    • 1. 发明公开
    • METHOD FOR PREPARING BIODEGRADABLE ALIPHATIC-AROMATIC POLYESTER COPOLYMER RESIN WITH IMPROVED HYDROLYSIS RESISTANCE
    • METHOD FOR PRODUCING具有改善的抗水解性的生物降解性脂肪族 - 芳香族聚酯共聚物树脂
    • EP2886579A1
    • 2015-06-24
    • EP13829195.0
    • 2013-05-10
    • Samsung Fine Chemicals Co., Ltd.
    • CHUN, Jong PilKIM, Hee SooKIM, Ye JinCHOI, Soo YounYUN, Ki ChullKIM, Min KyoungYEOM, Nam YeongKANG, Sang Mi
    • C08G63/78C08G63/12C08L67/02
    • C08G63/46C08G63/181C08G63/20C08G63/78
    • There is provided a method of preparation for a biodegradable co-polyester resin with improved hydrolysis resistance, the method including performing a primary esterification reaction between an aliphatic dihydroxy compound and an aliphatic dicarboxylic acid compound, and performing a secondary transesterification reaction with addition of an aromatic dicarboxylate after the primary esterification reaction, in which a short chain alcohol-type branching agent is added to the primary esterification reaction or to the secondary transesterification reaction. In the method of the present invention, the slow esterification reaction caused by acid is performed first and the aromatic dicarboxylate compound without acidity is added thereto, thereby efficiently controlling a non-reactant or a partial-reactant affecting an acid value of a product during the reaction, so that an acid value can be controlled and hydrolysis resistance can be improved without using an excessive amount of expensive BDO, an reaction of an excessive amount of a chain extender, or using an expensive anti-hydrolysis agent. Further, by minimizing an amount of the branching agent used herein, tear strength can be improved.
    • 本发明提供制备的方法中具有改善的抗水解性的生物可降解共聚酯树脂,该方法包括在脂肪族二羟基化合物和脂肪族二羧酸化合物进行之间的初级酯化反应,并用另外的芳族的执行辅助酯交换反应 初级酯化反应,其中短链醇型支化剂添加到主酯化反应或酯交换反应到二次后二羧酸酯。 在本发明的方法中,由酸引发的慢酯化反应中进行第一和无酸性的芳族二羧酸化合物加入其中,从而有效地控制非反应物或部分反应物影响上时的产品的酸值 反应,所以没有对酸值可被控制,耐水解性可以在不使用昂贵的BDO过量,在扩链剂的过量的反应,或使用昂贵的抗水解剂来改善。 此外,通过所述支化剂的量最小化用于,撕裂强度可以提高。
    • 5. 发明公开
    • PRODUCTION METHOD FOR A BIODEGRADABLE POLYESTER COPOLYMER RESIN
    • VERFAHREN ZUR HERSTELLUNG EINES BIOLOGISCH ABBAUBAREN POLYESTERCOPOLYMERHARZES
    • EP2752438A2
    • 2014-07-09
    • EP12828683.8
    • 2012-07-31
    • Samsung Fine Chemicals Co., Ltd.
    • KANG, Gyung DonYUN, Ki ChullCHUN, Jong PilPARK, Sung Bae
    • C08G63/16C08G63/78C08L67/02C08L101/16
    • C08G63/91C08G63/181C08G63/78
    • There is provided a production method for a biodegradable resin using a relatively inexpensive compound as an aromatic dicarboxylic acid compound, wherein, during the process of producing a biodegradable resin in the form of an aliphatic-aromatic polyester copolymer, an aliphatic dihydroxyl compound used as a starting material is used in an amount of between 1 and 1.5 equivalent weight with respect to aliphatic and aromatic dicarboxylic acid compounds. The present invention includes the steps of: causing a hydroxyl group of the aliphatic dihydroxyl compound to undergo a first reaction with a carboxyl group of the aliphatic dicarboxylic acid compound; and causing the residual hydroxyl group of the aliphatic dihydroxyl compound to undergo a second reaction with a carboxyl group of the aromatic dicarboxylic acid compound. The present invention has the advantage that it is possible to produce the aliphatic-aromatic polyester copolymer biodegradable resin by means of an efficient method while not detracting from the mechanical properties of the biodegradable resin.
