会员体验
专利管家(专利管理)
工作空间(专利管理)
风险监控(情报监控)
数据分析(专利分析)
侵权分析(诉讼无效)
联系我们
交流群
官方交流:
QQ群: 891211   
微信请扫码    >>>
现在联系顾问~
热词
    • 1. 发明公开
    • PRODUCTION METHOD FOR HEMATITE FOR IRON PRODUCTION
    • HERSTELLUNGSVERFAHRENFÜRHÄMATIT祖尔EISENERZEUGUNG
    • EP3048083A1
    • 2016-07-27
    • EP14845100.8
    • 2014-09-04
    • Sumitomo Metal Mining Co., Ltd.
    • SASAKI HidekiKAN YasumasaMITSUI Hiroyuki
    • C01G49/06C22B1/02C22B3/04C22B3/44C22B23/00
    • C01G49/06C01P2006/80C22B23/043C22B23/0461Y02P10/212
    • Provided is a production method for refining iron oxide (hematite) having such a low sulfur content as to be used as a raw material for ironmaking from a leach residue containing iron oxide, the leach residue being produced by a high pressure acid leach (HPAL) process.
      The method is to produce (high-purity) hematite for ironmaking by a process of adding an oxidant and sulfuric acid to nickel oxide ore and then leaching nickel, the method further including: forming a neutralized residue having a sulfur grade exceeding 1.0% by weight by adding a neutralizing agent to leach slurry and being subjected to solid-liquid separation, the neutralizing agent serving to form plaster by reaction with a free sulfuric acid of surplus acid contained in the leach slurry, the leach slurry being a mixture of a leachate and a leach residue obtained after leaching the nickel; and heating the neutralized residue at a heating temperature of 600°C or more and 1400°C or less to form hematite having a sulfur grade of 1.0% or less by weight.
      Provided is a method of producing (high-purity) hematite for ironmaking by a process of adding an oxidant and sulfuric acid to nickel oxide ore and then leaching nickel, the method further including: forming a neutralized residue having a sulfur grade exceeding 1.0% by weight by adding a neutralizing agent to leach slurry and being subjected to solid-liquid separation, the neutralizing agent serving to form plaster by reaction with a free sulfuric acid of surplus acid contained in the leach slurry, the leach slurry being a mixture of a leachate and a leach residue obtained after leaching the nickel; and heating the neutralized residue at a heating temperature of 600°C or more and 1400°C or less to form hematite having a sulfur grade of 1.0% or less by weight.
      (128 words)
    • 本发明提供了一种用于从含有氧化铁的浸出残渣中用作具有低硫含量的氧化铁(赤铁矿)作为炼铁原料的生产方法,该浸出残渣由高压酸浸(HPAL) 处理。 该方法是通过向氧化镍矿中加入氧化剂和硫酸然后浸出镍的方法生产(高纯度)赤铁矿,该方法还包括:形成硫含量超过1.0%的中和残渣 通过添加中和剂浸出浆料并进行固液分离,中和剂通过与浸出浆料中所含的剩余酸的游离硫酸反应形成石膏,浸出浆料是渗滤液和 浸出镍后获得的浸出渣; 并在600℃以上且1400℃以下的加热温度下加热中和的残渣,形成硫等级为1.0%以下的赤铁矿。 本发明提供一种通过向氧化镍矿石中加入氧化剂和硫酸然后浸出镍的方法制造(高纯度)的炼铁赤铁矿的方法,该方法还包括:通过以下步骤形成硫等级超过1.0%的中和残渣: 通过添加中和剂以浸出浆料并进行固液分离,中和剂通过与浸出浆料中所含的剩余酸的游离硫酸反应形成石膏,浸出浆料是浸出液的混合物 浸出镍后得到的浸出渣; 并在600℃以上且1400℃以下的加热温度下加热中和的残渣,形成硫等级为1.0%以下的赤铁矿。 (128字)