are tightly adhered to the front and rear surface patterns 21 and 31, the first and second conductive pastes 41 and 51 less easily fluidize when the laminate 80 is pressed at the temperature equal to or higher than the melting point.
    • 在对叠层体80进行冲压的工序中,首先,一边加热至比热塑性树脂的熔点低的温度,一边对叠层体80进行冲压加工,使热塑性树脂弹性变形,向与层叠方向正交的方向 从而使第一导电膏41和第二导电膏51紧密地粘附到正面和背面图案21和31.接下来,在加热到等于或高于热塑性树脂的熔点的温度的同时对层压体80进行压制 使热塑性树脂流体化,同时使热塑性树脂从层压体中流出,并在垂直于层压方向的方向上施加压力,从而使第一和第二导电膏41和51固体烧结。 由于第一导电膏41和第二导电膏51紧密地粘附到前表面图案21和31,所以当层压材料80在等于或大于等于100℃的温度下被挤压时,第一导电膏41和第二导电膏51不易流动 熔点。