    • WATER-DISPERSING ACRYLIC ADHESIVE COMPOSITION AND ADHESIVE SHEET
    • 在高分辨率分辨率的ACRYLHAFTMITTELZUSAMMENSETZUNG UND HAFTFOLIE DARAUS
    • EP2562228A1
    • 2013-02-27
    • EP11771902.1
    • 2011-04-12
    • Nitto Denko Corporation
    • MORIMOTO, YuAMANO, TatsumiMITSUI, KazumaYONEZAKI, KousukeTAKASHIMA, KyokoTAKASHIMA, Atsushi
    • C09J133/00C09J7/02C09J11/06C09J171/02
    • C09J143/02C08F2220/1858C08L33/06C09J7/38C09J133/10C09J171/02C09J2203/318C09J2433/00C09J2471/00Y10T428/2887Y10T428/2891C08F220/14C08F220/06
    • Provided is a water-dispersible acrylic pressure-sensitive adhesive composition capable of forming a pressure-sensitive adhesive layer which is resistant to increase in adhesive strength with time, has a good appearance, and less stains an adherend. The water-dispersible acrylic pressure-sensitive adhesive composition includes an acrylic emulsion polymer; and a water-insoluble crosslinking agent having two or more carboxyl-reactive functional groups per molecule. The acrylic emulsion polymer is formed from constitutive monomers essentially including a (meth)acrylic alkyl ester (A), a carboxyl-containing unsaturated monomer (B), and at least one monomer (C) selected from methyl methacrylate, vinyl acetate, and diethylacrylamide and has a solvent-insoluble content of 70 percent by weight or more. When the acrylic pressure-sensitive adhesive composition is applied so as to have a dry thickness of 50 µm, dried at 120°C for 2 minutes, and aged at 50°C for 3 days to give a cross-linked acrylic pressure-sensitive adhesive film, the film has a solvent-insoluble content of 90 percent by weight or more and an elongation at break of 130% or less at 23°C.
    • 本发明提供一种能够形成耐粘合强度随时间增加的粘合剂层的水分散性丙烯酸类压敏粘合剂组合物,具有良好的外观,并且较少污染被粘物。 水分散性丙烯酸类压敏粘合剂组合物包括丙烯酸乳液聚合物; 和每分子具有两个以上羧基反应性官能团的水不溶性交联剂。 丙烯酸乳液聚合物由主要包含(甲基)丙烯酸烷基酯(A),含羧基不饱和单体(B)和至少一种选自甲基丙烯酸甲酯,乙酸乙烯酯和二乙基丙烯酰胺的单体(C))的组成单体形成 并且溶剂不溶物含量为70重量%以上。 当丙烯酸类压敏粘合剂组合物施加到干燥厚度为50μm时,在120℃下干燥2分钟,并在50℃下老化3天,得到交联的丙烯酸类压敏粘合剂 薄膜,在23℃下,溶剂不溶物含量为90重量%以上,断裂伸长率为130%以下。