会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明公开
    • SOLAR CELL BACK SURFACE SEALING SHEET
    • SOLARZELLEN-RÜCKOBERFLÄCHEN-VERSIEGELUNGSBLATT
    • EP2040306A1
    • 2009-03-25
    • EP07767327.5
    • 2007-06-21
    • Toppan Printing Co., Ltd.Toyo Ink Mfg. Co., Ltd
    • SUZUTA, MasayoshiYOSHINAGA, MasanobuSHIMENO, IkunoTSUJII, AtsushiYASUI, BungoMAEDA, Seiji
    • H01L31/04B32B9/00B32B15/095B32B27/36B32B27/40C09J175/06C09J175/14
    • B32B27/06B32B7/12C08G18/44C08G18/6229C08G18/725C09J175/04H01L31/049Y02E10/50Y10T428/31515Y10T428/31551
    • The present invention provides a sheet for sealing a rear surface of a solar cell in which degradation due to hydrolysis of the material constituting the solar cell is prevented, and the weather resistance is excellent such that electric output properties of the solar cell can be maintained not only under conditions of actual usage of the solar cell module but also conditions for evaluation under high temperatures and high moistures, and provides a sheet for sealing a rear surface of a solar cell comprising a laminate in which at least two substrates are laminated by an polyurethane-based adhesive, wherein the polyurethane-based adhesive comprises an adhesive having hydrolysis resistance which satisfies the following conditions:
      condition 1: the lamination strength of the adhesive is 1 N/15 mm or more after keeping the laminate in a chamber which acts as a highly accelerated stress test system under pressurized steam conditions of 105°C and 1.05 atm for 168 hours; and condition 2: the adhesive does not bring on a delamination and a blister between the substrates after keeping the laminate in a chamber which acts as a highly accelerated stress test system under pressurized steam conditions of 105°C and 1.05 atm for 168 hours.
    • 本发明提供了一种用于密封太阳能电池的后表面的片材,其中防止了构成太阳能电池的材料的水解导致的劣化,并且耐候性优异,使得太阳能电池的电输出特性可以不被维持 仅在实际使用太阳能电池模块的条件下,而且在高温高湿条件下进行评估的条件,并且提供一种用于密封太阳能电池的后表面的片材,其包括层压体,其中至少两个基底由聚氨酯 的粘合剂,其中所述聚氨酯类粘合剂包含具有耐水解性的粘合剂,其满足以下条件:条件1:将层压体保持在作为其的室中后,粘合剂的层压强度为1N / 15mm以上 在105℃和1.05atm的加压蒸汽条件下高度加速的应力测试系统168小时; 条件2:在105℃和1.05atm的加压蒸汽条件下将层压体保持在作为高加速应力测试系统的室中168小时之后,粘合剂不会在基板之间引起分层和起泡。