    • 提供了使用相对便宜的化合物作为芳族二羧酸化合物的生物降解性树脂的制备方法,其中在制备脂族 - 芳族聚酯共聚物形式的生物可降解树脂的过程中,使用脂族二羟基化合物作为 相对于脂族和芳族二羧酸化合物,原料的使用量为1-1.5当量。 本发明包括以下步骤:使脂族二羟基化合物的羟基与脂族二羧酸化合物的羧基进行第一反应; 使残存的脂肪族二羟基化合物的羟基与芳香族二羧酸化合物的羧基进行第二次反应。 本发明的优点在于,可以通过有效的方法制造脂肪族 - 芳香族聚酯共聚物生物降解性树脂,而不会降低生物降解性树脂的机械性能。
    • 6. 发明公开
    • BIODEGRADABLE RESIN COMPOSITION, AND DRAINING BOARD CORE MATERIAL AND DRAINING BOARD PRODUCED THEREFROM
    • 生物降解性树脂排水板和核材料和制品生产排水板
    • EP2749605A2
    • 2014-07-02
    • EP12825113.9
    • 2012-08-22
    • Samsung Fine Chemicals Co., Ltd.S-Enpol Co., Ltd.
    • YOON, Yoon MoCHO, Kwan YoungOH, UkCHUN, Jong PilYUN, Ki ChullPARK, Yong Dae
    • C08L101/16C08L67/02C08L23/00C08K3/26
    • C08L67/02C08K3/26C08K2003/265C08L23/02C08L23/04C08L23/06C08L23/10C08L23/12C08L83/04C08L101/16Y10T428/23
    • A biodegradable resin composition is provided. More particularly, a biodegradable resin composition for a core of a drain board, which has excellent extrusion productivity and thus improves productivity by improving physical properties, for example, reducing contractibility and elasticity recovery, according to original characteristics of a biodegradable resin without degradation in biodegrability of the biodegradable resin by mixing the biodegradable resin with an additional material for improving processibility in suitable amounts, a core of a drain board using the same, and a method of manufacturing a drain board.
      The biodegradable resin composition is prepared by mixing 5 to 60 parts by weight of calcium carbonate, 1 to 10 parts by weight of a thermoplastic resin, and 0.1 to 5 parts by weight of a lubricant with respect to 100 parts by weight of a biodegradable polymer compound, or mixing 1 to 5 parts by weight of the additives, which are formed in a pellet state to have 60 to 90 parts by weight of calcium carbonate, 5 to 15 parts by weight of a thermoplastic resin, and 1 to 5 parts by weight of a lubricant, with respect to 100 parts by weight of a biodegradable polymer compound.
    • 本发明提供一种生物降解性树脂组合物。 更具体地,排水板的芯,其具有优异的挤出生产率并因此通过提高物理特性,例如,在可生物降解性降低收缩和弹性恢复,雅丁到生物降解性树脂的原始特性,而不会退化提高生产率的生物降解性树脂组合物 通过在额外材料与所述生物降解性树脂混合在合适的量提高加工性能的可生物降解的树脂的,使用其的排水板的芯,和一种制造滴水板的方法。 生物降解性树脂组合物是通过按重量计的可生物降解的聚合物的重量,相对于100份润滑剂混合5〜60重量份的碳酸钙,1至10重量份的热塑性树脂,和0.1〜5重量份制备 化合物,或按重量计的添加剂,其在颗粒状态形成为具有60至90重量份的碳酸钙混合1至5份,5〜15重量份的热塑性树脂,和1〜5质量份 重量的润滑剂,与按重量计的可生物降解的高分子化合物的相对于100份。