    • Method of welding and adhesive bonding of dissimilar metal plates with pre-heating, cooling and welding steps; Dissimilar metal joined body
    • 一种用于与Vorwärmen-,冷却和焊接步骤Klebschweissen异种金属板的方法; 异种金属接头体
    • EP2314408A1
    • 2011-04-27
    • EP10013776.9
    • 2010-10-19
    • Mazda Motor CorporationKobe Steel Ltd.
    • Tanaka, KoujirouNishiguchi, KatsuyaSasabe, Seiji
    • B23K11/11B23K11/16B23K11/18B23K11/20C09J5/10B23K11/24
    • B23K11/115B23K11/166B23K11/185B23K11/20B23K11/24B23K2201/006B23K2201/18B23K2201/34B23K2203/20C09J5/10C09J2400/163Y10T428/12347
    • The joining method of the present invention includes a step of lapping the aluminum alloy plate (1) and the plated steel plate (2) via the adhesive (5), a pre-heating step of clamping both of the metal plates (1, 2) that have been lapped in the lapping step between a pair of electrodes (7, 7) for spot welding and applying pressure thereto, and applying a current between the pair of electrodes (7, 7), a cooling step of pressurizing, after the pre-heating step, both of the metal plates (1, 2) at a pressing force which is higher than that at the start of the pre-heating step in a state where conduction between the electrodes (7, 7) is stopped, and continuing this pressurization over a predetermined cooling time, and a welding step of pressurizing, after the cooling step, both of the metal plates (1, 2) at a pressing force which is higher than that at the start of the pre-heating step, and welding both of the metal plates (1, 2) by applying a current which is higher than the conduction current value in the pre-heating step between the pair of electrodes (7, 7). It is thereby possible to firmly join the dissimilar metal plates (1, 2) by combining adhesion due to an adhesive and spot welding.
    • 本发明的接合方法,包括通过粘接剂(1)和所述镀层钢板(2)研磨所述铝合金板的工序(5),夹紧两个金属板(1,2中的预加热工序 )thathave被套圈的一对电极(7之间的研磨工序中,7),用于点焊和对其施加压力,并在该对电极(7,7),加压的冷却步骤的之间的电流,在将 预加热步骤,这两个金属板(1,2)在一压紧力所有这一切是在其中电极之间的导通(7,7)被停止的状态下的预加热步骤开始时高于和 继续该加压超过预定的冷却时间,和加压,冷却工序后的焊接工序中,这两个金属板(1,2)在一压紧力所有这比在预加热步骤开始时更高, 和(1,2)通过将电流施加的所有比所述传导CUR更高焊接上述两金属板的 在一对电极之间的预加热工序租值(7,7)。 由此,能够利用粘接由于粘结剂和点焊的组合牢固地接合的异种金属板(1,2)。