    • 2. 发明公开
    • Iron antimony-containing metal oxide catalyst composition and process for producing the same
    • Eisen-Antimon enthaltender Katalysator sowie Verfahren zur Herstellung desselben。
    • EP0476579A1
    • 1992-03-25
    • EP91115741.0
    • 1991-09-17
    • NITTO CHEMICAL INDUSTRY CO., LTD.
    • Sasaki, Yutaka, c/o Nitto Chem.Ind.Co.,Ltd.Utsumi, Hiroshi, c/o Nitto Chem.Ind.Co.,Ltd.Miyaki, Kenichi, c/o Nitto Chem.Ind.Co.,Ltd.
    • B01J23/88
    • C01C3/0216B01J23/881B01J23/8876B01J23/8877C01C3/0241
    • An iron. antimony-containing metal oxide catalyst composition comprising as essential components iron, antimony, and at least one element selected from the group consisting of vanadium, molybdenum, and tungsten and a process for producing the same are disclosed, the composition being represented by empirical formula:
      wherein Q represents at least one element selected from the group consisting of Li, Na, K, Rb, Cs, Be, Mg, Ca, Sr, Ba, Sc, Y, La, Ce, Pr, Nd, Sm, Th, U, Ti, Zr, Hf, Nb, Ta, Cr, Mn, Re, Co, Ni, Ru, Rh, Pd, Os, lr, Pt, Cu, Ag, Au, Zn, Cd, Hg, Al, Ga, In, TI, Ge, Sn, and Pb; R represents at least one element selected from the group consisting of B, As, Bi, and Se; and a, b, c, d, e, f, g, h, and i each represent an atomic ratio of the respective element, wherein

      a is from 5 to 15,
      b is from 5 to 100,
      the sum of c, d, and e is from 3 to 15, provided that (i) when the sum of c and e is 0, d/a is more than 1, (ii) when the sum of c and e is not 0, (c + e)/a is more than 0.3,
      f is from 0 to 15,
      the sum of g and h is from 0 to 10, provided that when h is not 0, (c + d + e)/h is more than 1, and
      i is a number of oxygen atom as determined corresponding to the oxides formed by combining the above components,

      and said catalyst composition containing a crystalline iron antimonate. The process comprises preparing a slurry essentially containing (i) crystalline iron antimonate and (ii) at least one element selected from the group consisting of vanadium, molybdenum, and tungsten and optionally containing (iii) at least one element selected from the group consisting of the catalyst components represented by Q, R and P, drying the aqueous slurry, and calcining a dried material. The catalyst exhibits excellent activity and physical properties. The process has improved reproducibility.
    • 公开了一种含铁锑的金属氧化物催化剂组合物及其制备方法,该组合物包含作为铁,锑和至少一种选自钒,钼和钨的元素作为必需组分,其组成由 经验式:FeaSbbVcModWeQfRgPhOi其中Q表示选自Li,Na,K,Rb,Cs,Be,Mg,Ca,Sr,Ba,Sc,Y,La,Ce,Pr,Nd,Sm中的至少一种元素 ,Th,U,Ti,Zr,Hf,Nb,Ta,Cr,Mn,Re,Co,Ni,Ru,Rh,Pd,Os,Ir,Pt,Cu,Ag,Au,Zn,Cd,Hg,Al ,Ga,In,Tl,Ge,Sn和Pb; R表示选自B,As,Bi和Se中的至少一种元素; a,b,c,d,e,f,g,h和i分别表示各元素的原子比,a为5〜15,b为5〜100,c,d的和 ,并且e为3至15,条件是(i)当c和e的和为0时,d / a大于1,(ii)当c和e的和不为0时,(c + e )/ a大于0.3,f为0〜15,g和h的和为0〜10,条件是当h不为0时,(c + d + e)/ h大于1, i是对应于通过组合上述组分形成的氧化物确定的氧原子数,以及含有结晶锑酸锑的催化剂组合物。 该方法包括制备基本上含有(i)结晶铁锑酸盐和(ii)至少一种选自钒,钼和钨的元素的浆料,并且任选地含有(iii)至少一种选自以下的元素: 由Q,R和P表示的催化剂组分,干燥含水浆料,并煅烧干燥的材料。 催化剂表现出优异的活性和物理性能。 该方法具有改进的再现性。