    • 2. 发明公开
    • LOW ALLOY STEEL
    • 低合金钢
    • EP1873270A1
    • 2008-01-02
    • EP06745409.0
    • 2006-04-17
    • SUMITOMO METAL INDUSTRIES, LTD.
    • IGARASHI, Masaaki, Sumitomo Metal Industries, Ltd.KAWANO, Kaori, Sumitomo Metal Industries, Ltd.
    • C22C38/00C22C38/32C22C38/54
    • C22C38/22C22C38/02C22C38/04C22C38/24
    • A low alloy steel for a heat-resisting structural member being improved in long time creep ductility at high temperatures and temper softening resistance, characterized by comprising, by mass percent, C: 0.03 to 0.10%, Si: not more than 0.30%, Mn: not more than 1.0%, Cr: more than 1.5% to not more than 2.5%, Mo: 0.01 to 1.0%, V: 0.04 to 0.30%, Nb: 0.001 to 0.10%, Ti: 0.001 to 0.020%, B: 0.0001 to 0.020%, Al: 0.001 to 0.01% and Nd: 0.0001 to 0.050%, with the balance being Fe and impurities, wherein the content of P is not more than 0.020%, the content of S is not more than 0.003%, the content of N is less than 0.0050% and the content of O (oxygen) is not more than 0.0050% among the impurities, in which the value of BSO represented by the following formula (1) is 0.0001 to 0.010: BSO = B - ( 11 / 14 ) N - ( 11 / 32 ) S - ( 11 / 16 ) O
      wherein each element symbol in the formula (1) represents the content (by mass %) of the element concerned. The steel may further contain one or more element selected from among W, Cu, Ni, Co, Mg, Ca, La, Ce, Y, Sm and Pr.
    • 一种用于耐热构件的低合金钢,其在高温下的长时间蠕变延展性和抗回火软化性得到改善,其特征在于以质量百分比计含有C:0.03-0.10%,Si:不大于0.30%,Mn :1.0%以下,Cr:超过1.5%且不超过2.5%,Mo:0.01〜1.0%,V:0.04〜0.30%,Nb:0.001〜0.10%,Ti:0.001〜0.020%,B: 0.0001〜0.020%,Al:0.001〜0.01%,Nd:0.0001〜0.050%,其余为Fe和杂质,P含量为0.020%以下,S含量为0.003% 在下述式(1)所示的BSO的值为0.0001〜0.010的杂质中,N的含量小于0.0050%,O(氧)的含量为0.0050%以下。BSO = B- (11/14)N-(11/32)S-(11/16)O式(1)中的各元素符号表示相关元素的含量(以质量%计)。 该钢还可以含有选自W,Cu,Ni,Co,Mg,Ca,La,Ce,Y,Sm和Pr中的一种或多种元素。
    • 5. 发明公开
    • MARTENSITIC STAINLESS STEEL
    • 马氏体不锈钢
    • EP1403391A1
    • 2004-03-31
    • EP02728217.7
    • 2002-05-31
    • SUMITOMO METAL INDUSTRIES, LTD.
    • KONDO, Kunio, Sumitomo Metal Industries, Ltd.KUSHIDA, Takahiro, Sumitomo Metal Industries, Ltd.KOMIZO, Yuichi, Sumitomo Metal Industries, Ltd.IGARASHI, Masaaki, Sumitomo Metal Industries, Ltd.
    • C22C38/00
    • C22C38/44C21D8/005C21D8/0263C21D2211/008C22C38/42C22C38/46
    • A martensitic stainless steel having a C content of 0.01 to 0.1 mass %, a Cr content of 9 to 15 mass % and a N content of not more than 0.1 mass %, wherein the content of carbides inside old austenite grain boundaries in the steel is not more than 0.5 volume %, or wherein the maximum length of the carbides in the steel is 10 to 200 nm in the direction of the minor axis, or wherein the ratio ([Cr]/[Fe]) of the average Cr concentration [Cr] to the average Fe concentration [Fe] in carbides in the steel is not more than 0.4, or wherein the content of M 23 C 6 type carbides is not more than 1 volume %, the content of M 3 C type carbides is 0.01 to 1.5 volume % and the content of MN type or M 2 N type nitrides is not more than 0.3 volume % is provided. This stainless steel has a high toughness in spite of both a relatively more C content and a high strength, thereby providing a wide applicability to pipe material for oil wells containing carbon dioxide and a very small amount of hydrogen sulfide, in particular for oil wells having a much greater depth.
    • 1。一种马氏体系不锈钢,其中,C含量为0.01〜0.1质量%,Cr含量为9〜15质量%,N含量为0.1质量%以下,其中钢中的旧奥氏体晶界内的碳化物含量为 不超过0.5体积%,或者其中钢中碳化物的最大长度在短轴方向上为10至200nm,或者其中平均Cr浓度的比率[(Cr)/ [Fe] Cr]与钢中碳化物中的平均Fe浓度[Fe]之比不大于0.4,或其中M23C6型碳化物的含量不大于1体积%,M3C型碳化物的含量为0.01-1.5体积%和 提供MN型或M2N型氮化物的含量不超过0.3体积%。 尽管C含量和强度都较高,但这种不锈钢具有高韧性,因此对含有二氧化碳和极少量硫化氢的油井的管道材料提供了广泛的适用性,特别是对于具有 更深入。