    • 3. 发明公开
    • SPUNBONDED NONWOVEN FABRIC AND PRODUCTION METHOD THEREFOR
    • EP3508639A1
    • 2019-07-10
    • EP17846327.9
    • 2017-08-25
    • Toray Industries, Inc.
    • SHIMADA, DaikiIKEJIRI, YukiNAKANO, Yohei
    • D04H3/147B01D63/00D04H3/011
    • The present invention provides a spunbonded nonwoven fabric which has a smooth surface, is highly unlikely to cause a widthwise curl due to a difference between the states of front and back surfaces, has a superior membrane formability of not allowing, at the time of casting of a resin solution, a bleed-through of the resin solution due to excessive permeation, a peel-off of a membrane substance, or any other defect such as nonuniform membrane or pin hole due to fluffing of the support, and further exhibits membrane bondability that is strong enough to prevent the membrane substance from peeling off after membrane formation.
      The spunbonded nonwoven fabric of the present invention is a spunbonded nonwoven fabric composed of thermoplastic fibers. In this spunbonded nonwoven fabric, the thermoplastic fiber is a conjugate fiber in which a low-melting polymer having a melting point lower by 10 to 140°C than that of a high-melting polymer is provided around the high-melting polymer, an apparent single fiber fineness of the conjugate fiber as viewed from the surface of the spunbonded nonwoven fabric is 0.5 dtex or more and 10 dtex or less. When the apparent single fiber fineness of the conjugate fiber is 0.5 dtex or more and less than 2 dtex, an apparent density is 0.50 to 0.70 g/cm 3 , and air permeability satisfies the following [formula 1]. When the apparent single fiber fineness of the conjugate fiber is 2 dtex or more and 10 dtex or less, the apparent density is 0.50 to 0.80 g/cm 3 , and the air permeability satisfies the following [formula 2].
      . 3.8 × 10 4 × basis weight g / m 2 − 2 ≤ air permeability cc / cm 2 ⋅ sec ≤ 6.0 × 10 4 × basis weight g / m 2 − 2
      . 2.2 × 10 4 × basis weight g / m 2 − 2 ≤ air permeability cc / cm 2 ⋅ sec ≤ 4.6 × 10 4 × basis weight g / m 2 − 2
    • 5. 发明公开
    • SPUNBONDED NONWOVEN FABRIC AND PRODUCTION METHOD THEREFOR
    • EP3508640A1
    • 2019-07-10
    • EP17846329.5
    • 2017-08-25
    • Toray Industries, Inc.
    • SHIMADA, DaikiIKEJIRI, YukiNAKANO, Yohei
    • D04H3/147B01D69/10D04H3/011
    • The present invention provides a spunbonded nonwoven fabric, which has a superior membrane formability of not allowing, at the time of casting of a resin solution, a bleed-through of the resin solution due to excessive permeation, a peel-off of a membrane substance, or any other defect such as nonuniform membrane or pin hole due to fluffing of the support, and further exhibits membrane bondability that is strong enough to prevent the membrane substance from peeling off after membrane formation, and a production method for the spunbonded nonwoven fabric. The spunbonded nonwoven fabric of the present invention is a spunbonded nonwoven fabric composed of thermoplastic fibers. In this spunbonded nonwoven fabric, the thermoplastic fiber is a conjugate fiber in which a low-melting polymer having a melting point lower by 10 to 140°C than that of a high-melting polymer is provided around the high-melting polymer, the spunbonded nonwoven fabric has a non-pressure bonding portion having an apparent density of 0.20 to 0.60 g/cm 3 , when a length of a long axis of a fiber cross section of the non-pressure bonding portion is a and a length of a short axis thereof is b, a fiber flatness a/b is 1.5 to 5, and an air permeability satisfies the following [formula 1]. air permeability cc / cm 2 • sec ≤ 520 × exp − 0.0236 × basis weight g / m 2 − 2.85 × apparent density g / cm 3
    • 6. 发明公开
    • MELT-BLOWN NONWOVEN FABRIC AND METHOD FOR MANUFACTURING SAME
    • 熔喷非织造织物及其制造方法
    • EP3187637A1
    • 2017-07-05
    • EP15836602.1
    • 2015-08-21
    • Toray Industries, Inc.
    • SHIMADA, DaikiNAKANO, YouheiYAKAKE, YoshikazuKOBAYASHI, Takuji
    • D04H3/14H01M2/16
    • D04H3/14H01M2/145H01M2/16H01M2/162
    • The present invention provides a melt-blown nonwoven fabric which exhibits good texture with no waviness or surface unevenness as well as high thermal size stability without undergoing drastic decrease in the gas flow rate in heat treatment.
      The melt-blown nonwoven fabric of the present invention comprises a fiber containing a thermoplastic resin as its main component, wherein apparent density is 0.1 to 0.4 g/cm 3 , KES surface roughness of at least one surface of the fabric sheet is up to 1.2 µm, and dry heat shrinkage at a temperature of 200°C is up to 2%.
      The method for producing a melt-blown nonwoven fabric of the present invention comprises the step of conveying a web of nonwoven fabric comprising a fiber containing a thermoplastic resin as its main component by sandwiching the web between 2 sets of belt conveyers each comprising a belt of flexible material having a smooth surface; wherein a heat treatment zone where surface of one or both of the two sets of the belt conveyers has been heated to a temperature not lower than cold crystallization temperature of the thermoplastic resin and not higher than the temperature -3°C lower than melting temperature of the thermoplastic resin is provided in at least a part of the course where the nonwoven fabric is conveyed between the belts; and wherein the nonwoven fabric web is heated in the heat treatment zone by bringing both surfaces of the nonwoven fabric web in contact with the belt conveyers.
    • 本发明提供了一种熔喷非织造织物,其具有良好的织构,没有波纹或表面不平坦,并且热尺寸稳定性高,而热处理中的气体流速没有急剧下降。 本发明的熔喷非织造织物包含含有热塑性树脂作为其主要组分的纤维,其中表观密度为0.1-0.4g / cm 3,织物片至少一个表面的KES表面粗糙度为1.2μm ,在200℃的温度下的干热收缩率高达2%。 本发明的熔喷非织造布的制造方法包括以下步骤:通过将纤维网夹在两组皮带输送机之间来输送由包含热塑性树脂作为其主要成分的纤维构成的非织造纤维网,每组皮带输送机包括 具有光滑表面的柔性材料; 其中,所述两组带式输送机中的一组或两组的表面已经被加热到不低于所述热塑性树脂的冷结晶温度并且不高于比所述热塑性树脂的熔融温度低-3℃的温度 在传送带之间传送无纺布的过程的至少一部分中设置热塑性树脂; 并且其中通过使所述非织造织物网的两个表面与所述带式输送器接触而在所述热处理区中加热所述非织造织物网。